# US 2022/0265079 A1 · Cookware with copper bonded layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0265079 A1
- Document ID: US20220265079A1
- Status: Published application
- Kind: A1
- Application number: 17/668,412
- Filed: 2022-02-10
- Published: 2022-08-25
- Earliest claimed: 2017-07-31
- Assignees: All-Clad Metalcrafters LLC
- Applicants: All-Clad Metalcrafters, L.L.C.
- Inventors: William A. Groll; Bruce W. Perry
- Web page: https://patentgrep.com/patent/US20220265079A1

## CPC

- A47J 27/002: {Construction of cooking-vessels; Methods or processes of manufacturing specially adapted for cooking-vessels}
- A47J 36/02: Selection of specific materials, e.g. heavy bottoms with copper inlay or with insulating inlay
- B23K 20/023: {Thermo-compression bonding}
- B32B 15/01: all layers being exclusively metallic {(making layered metal workpieces by pressure cladding B23K20/22; making coatings with a metallic material characterised by its composition C23C30/00)}
- C22C 9/00: Alloys based on copper
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- H05B 6/36: Coil arrangements
- B32B 7/04: Interconnection of layers
- B32B 15/015: {the said other metal being copper or nickel or an alloy thereof}
- B32B 2250/42: Alternating layers, e.g. ABAB(C), AABBAABB(C)
- B32B 2307/302: Conductive
- B32B 2311/12: Copper
- B32B 2311/30: Iron, e.g. steel
- A47J: KITCHEN EQUIPMENT; COFFEE MILLS; SPICE MILLS; APPARATUS FOR MAKING BEVERAGES
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H05B: ELECTRIC HEATING; ELECTRIC LIGHT SOURCES NOT OTHERWISE PROVIDED FOR; CIRCUIT ARRANGEMENTS FOR ELECTRIC LIGHT SOURCES, IN GENERAL

## Abstract

Provided is an article of cookware and a method of making the same. The cookware has at least one stainless steel layer and at least one copper layer metallurgically bonded directly to the at least one stainless steel layer via solid state bonding. The at least one stainless steel layer may be a ferritic stainless steel layer, and the at least one copper layer may be a grain stabilized copper. The at least one stainless steel layer may be made from a 400 series stainless steel, such as a 436 stainless steel alloy, a 439 stainless steel alloy, or a 444 stainless steel alloy. The at least one copper layer may be made from a high purity, oxygen free copper alloy, such as a C101 copper alloy, a C102 copper alloy, or a C107 copper alloy.

## Claims

### Claim at position 1

1-31. (canceled)

### Claim 32

A method of making multi-layer, bonded cookware, the method comprising:
providing at least one stainless steel layer and at least one copper layer in a stacked blank assembly; and
applying heat and pressure to the stacked blank assembly for a predetermined period of time such that at least one stainless steel layer is metallurgically bonded to the at least one copper layer via solid state bonding to form a bonded blank assembly,
wherein the at least one stainless steel layer is a ferritic stainless steel layer, and
wherein the at least one copper layer is a copper alloy having controlled grain growth properties.

### Claim 33 (depends on 32)

The method of claim 32, wherein heat is applied at a temperature below a grain growth temperature of the at least one copper layer.

### Claim 34 (depends on 33)

The method of claim 33, wherein heat is applied at a temperature between about 1150° F. (625° C.) to about 1250° F. (675° C.).

### Claim 35 (depends on 32)

The method of claim 32, wherein pressure is applied at about 5,000 psi (350 kg/cm2) to about 20,000 psi (1,400 kg/cm2).

### Claim 36 (depends on 32)

The method of claim 32, wherein pressure is applied in a direction normal to a plane of the at least one stainless steel plate and the at least one copper plate.

### Claim 37 (depends on 32)

The method of claim 32, wherein the predetermined period of time is about 1 hour to about 3 hours.

### Claim 38 (depends on 32)

The method of claim 32, wherein the step of applying heat and pressure is carried out by an induction heating coil surrounding the stacked blank assembly and wherein a non-oxidizing atmosphere is present between the induction heating coil and the stacked blank assembly.

### Claim 39 (depends on 32)

The method of claim 32, further comprising cooling the bonded blank assembly after applying heat and pressure.

### Claim 40 (depends on 40)

The method of claim 40, wherein cooling the bonded blank assembly comprises exposing the bonded blank assembly to ambient air or using a cooling agent.

### Claim 41 (depends on 32)

The method of claim 32, further comprising forming the bonded blank assembly into the cookware.

### Claim 42 (depends on 41)

The method of claim 41, wherein forming the bonded blank assembly comprises shaping the bonded blank assembly in a drawing press or a hydroform machine.

### Claim 43 (depends on 41)

The method of claim 41, further comprising removing a ring-shaped portion of the at least one stainless steel layer to visually expose an underlying surface of the at least one copper layer.

### Claim 44 (depends on 32)

The method of claim 32, wherein the grain stabilized copper is a C101 copper alloy.

### Claim 45 (depends on 32)

The method of claim 32, wherein the grain stabilized copper is a C102 copper alloy.

### Claim 46 (depends on 32)

The method of claim 32, wherein the grain stabilized copper is a C107 copper alloy comprising silver.

### Claim 47

A method of making multi-layer, bonded cookware, the method comprising:
stacking a plurality of metal layers in a stacked blank assembly, the plurality of metal layers comprising:
an upper layer of stainless steel;
an intermediate layer of copper; and
a lower layer of stainless steel; and
applying heat and pressure to the stacked blank assembly for a predetermined period of time such that the plurality of metal layers are metallurgically bonded via solid state bonding to form a bonded blank assembly,
wherein the upper layer and the lower layer are formed from a ferritic stainless steel, and
wherein the intermediate layer is formed from a copper alloy having controlled grain growth properties.

### Claim 48 (depends on 47)

The method of claim 47, further comprising forming the bonded blank assembly into the cookware by shaping the bonded blank assembly in a drawing press or a hydroform machine.

### Claim 49 (depends on 48)

The method of claim 48, further comprising removing a ring-shaped portion of the lower layer of stainless steel to visually expose an underlying surface of the intermediate layer of copper.

### Claim 50

A method of making multi-layer, bonded cookware, the method comprising:
stacking a plurality of metal layers in a stacked blank assembly, the plurality of metal layers comprising:
a first layer of stainless steel;
a first layer of copper;
a second layer of stainless steel;
a second layer of copper; and
a third layer of stainless steel; and
applying heat and pressure to the stacked blank assembly for a predetermined period of time such that the plurality of metal layers are metallurgically bonded via solid state bonding to form a bonded blank assembly,
wherein the first, second, and third layers of stainless steel are formed from a ferritic stainless steel, and
wherein the first and second layers of copper are formed from a copper alloy having controlled grain growth properties.

### Claim 51 (depends on 50)

The method of claim 50, further comprising forming the bonded blank assembly into the cookware by shaping the bonded blank assembly in a drawing press or a hydroform machine.