# US 2022/0275192 A1 · Polyvinyl Alcohol-based Degradable Plastic, Preparation Method Therefor and Application Thereof, and Recycling Method Therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0275192 A1
- Document ID: US20220275192A1
- Status: Published application
- Kind: A1
- Application number: 17/634,560
- Filed: 2020-08-27
- Published: 2022-09-01
- Earliest claimed: 2019-08-27
- Assignees: Jilin University
- Applicants: Jilin University
- Inventors: Junqi Sun; Xu Fang; Yixuan Li
- Web page: https://patentgrep.com/patent/US20220275192A1

## CPC

- C08J 11/06: without chemical reactions
- C08L 29/04: Polyvinyl alcohol; Partially hydrolysed homopolymers or copolymers of esters of unsaturated alcohols with saturated carboxylic acids
- C08F 8/28: Condensation with aldehydes or ketones
- C08F 261/04: on to polymers of vinyl alcohol
- C08G 83/008: {Supramolecular polymers}
- C08J 5/18: Manufacture of films or sheets
- C08J 11/08: using selective solvents for polymer components
- C08J 2329/04: Polyvinyl alcohol; Partially hydrolysed homopolymers or copolymers of esters of unsaturated alcohols with saturated carboxylic acids
- C08L 2201/06: Biodegradable
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

Disclosed in the present invention are a polyvinyl alcohol (PVA)-based degradable plastic, a preparation method therefor and application thereof, and a recycling method therefor. The preparation method comprises the following steps: a PVA solution is subjected to a chemical grafting reaction under an acidic condition under the action of a modifier; there are a phenyl group, an aldehyde group, and at least one group capable of forming a hydrogen bond with PVA in a structural formula of the modifier. The polyvinyl alcohol-based degradable plastic provided in the present invention has the advantages of being high in transparency, high in mechanical strength, not affected by environmental humidity, easy to degrade, good in thermal stability and good in biocompatibility, and has the advantages of recyclability, low costs, easy large-scale preparation and the like.

## Claims

### Claim 1

A preparation method for polyvinyl alcohol-based degradable plastic, wherein the preparation method comprises the following steps: the PVA solution is subjected to a chemical grafting reaction under an acidic condition and under the action of a modifier; there are a phenyl group, an aldehyde group, and at least one group capable of forming a hydrogen bond with PVA in a structural formula of the modifier; the aldehyde group and the group capable of forming a hydrogen bond with PVA respectively substitute the hydrogen on the different carbon atoms on the phenyl group; the group capable of forming a hydrogen bond with PVA is one or more selected from the group consisting of hydroxyl, methoxy, ethoxy, fluoro, carboxy, methoxycarbonyl and methyl; the mole percentage of the modifier with respect to a repeating structural unit of the PVA is 15% to 60%.

### Claim 2 (depends on 1)

The preparation method according to claim 1, wherein, the molecular weight of the modifier is 106-300;
or, the aldehyde group and the group capable of forming a hydrogen bond with PVA substitute the hydrogen on different carbon atoms on the phenyl group by using meta or para substitution.

### Claim 3 (depends on 1)

The preparation method according to claim 1, wherein the molar percentage of the modifier with respect to a repeating structural unit of the PVA is 20%-40%.

### Claim 4 (depends on 1)

The preparation method according to claim 1, wherein the PVA solution is a solution obtained by dissolving PVA in a soluble solvent.

### Claim 5 (depends on 1)

The preparation method according to claim 1, wherein the acidic condition is a strongly acidic condition, an acidic condition with pH of 3 or less;
or, the acidic condition is achieved by using a pH regulator.

### Claim 6 (depends on 1)

The preparation method according to claim 1, wherein after the chemical grafting reaction, a post-treatment is further performed;
the post-treatment comprises carrying out drying in form of coating film or melt-blowing film forming for the reaction solution.

### Claim 7 (depends on 1)

A polyvinyl alcohol-based degradable plastic prepared by the preparation method according to claim 1.

### Claim 8 (depends on 7)

An application of the polyvinyl alcohol-based degradable plastic according to claim 7.

### Claim 9 (depends on 7)

A recycling method for the polyvinyl alcohol-based degradable plastic according to claim 7, wherein it comprises the following steps: completely dissolving the polyvinyl alcohol-based degradable plastics in a soluble solvent.

### Claim 10 (depends on 9)

The recycling method according to claim 9, wherein the soluble solvent is dimethyl sulfoxide, or a mixed solvent formed by dimethyl sulfoxide and water;
or, the dissolving is performed at room temperature;
or, after the completely dissolving, a post-treatment is further performed; the post-treatment comprises carrying out drying in form of coating film or melt-blowing film forming for the reaction solution.

### Claim 11 (depends on 1)

The preparation method according to claim 1, wherein, the modifier is one or more selected from the group consisting of p-hydroxybenzaldehyde, 3,4-dihydroxybenzaldehyde, vanillin, ethyl vanillin, 4-fluorobenzaldehyde, p-aldehyde benzoic acid, m-aldehyde benzoic acid, 4-dimethylaminobenzaldehyde, methyl p-formyl benzoate and p-tolualdehyde.

### Claim 12 (depends on 11)

The preparation method according to claim 11, wherein, the modifier is p-formyl benzoic acid, or methyl p-formyl benzoate, or m-formyl benzoic acid, or a combination of p-methylbenzaldehyde and ethyl vanillin.

### Claim 13 (depends on 12)

The preparation method according to claim 12, wherein, when the modifier is a combination of p-tolualdehyde and ethyl vanillin, the molar ratio of p-tolualdehyde and ethyl vanillin is 1:1-1:3.

### Claim 14 (depends on 4)

The preparation method according to claim 4, wherein, the mass percentage of PVA in the PVA solution is 6%-11%.

### Claim 15 (depends on 4)

The preparation method according to claim 4, wherein, the molecular weight of PVA is 40,000 to 140,000.

### Claim 16 (depends on 4)

The preparation method according to claim 4, wherein, the soluble solvent is dimethyl sulfoxide, or a mixed solvent formed by dimethyl sulfoxide and water.

### Claim 17 (depends on 4)

The preparation method according to claim 4, wherein, the dissolving is carried out at 70-90° C.

### Claim 18 (depends on 5)

The preparation method according to claim 5, wherein, the acidic condition is an acidic condition with pH of 1;
or, the acidic condition is achieved by using a pH regulator, and the pH regulator is preferably hydrochloric acid.

### Claim 19 (depends on 5)

The preparation method according to claim 5, wherein, the temperature of the chemical grafting reaction is 70-90° C.;
or, the time of the chemical grafting reaction is 1-3 h.

### Claim 20 (depends on 6)

The preparation method according to claim 6, wherein, the temperature of drying in form of coating film is 60-120° C., and the time is 10 min-30 min;
or, the temperature of the melt-blowing film forming is 160-190° C.