# US 2022/0275191 A1 · Resin powder and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0275191 A1
- Document ID: US20220275191A1
- Status: Published application
- Kind: A1
- Application number: 17/630,823
- Filed: 2020-07-27
- Published: 2022-09-01
- Earliest claimed: 2019-07-30
- Assignees: Kuraray Co., Ltd.
- Applicants: Kuraray Co., Ltd.
- Inventors: Shinsuke NII
- Web page: https://patentgrep.com/patent/US20220275191A1

## CPC

- C08L 29/04: Polyvinyl alcohol; Partially hydrolysed homopolymers or copolymers of esters of unsaturated alcohols with saturated carboxylic acids
- B29B 9/12: characterised by structure or composition
- B29B 9/16: Auxiliary treatment of granules
- C08J 3/12: Powdering or granulating
- C08J 3/124: {Treatment for improving the free-flowing characteristics}
- B29B 9/02: by dividing preformed material
- B29B 2009/125: {Micropellets, microgranules, microparticles}
- B29B 2009/166: {Deforming granules to give a special form, e.g. spheroidizing, rounding}
- C08F 8/12: Hydrolysis
- C08F 216/06: Polyvinyl alcohol {; Vinyl alcohol}
- C08J 2329/04: Polyvinyl alcohol; Partially hydrolysed homopolymers or copolymers of esters of unsaturated alcohols with saturated carboxylic acids
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

A resin powder may be superior in passability through pipes and silos, and a method may produce such a resin powder. The resin powder contains a vinyl alcohol polymer, an average particle diameter thereof is 100 to 2,000 μm, and an average value PA of a roundness P by formula (1), of 50 particles arbitrarily extracted from the particles of the resin powder having a particle diameter of 100 to 1,000 μm, is 0.1 to 0.8. P=(Σi=1Nri)/NR (1) ri being a radius of curvature of each particle corner of the 50 particles; R being a maximum inscribed circle radius of the particle; and N being a number of particle corners. If the number of particle corners is 9 or more, the radii of curvature of eight corners, in increasing order from a smallest radius of curvature, are adopted, and N is 8.

## Claims

### Claim 1

A resin powder, consisting of particles,
wherein the resin powder comprises a vinyl alcohol polymer,
wherein an average particle diameter of the particles is in a range of from 100 to 2,000 μm, and
wherein an average value PA of a roundness P, by formula (1), of 50 particles arbitrarily extracted from the particles of the resin powder having a particle diameter in a range of from 100 to 1,000 μm, is in a range of from 0.1 to 0.8:
P=(Σi=1Nri)/NR (1),
wherein, in the formula (1),
ri is a curvature radius of each corner of a particle of the 50 particles arbitrarily extracted,
R is a maximum inscribed circle radius of the particle, and
N is a number of corners of the particle,
wherein, when a number of corners of the particle is 9 or more, radii of curvature of eight corners, in increasing order from a smallest radius of curvature, are adopted, and N is set to 8.

### Claim 2 (depends on 1)

The powder of claim 1, wherein the vinyl alcohol polymer has a viscosity-average degree of polymerization in a range of from 200 to 5,000, and
wherein the vinyl alcohol polymer a degree of saponification in a range of from 35 to 99.99 mol %.

### Claim 3 (depends on 1)

The powder of claim 1, wherein the average particle diameter is in a range of from 100 to 1,000 μm, and satisfying inequality (2):
PA×S≥18 (2),
wherein, in the inequality (2), S is a degree of saponification (mol %) of the vinyl alcohol polymer.

### Claim 4 (depends on 1)

The powder of claim 1, wherein a percentage content of particles which have a particle diameter of 100 to 1,000 μm is 50% by mass or more.

### Claim 5 (depends on 1)

A method for producing the resin powder of claim 1, the method comprising:
grinding a resin solid comprising the vinyl alcohol polymer to obtain a coarse powder; and
processing surfaces of the coarse powder.

### Claim 6

A resin powder, comprising particles,
wherein the resin powder comprises a vinyl alcohol polymer,
wherein an average particle diameter of the particles is in a range of from 100 to 2,000 μm, and
wherein an average value PA of a roundness P, by formula (1), of 50 particles arbitrarily extracted from the particles of the resin powder having a particle diameter in a range of from 100 to 1,000 μm is in a range of from 0.1 to 0.8:
P=(Σi=1Nri)/NR (1),
wherein, in the formula (1),
ri is a curvature radius of each corner of a particle of the 50 particles arbitrarily extracted;
R is a maximum inscribed circle radius of the particle; and
N is a number of corners of the particle,
wherein, when a number of corners of the particle is 9 or more, radii of curvature of eight corners, in increasing order from a smallest radius of curvature, are adopted, and N is set to 8.

### Claim 7 (depends on 6)

The powder of claim 6, wherein the vinyl alcohol polymer has a viscosity-average degree of polymerization in a range of from 200 to 5,000, and
wherein the vinyl alcohol polymer has a degree of saponification in a range of from 35 to 99.99 mol %.

### Claim 8 (depends on 6)

The powder of claim 6, wherein the average particle diameter is in a range of from 100 to 1,000 μm, and satisfying inequality (2):
PA×S≥18 (2),
wherein, in the inequality (2), S is a degree of saponification (mol %) of the vinyl alcohol polymer.

### Claim 9 (depends on 6)

The powder of claim 6, wherein a percentage content of particles having a particle diameter in a range of from 100 to 1,000 μm is 50% by mass or more.

### Claim 10 (depends on 1)

A method for producing the resin powder of claim 1, the method comprising:
grinding a resin solid comprising the vinyl alcohol polymer to obtain a coarse powder; and
processing surfaces of the coarse powder.