# US 2022/0266332 A1 · Creep resistant Ni-based superalloy casting and method of manufacture for advanced high-temparature applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0266332 A1
- Document ID: US20220266332A1
- Status: Published application
- Kind: A1
- Application number: 17/184,542
- Filed: 2021-02-24
- Published: 2022-08-25
- Earliest claimed: 2021-02-24
- Assignees: United States Department of Energy
- Applicants: United States Department of Energy
- Inventors: Paul D. Jablonski; Jeffrey Hawk; Martin Detrois
- Web page: https://patentgrep.com/patent/US20220266332A1

## CPC

- B22D 25/06: by its physical properties (B22D27/00 takes precedence)
- B22D 18/06: Vacuum casting, i.e. making use of vacuum to fill the mould
- B22D 21/025: {Casting heavy metals with high melting point, i.e. 1000 - 1600 degrees C, e.g. Co 1490 degrees C, Ni 1450 degrees C, Mn 1240 degrees C, Cu 1083 degrees C}
- C22C 19/05: with chromium
- C22F 1/10: of nickel or cobalt or alloys based thereon
- F27B 14/061: {Induction furnaces}
- F27B 14/10: Crucibles
- C22C 2202/00: Physical properties
- F27B 2014/066: {Construction of the induction furnace}
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- F27B: FURNACES, KILNS, OVENS OR RETORTS IN GENERAL; OPEN SINTERING OR LIKE APPARATUS

## Abstract

One or more embodiments relates to a method of casting a creep-resistant Ni-based superalloy and a homogenization heat treatment for the alloy, The method includes forming a feed stock having Nickel (Ni) and at least one of Chromium (Cr), Cobalt (Co), Aluminum (Al), Titanium (Ti), Niobium (Nb), Iron (Fe), Carbon (C), Manganese (Mn), Molybdenum (Mo), Silicon (Si), Copper (Cu), Phosphorus (P), Sulfur (S) and Boron (B). The method further includes fabricating the creep-resistant Ni-based superalloy in a predetermined shape using the feed stock and at least one process such as vacuum induction melting (VIM), electroslag remelting (ESR) and/or vacuum arc remelting (VAR).

## Claims

### Claim 1

A method of casting a creep-resistant Ni-based superalloy, the method comprising: forming a feed stock comprising Nickel (Ni) and at least one of Chromium (Cr), Cobalt (Co): Aluminum (Al), Titanium (Ti), Niobium (Nb), Iron (Fe), Carbon (C), Manganese (Mn), Molybdenum (Mo), Silicon (Si), Copper (Cu), Phosphorus (P), Sulfur (S) and Boron (B);
fabricating an as-cast article comprising creep-resistant Ni-based superalloy in a predetermined shape using the feed stock and at least one process comprising vacuum induction melting (VIM), electroslag remelting (ESR) and/or vacuum arc remelting (VAR); and
homogenizing the as-cast article wherein homogenizing the as-cast article comprises a heating sequence of one hour at about 1075° C., three hours at about 1125° C., eight hours at about 1200° C. and eight hours at about 1250° C.

### Claim 2 (depends on 1)

The method of claim 1, wherein the feed stock comprises at least Nickel (Ni) and Chromium (Cr).

### Claim 3 (depends on 1)

The method of claim 1 wherein fabricating (he creep-resistant Ni-based superalloy comprises:
melting the feed stock in a furnace, forming a liquid metal;
pouring the liquid metal into a preheated mold, forming a molten metal; and
solidifying the molten metal in the preheated mold, forming the as-cast article.

### Claim 4 (depends on 3)

The method of claim 3 wherein homogenizing the as-cast article further comprises forming a controlled and random dispersal of alloy constituents that reduces chemical segregation within the as-cast article.

### Claim 5 (depends on 4)

The method of claim 4 wherein the homogenizing the as-cast article forms a specific element segregation below ±1% variation from the nominal chemistry of these elements throughout the as-cast article.

### Claim 6

(canceled)

### Claim 7 (depends on 4)

The method of claim 4 further comprises loading the feed stock into a crucible inside the furnace.

### Claim 8 (depends on 7)

The method of claim 7 further comprises loading the feed stock into a zirconia crucible inside the furnace, forming a loaded feedstock.

### Claim 9 (depends on 3)

The method of claim 3 wherein the furnace comprises a VIM furnace.

### Claim 10 (depends on 3)

The method of claim 3 wherein melting the feed stock is carried out in at least one of a vacuum and at a partial pressure between 50 and 400 Torr of Argon (Ar).

### Claim 11 (depends on 3)

The method of claim 3 wherein melting the metal Ni-based superalloy includes pouring the liquid metal into preheated mold when the temperature of the liquid metal is between 1 and 10 degrees Celsius above the melting temperature of the loaded feed stock.

### Claim 12 (depends on 3)

The method of claim 3 wherein the preheated mold is a graphite mold.

### Claim 13 (depends on 3)

The method of claim 3 wherein the preheated mold includes a zirconia washcoat and is preheated prior to being placed in the furnace.

### Claim 14 (depends on 3)

The method of claim 3 wherein the preheated mold is heated to about 300° C. to about 700° C. from about 10 minutes to about 5 hours.

### Claim 15

(canceled)

### Claim 16 (depends on 1)

The method of claim 1 wherein the cast alloy is characterizable by a level of chemical homogeneity, defined as variations between local and nominal chemistry following homogenizing and measured using wavelength dispersive x-ray fluorescence, of less than ±1%, or less than ±2%, or less than ±5%.

### Claim 17

A method of casting a creep-resistant Ni-based superalloy, the method comprising:
loading the feed stock comprising Nickel (Ni) and at least one of Chromium (Cr), Cobalt (Co), Aluminum (Al), Titanium (Ti), Niobium (Nb), Iron (Fe), Carbon (C) Manganese (Mn), Molybdenum (Mo), Silicon (Si), Copper (Cu), Phosphorus (P), Sulfur (S) and Boron (B) into a crucible inside a VIM furnace;
melting the feed stock forming a liquid metal, wherein the melting is performed in at least one of a vacuum and at a partial pressure between 50 and 400 Torr of Argon (Ar);
pouring the liquid metal into a preheated mold in the VIM furnace, forming a molten metal; and
solidifying the molten metal in the preheated mold, forming an as-cast article of the creep-resistant Ni-based superalloy in a predetermined shape.

### Claim 18 (depends on 17)

The method of claim 17 further comprising homogenizing the as-cast article in a vacuum heat treatment furnace using a computationally optimized homogenization heat treatment cycle, forming a controlled and random dispersal of alloy constituents that significantly reduces chemical segregation within the as-cast article.

### Claim 19 (depends on 18)

The method of claim 18 wherein the homogenizing the as-cast article forms a specific element segregation below ±1% variation from the nominal chemistry of these elements throughout the as-cast article.

### Claim 20 (depends on 18)

The method of claim 18 wherein the homogenizing the as-cast article comprises a sequence of one hour at about 1075° C., three hours at about 1125° C., eight hours at about 1200° C. and eight hours at about 1250° C.

### Claim 21 (depends on 17)

The method of claim 17 wherein melting the metal Ni-based superalloy includes pouring the liquid metal into the crucible when the temperature of the liquid metal is between 1 and 10 degrees Celsius above the melting temperature of the loaded feed stock.

### Claim 22 (depends on 17)

The method of claim 17 wherein the preheated mold is heated to about 300° C. to about 700° C. from about 10 minutes to about 5 hours.

### Claim 23 (depends on 17)

The method of claim 17 wherein the cast alloy is subjected to a homogenization heat treatment comprising at least two of the sequential steps of treating the cast alloy: 0.5 to 5 hours at 1075±25° C.; 1.5 to 3 hours at 1125±25° C.; 3 to 15 hours at 1200±25° C.; 3 to 24 hours at 1250±25° C.

### Claim 24 (depends on 23)

The method of claim 23 wherein the cast alloy is characterizable by a level of chemical homogeneity, defined as variations between local and nominal chemistry following homogenizing and measured using wavelength dispersive x-ray fluorescence, of less than ±1%, or less than ±2%, or less than ±5%.

### Claim 25 (depends on 1)

The method of claim 1 wherein the as-cast article comprises a equiaxed region with an average grain size of 289±42 μm.

### Claim 26

A method of casting a creep-resistant Ni-based superalloy, the method comprising:
forming a feed stock comprising Nickel (Ni) and at least one of Chromium (Cr), Cobalt (Co), Aluminum (Al), Titanium (Ti), Niobium (Nb), Iron (Fe), Carbon (C), Manganese (Mn), Molybdenum (Mo), Silicon (Si), Copper (Cu), Phosphorus (P), Sulfur (S) and Boron (B); and
fabricating an as-cast article comprising creep-resistant Ni-based superalloy in a predetermined shape using the feed stock and at least one process comprising vacuum induction melting (VIM), electroslag remelting (ESR) and/or vacuum arc remelting (VAR), wherein fabricating the creep-resistant Ni-based superalloy comprises,
melting the feed stock in a furnace, forming a liquid metal;
pouring the liquid metal into a preheated mold, forming a molten metal;
solidifying the molten metal in the preheated mold, forming the as-cast article; and
homogenizing the as-cast article, wherein homogenizing the as-cast article comprises a heating sequence of one hour at about 1075° C., three hours at about 1125° C., eight hours at about 1200° C. and eight hours at about 1250° C., wherein the homogenizing the as-cast article forms a specific element segregation below ±1% variation from the nominal chemistry of these elements throughout the as-cast article.

### Claim 27 (depends on 26)

The method of claim 26 wherein the as-cast article comprises a equiaxed region with an average grain size of 289±42 μm.

### Claim 28

A method of casting a creep-resistant Ni-based superalloy, the method comprising:
forming a feed stock comprising Nickel (Ni) and at least one of Chromium (Cr), Cobalt (Co), Aluminum (Al), Titanium (Ti), Niobium (Nb), Iron (Fe), Carbon (C), Manganese (Mn), Molybdenum (Mo), Silicon (Si), Copper (Cu), Phosphorus (P), Sulfur (S) and Boron (B); and
fabricating an as-cast article comprising creep-resistant Ni-based superalloy in a predetermined shape using the feed stock and at least one process comprising vacuum induction melting (VIM), electroslag remelting (ESR) and/or vacuum arc remelting (VAR), wherein fabricating the creep-resistant Ni-based superalloy comprises,
melting the feed stock in a furnace, forming a liquid metal;
pouring the liquid metal into a preheated mold, forming a molten metal, wherein preheating the mold comprises heating the mold to about 300° C. to about 700° C. from about 10 minutes to about 5 hours,
solidifying the molten metal in the preheated mold, forming the as-cast article; and
homogenizing the as-cast article, at least two of the sequential steps of treating the cast alloy: 0.5 to 5 hours at 1075±25° C.; 1.5 to 3 hours at 1125±25° C.; 3 to 15 hours at 1200±25° C.; 3 to 24 hours at 1250±25° C., wherein the homogenizing the as-cast article forms a specific element segregation below ±1% variation from the nominal chemistry of these elements throughout the as-cast article.

### Claim 29 (depends on 28)

The method of claim 28 wherein the as-cast article comprises a equiaxed region with an average grain size of 289±42 μm.