# US 2022/0255086 A1 · Method for producing a catalyst-coated membrane

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0255086 A1
- Document ID: US20220255086A1
- Status: Published application
- Kind: A1
- Application number: 17/624,725
- Filed: 2020-04-29
- Published: 2022-08-11
- Earliest claimed: 2019-07-04
- Assignees: Heraeus Deutschland GmbH & Co. KG
- Applicants: Heraeus Deutschland GmbH & Co. KG
- Inventors: Frédéric HASCHÉ; Markus NESSELBERGER; Nadia KUWERTZ; Florian EWEINER; Leonard STOICA
- Web page: https://patentgrep.com/patent/US20220255086A1

## CPC

- C09D 127/18: Homopolymers or copolymers of tetrafluoroethene
- H01M 4/881: {Electrolytic membranes}
- C25B 1/04: by electrolysis of water
- C25B 9/23: comprising ion-exchange membranes in or on which electrode material is embedded
- H01M 4/8828: {Coating with slurry or ink}
- H01M 4/8882: {Heat treatment, e.g. drying, baking}
- H01M 8/1004: characterised by membrane-electrode assemblies [MEA] (H01M8/12 takes precedence)
- H01M 8/102: characterised by the chemical structure of the main chain of the ion-conducting polymer
- H01M 8/1039: halogenated, e.g. sulfonated polyvinylidene fluorides
- H01M 4/8832: {Ink jet printing}
- H01M 4/8835: {Screen printing}
- H01M 4/8839: {Painting}
- H01M 2008/1095: {Fuel cells with polymeric electrolytes}
- Y02E 60/36: Hydrogen production from non-carbon containing sources, e.g. by water electrolysis
- Y02E 60/50: Fuel cells
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention relates to a method for producing a membrane for a fuel cell or electrolytic cell, in which (i) a liquid coating composition, which contains a supported catalyst containing precious metal and also contains an ionomer, is applied to a polymer electrolyte membrane which contains an ionomer, the ionomer of the liquid coating composition and the ionomer of the polymer electrolyte membrane each being a copolymer which contains as monomer a fluoroethylene and a fluorovinyl ether containing a sulfonic acid group, (ii) the coated polymer electrolyte membrane is heated to a temperature in the range from 178° C. to 250° C.

## Claims

### Claim 1

Method for producing a membrane for a fuel or electrolytic cell, wherein
(i) a liquid coating composition containing a supported precious metal-containing catalyst and an ionomer is applied to a polymer electrolyte membrane containing an ionomer so that a coated polymer electrolyte membrane with a catalyst-containing layer on its front and/or rear side is obtained, wherein the ionomer of the liquid coating composition and the ionomer of the polymer electrolyte membrane are each a copolymer which, as monomers, contain a fluoroethylene and a fluorovinyl ether containing a sulfonic acid group,
(ii) the coated polymer electrolyte membrane is thermally treated by heating it to a temperature in the range of 178° C. to 250° C.

### Claim 2 (depends on 1)

Method according to claim 1, wherein the fluoroethylene is a tetrafluoroethylene; and/or wherein the fluorovinyl ether containing a sulfonic acid group has the formula (I):
—CF(OR)-CF2— (I)
wherein
R has the following formula (II):
—(CF2-CF(CF3)-O)x-(CF2)y-SO3H (II)
where x=0-3 and y=1-5.

### Claim 3 (depends on 1, 2)

Method according to claim 1 or 2, wherein the polymer electrolyte membrane does not contain any additional ionomer; and/or the polymer electrolyte membrane does not contain any inorganic oxoacid of the phosphorus and/or sulfur.

### Claim 4

Method according to any one of the preceding claims, wherein no polymer containing a basic monomer is present in the polymer electrolyte membrane.

### Claim 5

Method according to any one of the preceding claims, wherein the precious metal is a platinum metal and the supported catalyst contains, as carrier material, a carbon material or an oxide.

### Claim 6

Method according to any one of the preceding claims, wherein the liquid coating composition is an aqueous coating composition.

### Claim 7 (depends on 6)

Method according to claim 6, wherein the aqueous coating composition contains the supported precious metal-containing catalyst in an amount of 5-20 wt %, the ionomer in an amount of 2-8 wt % and water in an amount of at least 60 wt %, and a C1-4 alcohol in an amount of 10-20 wt %.

### Claim 8

Method according to any one of the preceding claims, wherein the liquid coating composition is applied to the polymer electrolyte membrane with a nozzle, scraper, roller, rod, spraying device, screen printing, offset printing, stencil printing, or halftone printing, or a combination of at least two of these coating methods.

### Claim 9

Method according to any one of the preceding claims, wherein the coated polymer electrolyte membrane is subjected to a drying step prior to the thermal treatment in step (ii).

### Claim 10

Method according to any one of the preceding claims, wherein the coated polymer electrolyte membrane heated to 178° C. to 250° C. in step (ii) is maintained in this temperature range for a period of from 1 second to 5 minutes.

### Claim 11

Method according to any one of the preceding claims, wherein the fuel cell is a hydrogen fuel cell or a methanol fuel cell; or wherein the electrolytic cell is a water electrolytic cell.