# US 2022/0278306 A1 · Method of producing electrode for secondary battery and electrode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0278306 A1
- Document ID: US20220278306A1
- Status: Published application
- Kind: A1
- Application number: 17/680,305
- Filed: 2022-02-25
- Published: 2022-09-01
- Earliest claimed: 2021-03-01
- Assignees: Prime Planet Energy & Solutions, Inc.
- Applicants: Prime Planet Energy & Solutions, Inc.
- Inventors: Naohiro MASHIMO; Katsushi ENOKIHARA; Haruka SHIONOYA
- Web page: https://patentgrep.com/patent/US20220278306A1

## CPC

- H01M 4/0435: {Rolling or calendering}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0409: {by a doctor blade method, slip-casting or roller coating}
- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/139: Processes of manufacture
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/387: {Tin or alloys based on tin}
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/622: {being polymers}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/025: {with shapes other than plane or cylindrical}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method of producing an electrode disclosed here includes a step in which a moisture powder formed of agglomerated particles; a step in which a coating film composed of the moisture powder is formed using the moisture powder on the electrode current collector when a gas phase of the coating film remains; a step in which a concave/convex shape is formed on a surface part of the coating film; a step in which a coating material containing at least one type of inorganic compound is applied to the coating film on which the concave/convex shape is formed; and a step in which the coating film and the coating material are dried, and the electrode having an electrode active material layer and a coating component in a concave part of the concave/convex shape on the electrode active material layer is formed.

## Claims

### Claim 1

A method of producing an electrode for a secondary battery having any electrode current collector of positive and negative electrodes and an electrode active material layer, the method including the following steps:
a step in which a moisture powder is prepared, the moisture powder is formed of agglomerated particles containing at least an electrode active material, a binder resin, and a solvent, and at least 50% by number or more of the agglomerated particles have the following properties:
(1) a solid phase, a liquid phase, and a gas phase form a pendular state or a funicular state; and
(2) a layer of the solvent is not observed on the outer surface of the agglomerated particles in electron microscope observation;
a step in which a coating film composed of the moisture powder is formed using the moisture powder on the electrode current collector while leaving a gas phase of the coating film;
a step in which a concave/convex shape is formed on a surface part of the coating film with a predetermined pattern and a certain pitch;
a step in which a coating material containing at least one type of inorganic compound is applied to the coating film on which the concave/convex shape is formed; and
a step in which the coating film formed on the electrode current collector and the coating material are dried, and the electrode having an electrode active material layer made of the coating film and a coating component made of the coating material disposed in a concave part of the concave/convex shape on the active material layer is formed.

### Claim 2 (depends on 1)

The method of producing an electrode for a secondary battery according to claim 1, wherein the concave/convex forming step is carried out such a way as to form a concave/convex surface in which, when the surface area of a reference area of the coating film indicated by L cm×B cm (L and B are integers of 3 or higher) is measured at n (n is an integer of 5 or higher) different points, the average surface area is 1.05×L×B cm2 or more.

### Claim 3 (depends on 1)

The method of producing an electrode for a secondary battery according to claim 1, wherein the inorganic compound contains at least one selected from the group consisting of alumina, boehmite, silica, magnesia, zirconia and titania.

### Claim 4 (depends on 1)

The method of producing an electrode for a secondary battery according to claim 1, wherein the coating material contains at least one type of active material as the inorganic compound, and the active material contains at least one metal element of silicon and tin as a constituent element.

### Claim 5

An electrode for a secondary battery which is any electrode of positive and negative electrodes of a secondary battery, comprising
an electrode current collector, an electrode active material layer formed on the electrode current collector, and a coating component containing at least one type of inorganic compound,
wherein the surface of the electrode active material layer has a concave/convex shape with a predetermined pattern and a certain pitch, and
wherein a height difference between a concave part and a convex part of the concave/convex shape is 10 μm or more, and
wherein at least a part of the coating component is disposed in the concave part of the concave/convex shape.

### Claim 6 (depends on 5)

The electrode for a secondary battery according to claim 5,
wherein the electrode active material layer in the concave part is uniformly divided into three layers, an upper layer, an intermediate layer and a lower layer, in the thickness direction from the surface of the active material layer to the current collector, and when the electrode densities (g/cm3) of the upper layer, the intermediate layer, and the lower layer of the concave part are d1, d2, and d3, respectively, they have a relationship of 0.8<(d1/d3)<1.1.

### Claim 7 (depends on 5)

The electrode for a secondary battery according to claim 5, wherein the inorganic compound contains at least one selected from the group consisting of alumina, boehmite, silica, magnesia, zirconia and titania.

### Claim 8 (depends on 5)

The electrode for a secondary battery according to claim 5, wherein the coating component contains at least one type of active material as the inorganic compound, and the active material contains at least one metal element of silicon and tin as a constituent element.