# US 2022/0274173 A1 · Three-dimensional printing with stainless steel particles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0274173 A1
- Document ID: US20220274173A1
- Status: Published application
- Kind: A1
- Application number: 17/637,477
- Filed: 2019-10-23
- Published: 2022-09-01
- Earliest claimed: 2019-10-23
- Assignees: Hewlett-Packard Development Company, L.P.
- Applicants: Hewlett-Packard Development Company, L.P.
- Inventors: Pavan Suri; Mackensie Smith; James McKinnell
- Web page: https://patentgrep.com/patent/US20220274173A1

## CPC

- C22C 33/0285: {with Cr, Co, or Ni having a minimum content higher than 5%}
- B22F 3/1007: {Atmosphere (B22F3/1021 takes precedence)}
- B22F 10/14: by jetting of binder onto a bed of metal powder
- B29C 64/165: using a combination of solid and fluid materials, e.g. a powder selectively bound by a liquid binder, catalyst, inhibitor or energy absorber
- B29C 64/295: Heating elements
- B33Y 10/00: Processes of additive manufacturing
- B33Y 30/00: Apparatus for additive manufacturing; Details thereof or accessories therefor
- B33Y 40/20: Post-treatment, e.g. curing, coating or polishing
- B33Y 70/00: Materials specially adapted for additive manufacturing
- B33Y 70/10: Composites of different types of material, e.g. mixtures of ceramics and polymers or mixtures of metals and biomaterials
- C22C 38/42: with copper
- C22C 38/48: with niobium or tantalum
- B22F 1/05: Metallic powder characterised by the size or surface area of the particles
- B22F 2301/35: Iron
- B22F 2304/10: Micron size particles, i.e. above 1 micrometer up to 500 micrometer
- B22F 2998/10: Processes characterised by the sequence of their steps
- Y02P 10/25: Process efficiency
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Three-dimensional printing can include iteratively applying build material layers including stainless steel particles, iteratively applying a binding agent to individual build material layers to define individually patterned object layers that become adhered to one another to form a layered green body object, and sintering the layered green body object in a sintering oven. The stainless steel particles can include from about (2) wt % to about (6) wt % nickel, from about (14) wt % to about (19) wt % chromium, from about (2) wt % to about (6) wt % copper, and up to about (700) ppm carbon. Sintering can include ramping up the temperature to about (1240)° C. to about (1320)° C., pausing for about (30) minutes to about (12) hours, and ramping up the temperature to about (1350)° C. to about (1400)° C. for (10) minutes to about (6) hours.

## Claims

### Claim 1

A method of three-dimensional printing comprising:
iteratively applying individual build material layers a particulate build material including from about 80 wt % to 100 wt % stainless steel particles, wherein the stainless steel particles include from about 2 wt % to about 6 wt % nickel, from about 14 wt % to about 19 wt % chromium, from about 2 wt % to about 6 wt % copper, and up to about 700 ppm carbon;
based on a three-dimensional object model, iteratively applying a binding agent to individual build material layers to define individually patterned object layers that become adhered to one another to form a layered green body object; and
sintering the layered green body object in a sintering oven by:
ramping up a temperature of the sintering oven to a densification temperature of about 1240° C. to about 1320° C.,
pausing the ramping up of the temperature at the densification temperature for about 30 minutes to about 12 hours, and
ramping up the temperature of the sintering oven after pausing from the densification temperature to a fusing temperature of about 1350° C. to about 1400° C. for 10 minutes to about 6 hours to form a fused three-dimensional object.

### Claim 2 (depends on 1)

The method of claim 1, wherein the stainless steel particles have a D50 particle size from about 6 μm to about 25 μm.

### Claim 3 (depends on 1)

The method of claim 1, wherein the stainless steel particles include from about 3 wt % to about 5 wt % nickel; from about 15 wt % to about 17 wt % chromium; from about 3 wt % to about 5 wt % copper; and from about 0.15 wt % to about 0.45 wt % niobium, tantalum, or a combination of niobium and tantalum.

### Claim 4 (depends on 1)

The method of claim 1, wherein sintering occurs in an atmosphere including from about 1 wt % to 100 wt % hydrogen gas.

### Claim 6 (depends on 1)

The method of claim 1, wherein the sintering includes reducing the pressure in a sintering oven to a vacuum ranging from about 1 Torr to about 730 Torr.

### Claim 7 (depends on 1)

The method of claim 1, wherein the fused three-dimensional object has from about 0.5% to about 5% porosity by volume.

### Claim 8 (depends on 1)

The method of claim 1, wherein the fused three-dimensional object has a density ranging from about 7.5 g/cm3to about 7.8 g/cm3.

### Claim 8 (depends on 1)

The method of claim 1, wherein ramping up the temperature of the sintering oven to a densification temperature and ramping up the temperature from the densification temperature to the fusing temperature is at an average rate of about 2° C. to about 20° C. per minute.

### Claim 9

A three-dimensional printing kit comprising:
a particulate build material including from about 80 wt % to 100 wt % stainless steel particles, wherein the stainless steel particles include from about 2 wt % to about 6 wt % nickel, from about 14 wt % to about 19 wt % chromium, from about 2 wt % to about 6 wt % copper, and up to about 700 ppm carbon; and
a binding agent including binder particles dispersed in a liquid vehicle.

### Claim 10 (depends on 9)

The three-dimensional printing kit of claim 9, wherein the stainless steel particles have a D50 particle size from about 6 μm to about 25 μm.

### Claim 11 (depends on 9)

The three-dimensional printing kit of claim 9, wherein the stainless steel particles have a D90 particle size from about 10 μm to about 35 μm.

### Claim 12 (depends on 9)

The three-dimensional printing kit of claim 9, wherein the stainless steel particles include from about 3 wt % to about 5 wt % nickel, from about 15 wt % to about 17 wt % chromium, from about 3 wt % to about 5 wt % copper, and from about 0.15 wt % to about 0.45 wt % niobium, tantalum, or a combination of niobium and tantalum.

### Claim 13

A three-dimensional printing system comprising:
a particulate build material including from about 80 wt % to 100 wt % stainless steel particles including from about 2 wt % to about 6 wt % nickel, from about 14 wt % to about 19 wt % chromium, from about 2 wt % to about 6 wt % copper, and up to about 700 ppm carbon;
a binding agent applicator fluidly coupled or coupleable to a binding agent to iteratively apply the binding agent to the particulate build material to form individually patterned object layers of a green body object;
a sintering oven to receive and heat the green body object to cause the green body object to become fused; and
a hardware controller to generate a command to:
ramp up the temperature of the sintering oven to a densification temperature of about 1240° C. to about 1320° C.,
pause the ramping up of the temperature at the densification temperature for about 30 minutes to about 12 hours, and
ramp up the temperature of the sintering oven after pausing from the densification temperature to a fusing temperature of about 1350° C. to about 1400° C. for 10 minutes to about 6 hours to form a fused three-dimensional object.

### Claim 14 (depends on 13)

The three-dimensional printing system of claim 13, further comprising a binding agent applicator fluidly coupled or coupleable to the binding agent to iteratively apply the binding agent to the particulate build material to form the individually patterned object layers of the green body object.

### Claim 15 (depends on 13)

The system of claim 13, further comprising a build platform to support the particulate build material, wherein the build platform is positioned to receive the binding agent from the binding agent applicator onto a layer of the particulate build material.