# US 2022/0275495 A1 · Low temperature titanium hardening

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0275495 A1
- Document ID: US20220275495A1
- Status: Published application
- Kind: A1
- Application number: 17/637,431
- Filed: 2020-08-21
- Published: 2022-09-01
- Earliest claimed: 2019-08-23
- Assignees: Elos Medtech Pinol A/S
- Applicants: Elos Medtech Pinol A/S
- Inventors: Thomas Lundin CHRISTIANSEN; Morten Stendahl JELLESEN; Marcel A.J. SOMERS; Andreas Frederik Kielsholm KÖRKEL
- Web page: https://patentgrep.com/patent/US20220275495A1

## CPC

- C23C 8/16: using oxygen-containing compounds, e.g. water, carbon dioxide
- C23C 8/12: using elemental oxygen or ozone
- C23C 8/28: more than one element being applied in one step
- C23C 8/80: After-treatment
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

The present invention relates to a method of oxygen hardening a Group IV metal, the method comprising the steps of: providing a workpiece of a Group IV metal in its final shape; oxidising the Group IV metal over an oxidising duration of at least 10 minutes in an oxidising atmosphere at a first temperature to provide a non-stratified Group IV metal oxide on the surface of the workpiece using a gaseous oxidising species having an upper temperature limit of up to 800° C. wherein the first temperature is in the range of 500° C. and the upper temperature limit of the gaseous oxidising species; diffusing oxygen from the non-stratified Group IV metal oxide into the Group IV metal in an inert atmosphere at a second temperature in the range of 500° C. to 800° C. and at a partial pressure of the gaseous oxidising species of up to 10-4 mbar over a diffusive duration of at least 0.1 hour to provide a superficial diffusion zone comprising oxygen in solid solution. In another aspect, the invention relates to a Group IV metal component comprising a material core having a core hardness and a surface hardness of at least the core hardness +200 HV0.025. The component is obtainable in the method of the invention.

## Claims

### Claim 1

A method of oxygen hardening a Group IV metal, the method comprising the steps of:
providing a workpiece of a Group IV metal in its final shape;
oxidising the Group IV metal over an oxidising duration of at least 10 minutes in an oxidising atmosphere at a first temperature to provide a non-stratified Group IV metal oxide on the surface of the workpiece using a gaseous oxidising species selected from CO2, N2O and combinations of CO2 and N2O, the gaseous oxidising species having an upper temperature limit of up to 800° C. wherein the first temperature is in the range of 500° C. and the upper temperature limit of the gaseous oxidising species;
diffusing oxygen from the non-stratified Group IV metal oxide into the Group IV metal in an inert atmosphere at a second temperature in the range of 500° C. to 800° C. and at a partial pressure of the gaseous oxidising species of up to 10−4 mbar over a diffusive duration of at least 0.1 hour to provide a superficial diffusion zone comprising oxygen in solid solution.

### Claim 2 (depends on 1)

The method of oxygen hardening a Group IV metal according to claim 1, wherein the gaseous oxidising species is CO2, the upper temperature limit is 800° C., and the oxidising duration is in the range of 1 hour to 16 hours.

### Claim 3 (depends on 1)

The method of oxygen hardening a Group IV metal according to claim 1, wherein the gaseous oxidising species is N2O, the upper temperature limit is 700° C., and the oxidising duration is in the range of 10 minutes to 2 hours.

### Claim 4 (depends on 1)

The method of oxygen hardening a Group IV metal according to claim 1, wherein the pressure in the oxidising atmosphere is ambient pressure.

### Claim 5 (depends on 1)

The method of oxygen hardening a Group IV metal according to claim 1, wherein the first temperature is in the range of 600° C. to 700° C.

### Claim 6 (depends on 1)

The method of oxygen hardening a Group IV metal according to claim 1, wherein the total pressure in the inert atmosphere is up to 10−4 mbar.

### Claim 7 (depends on 1)

The method of oxygen hardening a Group IV metal according to claim 1, wherein the inert atmosphere is a noble gas.

### Claim 8 (depends on 1)

The method of oxygen hardening a Group IV metal according to claim 1, wherein the second temperature is in the range of 650° C. to 750° C.

### Claim 9 (depends on 8)

The method of oxygen hardening a Group IV metal according to claim 8, wherein the diffusive duration is in the range of 2 hours to 40 hours.

### Claim 10 (depends on 1)

The method of oxygen hardening a Group IV metal according to claim 1, wherein the Group IV metal comprises aluminium as an alloying element, and the first temperature is in the range of 500° C. to 700° C.

### Claim 11 (depends on 1)

The method of oxygen hardening a Group IV metal according to claim 1, wherein the oxidising atmosphere further comprises CO.

### Claim 12 (depends on 1)

The method of oxygen hardening a Group IV metal according to claim 1, wherein the workpiece of a Group IV metal is polished prior to oxidising the Group IV metal to provide a surface roughness of <0.1 μm in accordance with the ISO 1302:2002 standard.

### Claim 13 (depends on 1)

The method of oxygen hardening a Group IV metal according to claim 1, wherein the gaseous oxidising species is CO2, the first temperature is in the range of 600° C. to 750° C., the oxidising duration is in the range of 1 hour to 8 hours, the second temperature is in the range of 650° C. to 750° C., and the diffusive duration is in the range of 2 to 8 times the oxidising duration.

### Claim 14 (depends on 1)

The method of oxygen hardening a Group IV metal according to claim 1, wherein the gaseous oxidising species is CO2, the first temperature and the second temperature are both in the range of 650° C. to 700° C. with the second temperature being higher than the first temperature, the oxidising duration is in the range of 2 hours to 6 hours, and the diffusive duration is in the range of 3 to 6 times the oxidising duration.

### Claim 15 (depends on 1)

The method of oxygen hardening a Group IV metal according to claim 1, wherein the gaseous oxidising species is N2O, the first temperature is in the range of 600° C. to 650° C., the oxidising duration is in the range of 30 minutes to 2 hours, the second temperature is in the range of 650° C. to 700° C., and the diffusive duration is in the range of 4 to 20 times the oxidising duration.

### Claim 16 (depends on 1)

The method of oxygen hardening a Group IV metal according to claim 1, wherein the oxidising atmosphere is a mixture of CO2 and CO with 40% to 90% CO2 compared to the total of CO2 and CO.

### Claim 17 (depends on 1)

The method of oxygen hardening a Group IV metal according to claim 1, wherein the oxidising atmosphere is a mixture of N2O and CO with 40% to 60% N2O compared to the total of N2O and CO.

### Claim 18

A Group IV metal component comprising a material core having a core hardness and a surface hardness of at least the core hardness +200 HV0.025, a diffusion zone having oxygen in solid solution in the range of a level providing a hardness of 120% of the hardness of the material core to the saturation level of the Group IV metal over a thickness from the surface in the range of 10 μm to 100 μm, the diffusion zone further containing carbon and/or nitrogen in solid solution at a concentration showing a local maximum in the diffusion zone of the carbon content and/or the nitrogen content as detectable with Glow Discharge Optical Emission Spectroscopy (GDOES).

### Claim 19 (depends on 18)

The Group IV metal component according to claim 18, wherein surface hardness is at least 650 HV0.025.

### Claim 20 (depends on 18)

The Group IV metal component according to claim 18, wherein the component has a surface roughness of <0.1 μm in accordance with the ISO 1302:2002 standard.

### Claim 21

(canceled)

### Claim 22 (depends on 18)

The Group IV metal component according to claim 18, wherein the diffusion zone has a thickness of at least 5 μm.

### Claim 23 (depends on 18)

The Group IV metal component according to claim 18, wherein the Group IV metal is selected from the list consisting of titanium, a titanium alloy, zirconium, and a zirconium alloy.

### Claim 24 (depends on 23)

The Group IV metal component according to claim 23, wherein the titanium is titanium of grade 2, 4, or 5 or wherein the zirconium is Zr702 zirconium.