# US 2022/0278249 A1 · Near-infrared light emitting semiconductor element and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0278249 A1
- Document ID: US20220278249A1
- Status: Published application
- Kind: A1
- Application number: 17/682,093
- Filed: 2022-02-28
- Published: 2022-09-01
- Earliest claimed: 2019-09-03
- Assignees: Osaka University
- Applicants: Osaka University
- Inventors: Shuhei ICHIKAWA; Naoki YOSHIOKA; Yasufumi FUJIWARA; Jun TATEBAYASHI
- Web page: https://patentgrep.com/patent/US20220278249A1

## CPC

- H10H 20/01335: {the light-emitting regions comprising nitride materials}
- C23C 16/18: from metallo-organic compounds
- C23C 16/303: {Nitrides}
- C23C 16/34: Nitrides {(C23C16/303 takes precedence)}
- C23C 16/52: Controlling or regulating the coating process {(C23C16/45557, C23C16/279 take precedence)}
- C30B 25/02: Epitaxial-layer growth
- C30B 29/406: {Gallium nitride}
- C30B 29/68: Crystals with laminate structure, e.g. "superlattices"
- H10H 20/0137: {the light-emitting regions comprising nitride materials}
- H10H 20/825: containing nitrogen, e.g. GaN
- H10H 20/8252: {characterised by the dopants}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2921: {being crystalline insulating materials}
- H10P 14/3216: {Nitrides}
- H10P 14/3251: {consisting of three or more layers}
- H10P 14/3416: {Nitrides}
- H10P 14/3444: {P-type}
- H10P 14/3446: {Transition metal elements; Rare earth elements}
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Provided are: a near infrared light-emitting semiconductor element that does not contain any harmful elements and that makes it possible to obtain near infrared light of a stable wavelength in a narrow band regardless of the operating environment; and a method for producing the near infrared light-emitting semiconductor element. GaN is used in the method for producing a near infrared light-emitting semiconductor element, and an active layer added in order to substitute Tm with Ga is formed on GaN in a reaction container at a growth rate of 0.1-30 μm/h without removal from said reaction container using an organometallic vapor phase growth method under temperature conditions of 600-1400° C. in a series of formation steps including formation of a p-type layer and an n-type layer. GaN is used in the near infrared light-emitting semiconductor element, and said near infrared light-emitting semiconductor element includes an active layer sandwiched between an n-type layer and a p-type layer on a substrate. An organometallic vapor phase growth method is used to add the active layer to the GaN in order to substitute Tm with Ga.

## Claims

### Claim 1

A method for manufacturing a near-infrared light emitting semiconductor element, wherein
an active layer obtained by adding Tm to replace the Ga in GaN by supplying Tm(i-PrCp)3 and controlling the substitution site of Tm3+ ion so that it is in the Ga site and its immediate vicinity is formed at a growth rate of 1 to 30 μm/h in a reaction vessel without removing it from the reaction vessel, using a metal organic chemical vapor deposition, under the temperature condition of 600-1400° C., in a series of forming steps of a p-type layer and an n-type layer.

### Claim 2 (depends on 1)

The method for manufacturing a near-infrared light emitting semiconductor element according to claim 1, wherein the amount of Tm added is 1×1012 to 1×1023 cm−3.

### Claim 3 (depends on 1)

The method for manufacturing a near-infrared light emitting semiconductor element according to claim 1, wherein the active layer is formed by stacking a plurality of the Tm-added GaN layer and the Tm-free GaN layer as a pair.

### Claim 4 (depends on 1)

The method for manufacturing a near-infrared light emitting semiconductor element according to claim 1, wherein the growth pressure of the active layer in the metal organic chemical vapor deposition exceeds 0.01 kPa and is less than 300 kPa.

### Claim 5 (depends on 1)

The method for manufacturing a near-infrared light emitting semiconductor element according to claim 1, wherein the flow rate of the carrier gas in the metal organic chemical vapor deposition used for forming the active layer is 10 to 300 SLM.

### Claim 6

A near-infrared light emitting semiconductor element which uses GaN and emits light by current injection, and which has an active layer sandwiched between an n-type layer and a p-type layer on a substrate, wherein the active layer is obtained by adding Tin to replace the Ga in GaN by using a metal organic chemical vapor deposition.

### Claim 7 (depends on 6)

The near-infrared light emitting semiconductor element according to claim 6, wherein the amount of Tin added to the active layer is 1×1012 to 1×1023 cm−3.

### Claim 8 (depends on 6)

The near-infrared light emitting semiconductor element according to claim 6, wherein the active layer is formed by stacking a plurality of the Tm-added GaN layer and the Tm-free GaN layer as a pair.

### Claim 9 (depends on 2)

The method for manufacturing a near-infrared light emitting semiconductor element according to claim 2, wherein the active layer is formed by stacking a plurality of the Tm-added GaN layer and the Tm-free GaN layer as a pair.

### Claim 10 (depends on 2)

The method for manufacturing a near-infrared light emitting semiconductor element according to claim 2, wherein the growth pressure of the active layer in the metal organic chemical vapor deposition exceeds 0.01 kPa and is less than 300 kPa.

### Claim 11 (depends on 3)

The method for manufacturing a near-infrared light emitting semiconductor element according to claim 3, wherein the growth pressure of the active layer in the metal organic chemical vapor deposition exceeds 0.01 kPa and is less than 300 kPa.

### Claim 12 (depends on 2)

The method for manufacturing a near-infrared light emitting semiconductor element according to claim 2, wherein the flow rate of the carrier gas in the metal organic chemical vapor deposition used for forming the active layer is 10 to 300 SLM.

### Claim 13 (depends on 3)

The method for manufacturing a near-infrared light emitting semiconductor element according to claim 3, wherein the flow rate of the carrier gas in the metal organic chemical vapor deposition used for forming the active layer is 10 to 300 SLM.

### Claim 14 (depends on 4)

The method for manufacturing a near-infrared light emitting semiconductor element according to claim 4, wherein the flow rate of the carrier gas in the metal organic chemical vapor deposition used for forming the active layer is 10 to 300 SLM.

### Claim 15 (depends on 7)

The near-infrared light emitting semiconductor element according to claim 7, wherein the active layer is formed by stacking a plurality of the Tin-added GaN layer and the Tm-free GaN layer as a pair.