# US 2022/0278308 A1 · Electrode assembly and secondary battery comprising same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0278308 A1
- Document ID: US20220278308A1
- Status: Published application
- Kind: A1
- Application number: 17/632,090
- Filed: 2020-08-05
- Published: 2022-09-01
- Earliest claimed: 2019-08-13
- Assignees: Samsung SDI Co., Ltd.
- Applicants: Samsung SDI Co., Ltd.
- Inventors: Hyun Ki JEONG; Dong Jin AN; Seung Young PARK
- Web page: https://patentgrep.com/patent/US20220278308A1

## CPC

- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 10/0422: {Cells or battery with cylindrical casing}
- H01M 10/0431: {Cells with wound or folded electrodes (H01M10/045 takes precedence)}
- H01M 10/0587: of accumulators having only wound construction elements, i.e. wound positive electrodes, wound negative electrodes and wound separators
- H01M 10/052: Li-accumulators
- H01M 50/107: having curved cross-section, e.g. round or elliptic (H01M50/103, H01M50/109, H01M50/11 take precedence)
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- H01M 2004/028: {Positive electrodes}
- H01M 2010/4292: {Aspects relating to capacity ratio of electrodes/electrolyte or anode/cathode}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention relates to an electrode assembly and a secondary battery comprising same, wherein by adjusting at least one of a loading level of a positive electrode coating layer and a loading level of a negative electrode coating layer, the negative electrode coating layer can be prevented from unnecessarily increasing in capacity, and a minimum capacity ratio of a positive electrode versus a negative electrode can be maintained in order to minimize lithium precipitation according to the number of winding turns of an electrode assembly.

## Claims

### Claim 1

An electrode assembly comprising:
a negative electrode plate on which a negative electrode coating layer is formed on both surfaces of a negative electrode current collector;
a positive electrode plate on which a positive electrode coating layer is formed on both surfaces of a positive electrode current collector; and
a separator interposed between the positive electrode plate and the negative electrode plate,
wherein the positive electrode coating layer comprises:
a first positive electrode coating layer formed on a front end area of a first surface of the positive electrode current collector;
a second positive electrode coating layer formed on the front end area of a second surface that is an opposite surface of the first surface of the positive electrode current collector;
a third positive electrode coating layer formed on a rear end area of the first surface of the positive electrode current collector; and
a fourth positive electrode coating layer formed on the rear end area of the second surface of the positive electrode current collector,
wherein a loading level of the first positive electrode coating layer is greater than a loading level of the second positive electrode coating layer, and
each of a loading level of the third positive electrode coating layer and a loading level of the fourth positive electrode coating layer is less than the loading level of the first positive electrode coating layer and is greater than the loading level of the second positive electrode coating layer.

### Claim 2 (depends on 1)

The electrode assembly of claim 1, wherein the sum of the loading level of the first positive electrode coating layer and the leading level of the second positive electrode coating layer is equal to or less than the sum of the loading level of the third positive electrode coating layer and the loading level of the fourth positive electrode coating layer.

### Claim 3 (depends on 1)

The electrode assembly of claim 1, wherein the negative electrode coating layer comprises:
a first negative electrode coating layer formed on a front end area of a first surface of the negative electrode current collector;
a second negative electrode coating layer formed on the front end area of a second surface that is an opposite surface of the first surface of the negative electrode current collector;
a third negative electrode coating layer formed on a rear end area of the first surface of the negative electrode current collector; and
a fourth negative electrode coating layer formed on the rear end area of the second surface of the negative electrode current collector.

### Claim 4 (depends on 3)

The electrode assembly of claim 3, wherein the loading level of the first negative electrode coating layer and the leading level of the third negative electrode coating layer are the same, and
the loading level of the second negative electrode coating layer and the loading level of the fourth negative electrode coating layer are the same and less than the loading level of the first negative electrode coating layer.

### Claim 5 (depends on 3)

The electrode assembly of claim 3, wherein the loading level of the first negative electrode coating layer is greater than the leading level of the second negative electrode coating layer, and
the loading level of the third negative electrode coating layer and the loading level of the fourth negative electrode coating layer are less than the loading level of the first negative electrode coating layer and greater than the loading level of the second negative electrode coating layer.

### Claim 6 (depends on 5)

The electrode assembly of claim 5, wherein the sum of the loading level of the first negative electrode coating layer and the leading level of the second negative electrode coating layer is the same as the sum of the loading level of the third negative electrode coating layer and the loading level of the fourth negative electrode coating layer.

### Claim 7 (depends on 1)

The electrode assembly of claim 1, wherein the positive electrode plate further comprises:
a first positive electrode non-coating portion, on which the first positive electrode coating layer and the third positive electrode coating layer are spaced apart from each other so that the positive electrode coating layer is not formed, on the first surface;
a second positive electrode non-coating portion, on which the second positive electrode coating layer and the fourth positive electrode coating layer are spaced apart from each other so that the positive electrode coating layer is not formed, on the second surface; and
a positive electrode tab attached to any one of the first positive electrode non-coating portion or the second positive electrode non-coating portion.

### Claim 8 (depends on 3)

The electrode assembly of claim 3, wherein the negative electrode plate further comprises:
a first negative electrode non-coating portion, on which the first negative electrode coating layer and the third negative electrode coating layer are spaced apart from each other so that the negative electrode coating layer is not formed, on the first surface;
a second negative electrode non-coating portion, on which the second negative electrode coating layer and the fourth negative electrode coating layer are spaced apart from each other so that the negative electrode coating layer is not formed, on the second surface; and
a negative electrode tab attached to any one of the first negative electrode non-coating portion or the second negative electrode non-coating portion.

### Claim 9

An electrode assembly comprising:
a negative electrode plate on which a negative electrode coating layer is formed on both surfaces of a negative electrode current collector;
a positive electrode plate on which a positive electrode coating layer is formed on both surfaces of a positive electrode current collector; and
a separator interposed between the positive electrode plate and the negative electrode plate,
wherein the positive electrode coating layer comprises:
a first positive electrode coating layer formed on a front end area of a first surface of the positive electrode current collector;
a second positive electrode coating layer formed on the front end area of a second surface that is an opposite surface of the first surface of the positive electrode current collector;
a third positive electrode coating layer formed on a rear end area of the first surface of the positive electrode current collector; and
a fourth positive electrode coating layer formed on the rear end area of the second surface of the positive electrode current collector,
wherein a loading level of the first positive electrode coating layer is greater than a loading level of the second positive electrode coating layer, and
each of a loading level of the third positive electrode coating layer and a loading level of the fourth positive electrode coating layer is less than the loading level of the first positive electrode coating layer and is greater than the loading level of the second positive electrode coating layer.

### Claim 10 (depends on 9)

The electrode assembly of claim 9, wherein the sum of the loading level of the first negative electrode coating layer and the leading level of the second negative electrode coating layer is equal to or less than the sum of the loading level of the third negative electrode coating layer and the loading level of the fourth negative electrode coating layer.

### Claim 11 (depends on 9)

The electrode assembly of claim 9, wherein the positive electrode coating layer comprises:
a first positive electrode coating layer formed on a front end area of a first surface of the positive electrode current collector;
a second positive electrode coating layer formed on the front end area of a second surface that is an opposite surface of the first surface of the positive electrode current collector;
a third positive electrode coating layer formed on a rear end area of the first surface of the positive electrode current collector; and
a fourth positive electrode coating layer formed on the rear end area of the second surface of the positive electrode current collector,
wherein a loading level of the first positive electrode coating layer is the same as a loading level of the third positive electrode coating layer, and
a loading level of the second positive electrode coating layer and a loading level of the fourth positive electrode coating layer are the same and less than the loading level of the first positive electrode coating layer.

### Claim 12 (depends on 1)

A secondary battery comprising:
the electrode assembly of claim 1;
a case having an internal space, wherein the electrode assembly accommodates an electrolyte in the internal space; and
a cap plate coupled to an upper portion of the case to seal the case.