# US 2022/0251345 A1 · Vehicle tire rubber composite material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0251345 A1
- Document ID: US20220251345A1
- Status: Published application
- Kind: A1
- Application number: 17/666,875
- Filed: 2022-02-08
- Published: 2022-08-11
- Earliest claimed: 2021-02-08
- Assignees: Xiamen University; Cheng Shin Tire (Xiamen) Co., Ltd.
- Applicants: Xiamen University; Cheng Shin Tire (Xiamen) Co., Ltd.
- Inventors: Lizong DAI; Jing HONG; Hesheng CAO; Guorong CHEN; Weiang LUO; Conghui YUAN; Birong ZENG; Yiting XU
- Web page: https://patentgrep.com/patent/US20220251345A1

## CPC

- C08C 19/14: by reaction with halogens
- C08L 9/00: Compositions of homopolymers or copolymers of conjugated diene hydrocarbons
- B60C 1/00: Tyres characterised by the chemical composition or the physical arrangement or mixture of the composition
- C08L 7/00: Compositions of natural rubber
- C08L 2201/02: Flame or fire retardant/resistant
- C08L 2205/035: containing four or more polymers in a blend
- C08C: TREATMENT OR CHEMICAL MODIFICATION OF RUBBERS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B60C: VEHICLE TYRES; TYRE INFLATION; TYRE CHANGING; CONNECTING VALVES TO INFLATABLE ELASTIC BODIES IN GENERAL; DEVICES OR ARRANGEMENTS RELATED TO TYRES

## Abstract

A vehicle tire rubber composite material, raw materials of the vehicle tire rubber composite material comprise the following components by weight: 30-40 weight distributions of solution-polymerized styrene-butadiene rubber, 35-55 weight distributions of rare earth butadiene rubber, 10-30 weight distributions of phenyl modified natural rubber, 5-14 weight distributions of polyurethane elastomer, 3-9 weight distributions of acetylene carbon black, 2-5 weight distributions of multifunctional abrasion-resistant flame retardant Cu@HNT@MoS2-PZE, 3-6 weight distributions of elastic fiber, 1-3 weight distributions of heat stabilizer, 2-3 weight distributions of silane coupling agent, 1-2.5 weight distributions of anti-scorching agent, 1-2.5 weight distributions of turpentine oil, and 4-6 weight distributions of accelerator.

## Claims

### Claim 1

A low-energy-consumption multifunctional flame-retardant vehicle tire rubber composite material, wherein:
raw materials of the low-energy-consumption multifunctional flame-retardant vehicle tire rubber composite material comprise the following components by weight: 30-40 weight distributions of solution-polymerized styrene-butadiene rubber, 35-55 weight distributions of rare earth butadiene rubber, 10-30 weight distributions of phenyl modified natural rubber, 5-14 weight distributions of polyurethane elastomer, 3-9 weight distributions of acetylene carbon black, 2-5 weight distributions of multifunctional abrasion-resistant flame retardant Cu@HNT@MoS2-PZE, 3-6 weight distributions of elastic fiber, 1-3 weight distributions of heat stabilizer, 2-3 weight distributions of silane coupling agent, 1-2.5 weight distributions of anti-scorching agent, 1-2.5 weight distributions of turpentine oil, and 4-6 weight distributions of accelerator;
raw materials of the phenyl modified natural rubber comprise N-bromosuccinimide, natural rubber, methylene dichloride, methanol, tetrahydrofuran, potassium hydroxide, phenylboronic acid, and palladium catalyst; and
raw materials of the multifunctional abrasion-resistant flame retardant Cu@HNT@MoS2-PZE comprise halloysite nanotubes, CuSO4·5H2O, Na3C6H5O7·2H2O, hydrazine hydrate, Na2MoO4·2H2O, L-cysteine, eugenol, anhydrous potassium carbonate, and phosphonitrilic chloride trimer.

### Claim 2 (depends on 1)

The vehicle tire rubber composite material according to claim 1, wherein:
a method for preparing the phenyl modified natural rubber comprises the following steps:
(1) dissolving the natural rubber in the methylene dichloride, stirring for 1-3 hours under a nitrogen atmosphere at 29-31° C., then adding the N-bromosuccinimide, continually stirring at 29-31° C. for 2-4 hours, then adding the methanol to coagulate a first product, and drying under pressure less than 1 atm (atmospheric pressure) to obtain a brominated natural rubber; and
(2) dissolving the brominated natural rubber in the tetrahydrofuran, stirring for 1-3 hours under a nitrogen atmosphere at room temperature, then adding the phenylboronic acid or p-tolylboronic acid and adding an aqueous solution of the potassium hydroxide and the palladium catalyst, refluxing and reacting for 5-10 hours, adding the methanol to coagulate a second product, and then drying under pressure less than 1 atm to obtain the phenyl modified natural rubber.

### Claim 3 (depends on 2)

The vehicle tire rubber composite material according to claim 2, wherein a mass ratio of the natural rubber, the methylene dichloride, and the N-bromosuccinimide in the step (1) is 1-5: 95-100: 2-6.

### Claim 4 (depends on 2)

The vehicle tire rubber composite material according to claim 2, wherein a mass ratio of the brominated natural rubber, the tetrahydrofuran, the phenylboronic acid or the p-tolylboronic acid, the potassium hydroxide, and the palladium catalyst in the step (2) is 1-4: 95-100: 0.1-0.5: 6-10: 0.006-0.01.

### Claim 5 (depends on 1)

The vehicle tire rubber composite material according to claim 1, wherein:
a method for preparing the multifunctional abrasion-resistant flame retardant Cu@HNT@MoS2-PZE comprises the following steps:
(1) dissolving the halloysite nanotubes and the CuSO4·5H2O in a mixed solvent consisting of ethanol and water with a volume ratio of 20-40:2-10, then slowly dripping Na3C6H5O7·2H2O aqueous solution to obtain a solution, continually sonicating for 2-3 hours, then adding the hydrazine hydrate, reducing at 75-85° C. for 1-2 hours, centrifuging, washing, and drying to obtain Cu@HNT;
(2) sonicating to disperse the Cu@HNT and the Na2MoO4·2H2O in distilled water, then adding the L-cysteine while stirring, then reacting at 180-200° C. for 36-48 hours, centrifuging, washing, and drying to obtain Cu@HNT@MoS2; and
(3) adding the Cu@HNT@MoS2 and the eugenol into dried acetonitrile solvent, adding the anhydrous potassium carbonate, stirring, then slowly dripping an acetonitrile solution of the phosphonitrilic chloride trimer under nitrogen atmosphere, and reacting at 80-85° C. for 36-72 hours to obtain the multifunctional abrasion-resistant flame retardant Cu@HNT@MoS2-PZE.

### Claim 6 (depends on 5)

The vehicle tire rubber composite material according to claim 5, wherein a ratio of the halloysite nanotubes, the CuSO4·5H2O, the Na3C6H5O7·2H2O, and the hydrazine hydrate in the step (1) is 60 mg-120 mg: 10 mg-30 mg: 70 mg-100 mg: 2 mL-4 mL.

### Claim 7 (depends on 5)

The vehicle tire rubber composite material according to claim 5, wherein a mass ratio of the Cu@HNT, the Na2MoO4·2H2O, and the L-cysteine in the step (2) is 0.1-0.3: 0.5-0.9: 2-4.

### Claim 8 (depends on 5)

The vehicle tire rubber composite material according to claim 5, wherein a mass ratio of the Cu@HNT@MoS2, the eugenol, and the anhydrous potassium carbonate in the step (3) is 1-3: 3-5: 2-5.

### Claim 9 (depends on 1)

The vehicle tire rubber composite material according to claim 1, wherein the elastic fiber is at least one of elastic polyethylene fiber, silk, or polyurethane fiber.

### Claim 10 (depends on 1)

A vehicle tire, wherein the vehicle tire is made of raw materials comprising the vehicle tire rubber composite material according to claim 1.