# US 2022/0274107 A1 · Detection chip and modification method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0274107 A1
- Document ID: US20220274107A1
- Status: Published application
- Kind: A1
- Application number: 17/631,463
- Filed: 2021-03-04
- Published: 2022-09-01
- Earliest claimed: 2020-03-19
- Assignees: Boe Technology Group Co., Ltd.
- Applicants: BOE Technology Group Co., Ltd.
- Inventors: Yudan YIN; Jing YU; Haonan LIU; Zhukai LIU
- Web page: https://patentgrep.com/patent/US20220274107A1

## CPC

- B01L 3/502707: {characterised by the manufacture of the container or its components}
- C03C 17/42: at least one coating of an organic material and at least one non-metal coating
- C03C 17/28: with organic material (C03C17/34, C03C17/44 take precedence)
- C03C 17/30: with silicon-containing compounds
- G01N 33/543: with an insoluble carrier for immobilising immunochemicals
- B01L: CHEMICAL OR PHYSICAL LABORATORY APPARATUS FOR GENERAL USE
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

Disclosed are a detection chip and a modification method therefor. The method for modifying the detection chip comprises performing a surface film-forming treatment on a hydrophilic layer on a first substrate constituting the detection chip to form polydopamine film on a surface of the hydrophilic layer; and adopting a buffer solution containing sodium hyaluronate to perform a surface carboxylation treatment on the hydrophilic layer, on the surface of which the polydopamine film has been formed, in order to form a carboxyl-containing modification group on the surface of the hydrophilic layer.

## Claims

### Claim 1

A modification method of a detection chip, comprising:
forming a polydopamine film on a surface of the hydrophilic layer by adopting a dopamine-containing buffer solution to perform surface film-forming treatment on the hydrophilic layer on a first substrate constituting the detection chip, wherein the hydrophilic layer covers sample application platforms located on the first substrate; and
forming a carboxyl-containing modification group on a surface of the hydrophilic layer by adopting a buffer solution containing sodium hyaluronate to perform a surface carboxylation treatment on the hydrophilic layer with the polydopamine film.

### Claim 2 (depends on 1)

The modification method according to claim 1, wherein a mass concentration ratio of the dopamine to the sodium hyaluronate is 1:1-1:5.

### Claim 3 (depends on 2)

The modification method according to claim 2, wherein the adopting the dopamine-containing buffer solution to perform the surface film-forming treatment on the hydrophilic layer on the first substrate constituting the detection chip, comprises:
obtaining the buffer solution of the dopamine by weighing and taking 500 mg of dopamine to be dissolved in 250 mL of Tris-HCI, the Tris-HCI is of a pH value being 7-9 and a concentration being 10 mM;
putting the first substrate with the hydrophilic layer into the buffer solution of the dopamine to be subjected to still standing at a room temperature for a reaction for 12 h-24 h.

### Claim 4 (depends on 2)

The modification method according to claim 2, wherein the adopting the buffer solution containing the sodium hyaluronate to perform the surface carboxylation treatment on the hydrophilic layer with the polydopamine film, comprises:
obtaining the buffer solution of the sodium hyaluronate by weighing and taking 1.25 g of sodium hyaluronate to be dissolved in 250 mL of Tris-HCI, the Tris-HCI is of a pH value being 7-9 and a concentration being 10 mM; and
putting the first substrate with the polydopamine film formed on the surface of the hydrophilic layer into the buffer solution of the sodium hyaluronate, to be subjected to still standing under a temperature condition of 20° C.-40° C. for a reaction for 12 h-24 h.

### Claim 5 (depends on 1)

The modification method according to claim 1, wherein before the performing the surface film-forming treatment on the hydrophilic layer on the first substrate constituting the detection chip, the modification method further comprises:
forming the carboxyl-containing modification group on the surface of the hydrophilic layer by performing surface activation treatment on the hydrophilic layer on the first substrate.

### Claim 6 (depends on 5)

The modification method according to claim 5, wherein the performing the surface activation treatment on the hydrophilic layer on the first substrate, comprises:
putting the first substrate with the hydrophilic layer into a piranha solution, to be soaked under a temperature condition of 70° C.-90° C. for 12 h-24 h, wherein the piranha solution comprises concentrated sulfuric acid and 30% hydrogen peroxide, and a volume ratio of the concentrated sulfuric acid to the 30% hydrogen peroxide is 1:3.

### Claim 7 (depends on 5)

The modification method according to claim 5, wherein after the surface activation treatment, the surface film-forming treatment and the surface carboxylation treatment, following treatment is performed on the first substrate:
cleaning the first substrate for at least three times by adopting deionized water, and then blowing-drying the first substrate through nitrogen for standby application.

### Claim 8 (depends on 5)

The modification method according to claim 5, wherein before the performing the surface activation treatment on the hydrophilic layer on the first substrate, the modification method further comprises:
ultrasonic-cleaning the first substrate with the hydrophilic layer by sequentially adopting acetone, ethyl alcohol and deionized water as a solution, and blow-drying ultrasonic-cleaned first substrate for standby application.

### Claim 9 (depends on 8)

The modification method according to claim 8, wherein before the ultrasonic-cleaning the first substrate with the hydrophilic layer, the modification method further comprises:
forming the plurality of sample application platforms on the first substrate; and
respectively forming the hydrophilic layers on the sample application platforms.

### Claim 10 (depends on 9)

The modification method according to claim 9, wherein the respectively forming the hydrophilic layers on the sample application platforms, comprises:
depositing a silicon oxide layer with a thickness being 300 nm on a layer where the sample application platforms are located, by adopting a plasma enhanced chemical vapor deposition, under a temperature condition of 390° C.; and
obtaining the hydrophilic layer by etching the silicon oxide layer, and reserving a silicon oxide layer covering a region where all the sample application platforms are located to.

### Claim 11 (depends on 1)

A detection chip, comprising:
a first substrate;
sample application platforms, located on the first substrate; and
a hydrophilic layer, located on the first substrate and covering the sample application platforms, wherein a surface of the hydrophilic layer comprises a carboxyl-containing modification group, and
the carboxyl-containing modification group is obtained by adopting the modification method according to claim 1.

### Claim 12 (depends on 11)

The detection chip according to claim 11, further comprising:
a diversion dam, located on the first substrate, wherein the diversion dam extends in a first path and located between adjacent sample application platforms; and
the hydrophilic layer covers the diversion dam, and a part, covering the diversion dam, of the hydrophilic layer and a part, covering the sample application platforms, of the hydrophilic layer are mutually independent.

### Claim 13 (depends on 12)

The detection chip according to claim 12, wherein a height of the diversion dam in a direction perpendicular to the first substrate is greater than a height of the sample application platforms in the direction perpendicular to the first substrate.

### Claim 14 (depends on 12)

The detection chip according to claim 12, further comprising:
a hydrophobic layer, located on the first substrate, wherein the sample application platforms and the diversion dam are located on the hydrophobic layer.

### Claim 15 (depends on 1244)

The detection chip according to any one of claims 1244, further comprising:
a second substrate, disposed opposite to the first substrate, and spaced from the first substrate so as to provide a detection space.

### Claim 16 (depends on 15)

The detection chip according to claim 15, wherein at least one of the first substrate or the second substrate is a glass substrate.

### Claim 17 (depends on 16)

The detection chip according to claim 16, further comprising:
sealant, located between the first substrate and the second substrate, and surrounds the diversion dam and the plurality of sample application platforms.