# US 2022/0275477 A1 · Magnesium alloy based objects and methods of making and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0275477 A1
- Document ID: US20220275477A1
- Status: Published application
- Kind: A1
- Application number: 17/637,570
- Filed: 2020-08-06
- Published: 2022-09-01
- Earliest claimed: 2019-08-26
- Assignees: Ohio State Innovation Foundation
- Applicants: Ohio State Innovation Foundation
- Inventors: Aihua LUO; Thomas AVEY
- Web page: https://patentgrep.com/patent/US20220275477A1

## CPC

- C22C 1/02: by melting {(C22C1/1036 takes precedence)}
- C22C 23/00: Alloys based on magnesium
- C22C 23/04: with zinc or cadmium as the next major constituent
- C22F 1/06: of magnesium or alloys based thereon
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

Disclosed herein are magnesium alloy based objects and methods of making and use thereof. For example, disclosed herein are methods of making a magnesium alloy based object, the methods comprising: heating an object comprising a preliminary magnesium alloy at a first temperature for a first amount of time, the preliminary magnesium alloy comprising a first intermetallic phase, a second intermetallic phase, and an alloy phase, to thereby substantially dissolving the first intermetallic phase into the alloy phase to form an object comprising an intermediate magnesium alloy, the intermediate magnesium alloy comprising the second intermetallic phase and the alloy phase; and heating the object comprising the intermediate magnesium alloy at a second temperature for a second amount of time to thereby substantially dissolving the second intermetallic phase into the alloy phase and minimizing incipient melting of the alloy phase to form the magnesium alloy based object.

## Claims

### Claim 1

A method of making a magnesium alloy based object, the method comprising:
heating an object comprising a preliminary magnesium alloy at a first temperature for a first amount of time;
wherein the preliminary magnesium alloy comprises a first intermetallic phase having a melting temperature, a second intermetallic phase having a melting temperature, and an alloy phase having a solidus temperature;
wherein the melting temperature of the first intermetallic phase is lower than the melting temperature of the second intermetallic phase and the solidus temperature of the alloy phase;
wherein the melting temperature of the second intermetallic phase is higher than the solidus temperature of the alloy phase;
wherein the first temperature is above the melting temperature of the first intermetallic phase, below the melting temperature of the second intermetallic phase, and below the solidus temperature of the alloy phase;
thereby substantially dissolving the first intermetallic phase into the alloy phase to form an object comprising an intermediate magnesium alloy, the intermediate magnesium alloy comprising the second intermetallic phase and the alloy phase; and
heating the object comprising the intermediate magnesium alloy at a second temperature for a second amount of time;
wherein the second temperature is above the melting temperature of the second intermetallic phase;
thereby substantially dissolving the second intermetallic phase into the alloy phase and minimizing incipient melting of the alloy phase to form the magnesium alloy based object.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first temperature is from 10° C. to 50° C. above the melting temperature of the first intermetallic phase.

### Claim 3

(canceled)

### Claim 4 (depends on 1)

The method of claim 1, wherein the first amount of time is from 10 hours to 15 hours.

### Claim 5 (depends on 1)

The method of claim 1, wherein the second temperature is from 10° C. to 20° C. above the melting temperature of the second intermetallic phase.

### Claim 6

(canceled)

### Claim 7 (depends on 1)

The method of claim 1, wherein the second amount of time is from 1 hour to 5 hours.

### Claim 8 (depends on 1)

The method of claim 1, wherein the preliminary magnesium alloy comprises a biocompatible magnesium alloy.

### Claim 9 (depends on 1)

The method of claim 1, wherein the preliminary magnesium alloy comprises a Mg—Ca—Zn alloy or a Mg—Ca—Mn—Zn alloy.

### Claim 10

(canceled)

### Claim 11 (depends on 1)

The method of claim 1, wherein the first intermetallic phase comprises Mg6Ca2Zn3, the first temperature is from 340° C. to 360° C., or a combination thereof.

### Claim 12 (depends on 1)

The method of claim 1, wherein the second intermetallic phase comprises Mg2Ca, the second temperature is from 430° C. to 450° C., or a combination thereof.

### Claim 13 (depends on 1)

The method of claim 1, wherein the preliminary magnesium alloy is substantially free of rare earth elements.

### Claim 14

(canceled)

### Claim 15 (depends on 1)

The method of claim 1, further comprising thermomechanically treating the magnesium alloy based object by heating the magnesium based object at a third temperature for a third amount of time and, subsequently, mechanically treating the magnesium alloy based object, wherein the third temperature is above room temperature and below the solidus temperature.

### Claim 16

(canceled)

### Claim 17 (depends on 15)

The method of claim 15, wherein the third temperature is from 10° C. to 50° C. below the solidus temperature, the third amount of time is from 1 minute to 1 hour, or a combination thereof.

### Claim 18

(canceled)

### Claim 19

(canceled)

### Claim 20 (depends on 15)

The method of claim 15, further comprising determining the third temperature and/or the third amount of time.

### Claim 21 (depends on 15)

The method of claim 15, wherein mechanically treating the magnesium alloy based object comprises extrusion, forging, rolling, or a combination thereof the magnesium alloy based object.

### Claim at position 22

22-24. (Canceled)

### Claim 25 (depends on 15)

The method of claim 15, further comprising repeating the thermomechanical treatment.

### Claim 26 (depends on 15)

The method of claim 15, wherein the magnesium alloy based object exhibits improved mechanical properties after thermomechanical treatment.

### Claim 27

(canceled)

### Claim 28 (depends on 1)

The method of claim 1, further comprising determining the first temperature, the first amount of time, the second temperature, the second amount of time, or a combination thereof.

### Claim 29

(canceled)

### Claim 30 (depends on 1)

A magnesium alloy based object made by the method of claim 1.

### Claim 31 (depends on 30)

The magnesium alloy based object of claim 30, wherein the magnesium alloy based object has a yield stress of from 200 to 300 MPa, a ductility of 8-33%, an average thickness of from 1 mm to 4 mm, an average grain size of from 10 μm to 15 μm, or a combination thereof.

### Claim at position 30

32-35. (canceled)

### Claim 36 (depends on 30)

An article of manufacture comprising the magnesium alloy based object of claim 30, the article of manufacture comprising a bone fixation device, a load bearing implant, or a combination thereof.