# US 2022/0276196 A1 · Gas Sensor Device Containing Lithium Garnet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0276196 A1
- Document ID: US20220276196A1
- Status: Published application
- Kind: A1
- Application number: 17/562,658
- Filed: 2021-12-27
- Published: 2022-09-01
- Earliest claimed: 2021-02-26
- Assignees: Massachusetts Institute of Technology
- Applicants: Massachusetts Institute of Technology
- Inventors: Jennifer Lilia Rupp; Zachary Hood; Moran Balaish
- Web page: https://patentgrep.com/patent/US20220276196A1

## CPC

- G01N 27/4045: {for gases other than oxygen}
- G01N 27/4074: {for detection of gases other than oxygen}
- G01N 27/301: {Reference electrodes}
- G01N 27/4035: {Combination of a single ion-sensing electrode and a single reference electrode (G01N27/406 and G01N27/413 take precedence)}
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

An SOx sensor includes a lithium garnet electrolyte, a sensing electrode, a reference electrode, and a heating element. The sensing electrode includes Li2SO4 and at least one metal oxide or second metal sulfate. One surface of the sensing electrode is disposed on at least a portion of a surface of the lithium garnet electrolyte. A current collector is disposed on at least a portion another surface of the sensing electrode to electrically couple the sensing electrode to the reference electrode via a potentiometer. The reference electrode is disposed on the lithium garnet electrolyte. The heating element is capable of heating the sensing electrode and the lithium garnet electrolyte to a temperature sufficient to achieve a sensor response time of less than about 30 minutes.

## Claims

### Claim 1

An SOx sensor comprising:
a lithium garnet electrolyte;
a sensing electrode comprising Li2SO4 and at least one of a metal oxide or a second metal sulfate, wherein a first surface of the sensing electrode is disposed on at least a portion of a first surface of the lithium garnet electrolyte;
a current collector disposed on at least a portion of a second surface of the sensing electrode;
a reference electrode disposed on the lithium garnet electrolyte, wherein the reference electrode is electrically coupled to the current collector via a potentiometer; and
a heating element capable of heating the sensing electrode and the lithium garnet electrolyte to a temperature sufficient to achieve a sensor response time of less than about 30 minutes.

### Claim 2 (depends on 1)

The SOx sensor of claim 1, wherein the reference electrode is disposed on at least a portion of the first surface or a second surface of the lithium garnet electrolyte.

### Claim 3 (depends on 1)

The SOx sensor of claim 1, wherein the sensing electrode comprises Li2SO4 and the second metal sulfate, and the Li2SO4 and the second metal sulfate are present in a mole ratio of about 1:4 to about 9.5:0.5.

### Claim 4 (depends on 1)

The SOx sensor of claim 1, wherein:
the second metal sulfate is at least one of CaSO4, K2SO4, Na2SO4, Bi2(SO4)3, Ce(SO4)2, ZnSO4, Zr(SO4)2, Fe2(SO4)3, Y2(SO4)3, La2(SO4)3, Ta2SO4, or BaSO4; and
the metal oxide is at least one of FeO, Fe2O3, Fe3O4, VO, VO2, V2O3, V2O5, NiO, ZnO, CeO2, SnO2, Ga2O3, WO3, TiO2, Pt, In2O3, or LaxSm1−xFeO3 where x is 0.2, 0.4, 0.5, 0.6, or 0.8.

### Claim 5 (depends on 1)

The SOx sensor of claim 1, wherein a thickness of the lithium garnet electrolyte is about 100 nm to about 80 μm.

### Claim 6 (depends on 1)

The SOx sensor of claim 1, wherein the sensing electrode additionally comprises at least one of lithium garnet phase or (La0.6Sr0.4)0.99CoO3−δ phase.

### Claim 7 (depends on 1)

The SOx sensor of claim 1, wherein the sensing electrode additionally comprises a catalyst to facilitate oxidation of SOx.

### Claim 8 (depends on 1)

The SOx sensor of claim 1, wherein the lithium garnet has a cubic phase.

### Claim 9 (depends on 8)

The SOx sensor of claim 8, wherein the lithium garnet electrolyte comprises LixLayZrO12 with at least one additional dopant element.

### Claim 10 (depends on 9)

The SOx sensor of claim 9, wherein the lithium garnet electrolyte comprises Li7−xLa3Zr2−xTaxO12, where x is about 0.25 to about 0.6.

### Claim 11 (depends on 1)

The SOx sensor of claim 1, wherein the reference electrode comprises at least one of (La0.6Sr0.4)0.99CoO3−δ, gold, or platinum.

### Claim 12 (depends on 1)

The SOx sensor of claim 1, additionally comprising a capping layer to substantially reduce exposure of the lithium garnet electrolyte to air.

### Claim 13 (depends on 1)

The SOx sensor of claim 1, wherein the sensing electrode has a porous microstructure.

### Claim 14

A method of sensing a SOx gas using an electrochemical sensor comprising:
exposing the SOx gas to a sensing electrode comprising Li2SO4 and at least one of a metal oxide or a second metal sulfate, wherein a first surface of the sensing electrode is disposed on at least a portion of a first surface of a lithium garnet electrolyte;
heating the sensing electrode and the lithium garnet electrolyte to a temperature sufficient to achieve a reaction between the SOx gas, Li+ and O2 to form Li2SO4, thereby changing a potential of the electrochemical sensor; and
detecting a change in the potential of the electrochemical sensor.

### Claim 15 (depends on 14)

The method of claim 14, wherein:
the SOx comprises SO2; and
the method additionally comprises oxidizing the SO2 to SO3.

### Claim 16 (depends on 14)

The method of claim 14, additionally comprising determining a concentration of the SOx gas based at least in part on the change in the potential of the electrochemical sensor.

### Claim 17 (depends on 14)

The method of claim 14, wherein the temperature is between about 200° C. and about 500° C.

### Claim 18

A method of making an SOx sensing electrode comprising:
creating a mixture of Li2SO4 and at least one of a metal oxide or a second metal sulfate;
applying the mixture to at least a portion of a first surface of a lithium garnet electrolyte; and
annealing the lithium garnet electrolyte and the mixture to form the SOx sensing electrode on the at least a portion of the first surface of the lithium garnet electrolyte.

### Claim 19 (depends on 18)

The method of claim 18, wherein annealing comprises melting the mixture of Li2SO4 and the second metal sulfate.

### Claim 20 (depends on 18)