# US 2022/0251733 A1 · Process for the Production of a Low-Shrinkage Aliphatic Polyamide Yarn

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0251733 A1
- Document ID: US20220251733A1
- Status: Published application
- Kind: A1
- Application number: 17/731,613
- Filed: 2022-04-28
- Published: 2022-08-11
- Earliest claimed: 2014-12-19
- Assignees: Truetzschler Group SE
- Applicants: Truetzschler Group SE
- Inventors: Lassad NASRI; Roman STEPANYAN; Martinus Joseph Maria KEULERS
- Web page: https://patentgrep.com/patent/US20220251733A1

## CPC

- D01D 5/16: using rollers, or like mechanical devices, e.g. snubbing pins
- C08G 69/46: Post-polymerisation treatment
- D01D 4/02: Spinnerettes (alloys therefor C22C)
- D01F 6/60: from polyamides (from polyamino acids or polypeptides D01F6/68)
- D02G 3/02: Yarns or threads characterised by the material or by the materials from which they are made
- D02G 3/446: {Yarns or threads for use in automotive applications}
- D02J 1/228: {Stretching in two or more steps, with or without intermediate steps}
- D02J 1/229: {Relaxing (in combination with crimping D02G1/20)}
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- D02G: CRIMPING OR CURLING FIBRES, FILAMENTS, THREADS, OR YARNS; YARNS OR THREADS
- D02J: FINISHING OR DRESSING OF FILAMENTS, YARNS, THREADS, CORDS, ROPES OR THE LIKE (curling or crimping D02G; by treatment with liquids, gases or vapours D06B; finishing other than by liquid treatment, of yarns in warp or sheet form D06C; for chemical matters, see D06L, D06M, D06P, D06Q; treatment during rope-making, apparatus for treating ropes auxiliary to rope-making D07B)

## Abstract

A process for production of a low-shrinkage aliphatic polyamide fibre, in which polyamide is extruded through a spinneret to form filaments, then cooled and combined to form at least one yarn. The at least one yarn is subjected to drawing between the spinneret and a pair of inlet rolls, then in a further multi-stage drawing step is subjected to 4-fold to 6-fold drawing by pairs of draw rolls. The pairs of draw rolls successively heat the yarn and at least the last pair of draw rolls has a temperature of 5° C. to 20° C. below the melting point of the yarn. The yarn is relaxed by from 6% to 10% in a subsequent at least three-stage relaxation zone and is kept in a temperature range of 5° C. to 15° C. below the melting point of the yarn, and is subsequently wound up on a reel device.

## Claims

### Claim 1

An method for production of a low-shrinkage aliphatic polyamide yarn, comprising steps of:
extruding a polyamide through a spinneret to form filaments;
quenching the filaments from the spinneret to cool and combine the filaments to form at least one yarn;
conducting a first drawing of the quenched yarn through a first pair of inlet rolls;
following the first drawing, conducting a second drawing through a multi-stage drawing apparatus that includes at least three pairs of heatable draw rolls;
increasing the temperature of the at least three pairs of draw rolls from a temperature of a first pair of heatable draw rolls that is operated at a temperature of 5° C. below to 30° C. above the glass transition temperature of the yarn, to a temperature of a second pair of heatable draw rolls that operate at a temperature from 130° C., to 40° C. below a melting temperature of the yarn, to a temperature of a last pair of heatable draw rolls that is operated at a temperature of 5° C. to 20° C. below the melting point of the yarn; and
following the second drawing, relaxing the yarn from 4% to 10% in a temperature range of 5° C. to 15° C. below the melting point of the yarn via at least a three-stage relaxation zone comprising at least first and second pairs of rolls and a reel device that winds the yarn.

### Claim 2 (depends on 1)

The method according to claim 1, further including operating all pairs of draw rolls at a peripheral speed of 400 m/min to 4000 m/min.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the extruding step includes extruding a polyamide comprising at least 90% by weight, monomeric units derived from caprolactam, or monomeric units derived from hexamethylenediamine and adipic acid (AH salt), or mixtures thereof.