# US 2022/0266490 A1 · Method for manufacturing an injection-molded article, in particular a bottle preform

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0266490 A1
- Document ID: US20220266490A1
- Status: Published application
- Kind: A1
- Application number: 17/618,227
- Filed: 2020-06-10
- Published: 2022-08-25
- Earliest claimed: 2019-06-14
- Assignees: L'oreal
- Applicants: L'oreal
- Inventors: Jean-Marie HERVET; Judith VENIEZ; Aurelien PETIT; Olivier FARNAULT
- Web page: https://patentgrep.com/patent/US20220266490A1

## CPC

- B29B 11/08: Injection moulding
- B29C 45/7207: {of the moulded articles}
- B29B 11/14: characterised by structure or composition
- B29C 45/0001: {characterised by the choice of material}
- B29C 49/0005: {characterised by the material}
- B29C 49/06: Injection blow-moulding
- B29C 49/071: {Preforms or parisons characterised by their configuration, e.g. geometry, dimensions or physical properties}
- B29C 49/12: Stretching rods
- B29C 49/6452: {by heating the neck}
- B29C 49/6472: {in several stages}
- B29C 2045/7264: {Cooling or heating the neck portion of preforms}
- B29C 2049/023: {using inherent heat of the preform, i.e. 1 step blow moulding}
- B29C 2049/065: {Means for compensating or avoiding the shrinking of preforms, e.g. in the injection mould or outside the injection mould}
- B29C 2945/76625: Humidity, moisture
- B29C 2945/76903: After-treatment
- B29C 2949/0715: the preform having one end closed
- B29C 2949/0862: Crystallinity
- B29C 2949/0863: at the neck portion
- B29K 2995/004: Semi-crystalline
- B29K 2995/0093: hydrophobic
- B29L 2031/7142: {Aerosol containers}
- B29L 2031/7158: {Bottles}
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

A method for manufacturing an injection-molded article, preferably a preform (11) of a bottle (1), in particular an aerosol bottle, made of a crystallizable polymer material, this article having at least one crystallized part (3), in particular a neck, and preferably a tubular body (14) closed at one end (16), the method comprising the following steps: a) producing an injection-molded article, preferably an injection-molded preform (11), by injecting the crystallizable polymer into a mold, b) crystallizing said part (3) of the injection-molded article, in particular of the injection-molded preform, by heating and then cooling the latter, wherein, in said method, between step a) and step b), the injection-molded article, in particular the injection-molded preform (11), is held for a sufficient duration under storage conditions such that it undergoes moisture uptake of at least 0.4% by weight.

## Claims

### Claim at position 1

1: A method for manufacturing an injection-molded article made of a crystallizable polymer material, the article having at least one crystallized part, the method comprising:
a) producing an injection-molded article by injecting the crystallizable polymer into a mold,
b) crystallizing the injection-molded article by heating and then cooling the injection-molded article,
wherein, in said method, between a) and b), the injection-molded article is held for a sufficient duration under storage conditions such that it undergoes moisture uptake of at least 0.4% by weight.

### Claim at position 2 (depends on 1)

2: The method as claimed in claim 1, wherein the relative humidity of the storage conditions is at least 30%.

### Claim at position 3 (depends on 1)

3: The method as claimed in claim 1, wherein the relative humidity of the storage conditions at least 60%.

### Claim at position 4 (depends on 1)

4: The method as claimed in claim 1, wherein the relative humidity of the storage conditions is at least 80%.

### Claim at position 5 (depends on 1)

5: The method as claimed in claim 1, wherein the duration under storage conditions is at least 7 days.

### Claim at position 6 (depends on 1)

6: The method as claimed in claim 1, wherein the storage duration under conditions is at least 15 days.

### Claim at position 7 (depends on 1)

7: The method as claimed in claim 1, wherein the temperature of the storage conditions is between 5° C. and 35° C.

### Claim at position 8 (depends on 1)

8: The method as claimed claim 1, wherein the injection-molded article is stored in a large bag during the moisture uptake.

### Claim at position 9 (depends on 1)

9: The method as claimed in claim 1, wherein the crystallizable polymer material is polyethylene terephthalate (PET).

### Claim at position 10 (depends on 1)

10: The method as claimed in claim 1, wherein the crystallization is carried out with the aid of a heating device.

### Claim at position 11 (depends on 1)

11: The method as claimed in claim 1, wherein the injection-molded article is a preform of a bottle.

### Claim at position 12 (depends on 11)

12: The method as claimed in claim 11, wherein said crystallized part is the neck of the bottle preform.

### Claim at position 13 (depends on 11)

13: The method as claimed in claim 11, wherein said bottle is an aerosol bottle.

### Claim at position 14 (depends on 11)

14: The method as claimed in claim 11, wherein said bottle is a pump-action bottle.

### Claim 15 (depends on 1)

A method for manufacturing a bottle, wherein the bottle is formed by stretch-blow-molding the injection-molded article having a crystallized part obtained by the method as claimed in claim 1.

### Claim at position 16 (depends on 1)

16: The method as claimed in claim 1, wherein said injection-molded article has a tubular body closed at one end.

### Claim at position 17 (depends on 1)

17: The method as claimed in claim 1 wherein the temperature of the storage conditions is between 15° C. and 25° C.

### Claim at position 18 (depends on 10)

18: The method as claimed in claim 10, wherein the heating device comprises at least one infrared radiation lamp.

### Claim at position 19 (depends on 1)

19: The method as claimed in claim 1 wherein the storage duration is at least one month.

### Claim at position 20 (depends on 10)

20: The method as claimed in claim 10, wherein at least one cooling bar is brought close to the preform from the inside or outside thereof, simultaneously with the heating.