# US 2022/0278170 A1 · Trench formation scheme for programmable metallization cell to prevent metal redeposit

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0278170 A1
- Document ID: US20220278170A1
- Status: Published application
- Kind: A1
- Application number: 17/748,601
- Filed: 2022-05-19
- Published: 2022-09-01
- Earliest claimed: 2019-05-10
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Fu-Ting Sung; Chung-Chiang Min; Yuan-Tai Tseng
- Web page: https://patentgrep.com/patent/US20220278170A1

## CPC

- G11C 5/06: Arrangements for interconnecting storage elements electrically, e.g. by wiring
- H10B 63/30: {comprising selection components having three or more electrodes, e.g. transistors}
- G11C 13/0011: {comprising conductive bridging RAM [CBRAM] or programming metallization cells [PMCs]}
- H10B 63/10: Phase change RAM [PCRAM, PRAM] devices
- H10B 63/80: {Arrangements comprising multiple bistable or multi-stable switching components of the same type on a plane parallel to the substrate, e.g. cross-point arrays}
- H10N 70/063: {by etching of pre-deposited switching material layers, e.g. lithography}
- H10N 70/245: {the species being metal cations, e.g. programmable metallization cells}
- H10N 70/823: {adapted for essentially horizontal current flow, e.g. bridge type devices}
- H10N 70/826: {adapted for essentially vertical current flow, e.g. sandwich or pillar type devices}
- H10N 70/883: {Oxides or nitrides}
- H10N 70/8833: {Binary metal oxides, e.g. TaOx}
- G11C 13/003: {Cell access}
- G11C 2213/79: Array wherein the access device being a transistor
- G11C: STATIC STORES (semiconductor memory devices H10B)
- H10B: ELECTRONIC MEMORY DEVICES
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

Some embodiments relate to a method for forming a memory device. The method includes forming a lower dielectric layer over a conductive wire. A stack of memory layers is formed within the lower dielectric layer and over the conductive wire. The stack of memory layers comprises a top electrode, a bottom electrode, and a data storage layer between the top electrode and the bottom electrode. A removal process is performed on the stack of memory layers to define a programmable metallization cell that comprises the top electrode, the bottom electrode, and the data storage layer. The programmable metallization cell comprises a central region and a peripheral region that extends upwardly from the central region. A top surface of the programmable metallization cell and a top surface of the lower dielectric layer are coplanar.

## Claims

### Claim 1

A method for forming a memory device, the method comprising:
forming a lower dielectric layer over a conductive wire;
forming a stack of memory layers within the lower dielectric layer and over the conductive wire, wherein the stack of memory layers comprises a top electrode, a bottom electrode, and a data storage layer between the top electrode and the bottom electrode; and
performing a removal process on the stack of memory layers to define a programmable metallization cell that comprises the top electrode, the bottom electrode, and the data storage layer, wherein the programmable metallization cell comprises a central region and a peripheral region that extends upwardly from the central region, and wherein a top surface of the programmable metallization cell and a top surface of the lower dielectric layer are coplanar.

### Claim 2 (depends on 1)

The method of claim 1, wherein the removal process includes performing a planarization process into the stack of memory layers until the top surface of the lower dielectric layer is reached.

### Claim 3 (depends on 2)

The method of claim 2, wherein the planarization process comprises one or more slurry for a non-selective chemical-mechanical planarization.

### Claim 4 (depends on 2)

The method of claim 2, wherein the removal process further comprises performing a wet etch process after the planarization process.

### Claim 5 (depends on 4)

The method of claim 4, wherein the removal process further comprises performing a pullback etch process after the wet etch process, wherein the wet etch process utilizes one or more first etchants and the pullback etch process utilizes one or more second etchants different from the one or more first etchants.

### Claim 6 (depends on 5)

The method of claim 5, wherein the pullback etch process removes portions of the top and bottom electrodes such that top surfaces of the top and bottom electrodes are below the top surface of the lower dielectric layer.

### Claim 7 (depends on 5)

The method of claim 5, wherein the pullback etch process removes a portion of the data storage layer such that a top surface of the data storage layer is below the top surface of the lower dielectric layer.

### Claim 8 (depends on 1)

The method of claim 1, wherein a thickness of the data storage layer is less than a thickness of the bottom electrode and a thickness of the top electrode.

### Claim 9 (depends on 8)

The method of claim 8, wherein the thickness of the top electrode is greater than the thickness of the bottom electrode.

### Claim 10

A method for forming a memory device, the method comprising:
depositing a lower dielectric layer over a conductive wire;
performing a patterning process on the lower dielectric layer to form an opening in the lower dielectric layer that exposes an upper surface of the conductive wire, wherein the patterning process forms a pair of opposing sidewalls in the lower dielectric layer, wherein the pair of opposing sidewalls respectively comprise a slanted sidewall segment vertically above a curved sidewall segment;
depositing a stack of memory layers over the conductive wire and within the opening, wherein the stack of memory layers comprises a bottom electrode layer, a top electrode layer, and a data storage film between the bottom electrode layer and the top electrode layer, wherein the stack of memory layers conforms to the pair of opposing sidewalls of the lower dielectric layer; and
performing a planarization process on the stack of memory layers to remove portions of the bottom electrode layer, the top electrode layer, and the data storage film from over the lower dielectric layer, wherein the planarization process defines a memory cell comprising a top electrode, a bottom electrode, and a data storage layer in the opening.

### Claim 11 (depends on 10)

The method of claim 10, wherein the patterning process comprises performing a first etch process to form the slanted sidewall segment and a second etch process to form the curved sidewall segment, wherein the first etch process is different from the second etch process.

### Claim 12 (depends on 10)

The method of claim 10, wherein the planarization process includes performing a single chemical-mechanical planarization (CMP) process to define the memory cell.

### Claim 13 (depends on 10)

The method of claim 10, wherein the patterning process etches the conductive wire such that an upper surface of the conductive wire is vertically below a bottom surface of the lower dielectric layer by a non-zero distance.

### Claim 14 (depends on 13)

The method of claim 13, wherein a bottom surface of the memory cell contacts the upper surface of the conductive wire.

### Claim 15 (depends on 10)

The method of claim 10, further comprising:
performing a pullback etch process on the top and bottom electrodes, wherein top surfaces of the top and bottom electrodes are below a top surface of the data storage layer.

### Claim 16 (depends on 10)

The method of claim 10, further comprising:
performing a pullback etch process to recess the data storage layer below top surfaces of the top and bottom electrodes.

### Claim 17

A method for manufacturing a memory device, comprising:
forming a bottom dielectric layer over a conductive wire;
patterning the bottom dielectric layer to form an opening above the conductive wire, wherein the opening has a curved sidewall such that a width of the opening continuously increases from a bottom surface of the bottom dielectric layer to a top surface of the bottom dielectric layer;
forming a stack of memory layers over the conductive wire and within the opening, wherein the stack of memory layers comprises a top electrode overlying a bottom electrode and a data storage layer between the top electrode and the bottom electrode, wherein a thickness of the data storage layer is less than a thickness of the top electrode and a thickness of the bottom electrode; and
performing a planarization process on the stack of memory layers, such that a top surface of the top electrode is level with a top surface of the bottom electrode.

### Claim 18 (depends on 17)

The method of claim 17, wherein the stack of memory layers comprises a center region overlying and conformally lining the opening, such that the stack of memory layers comprises an outer region overlying a top surface of the bottom dielectric layer, wherein the outer region is vertically above the center region.

### Claim 19 (depends on 17)

The method of claim 17, wherein the patterning comprises performing an etch process and the planarization process comprises performing a chemical-mechanical planarization process.

### Claim 20 (depends on 17)

The method of claim 17, wherein the patterning removes a portion of the conductive wire, such that the stack of memory layers extends below a bottom surface of the bottom dielectric layer.