# US 2022/0235467 A1 · Electroless metal coatings exhibiting wave permeability and method for the manufacture thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0235467 A1
- Document ID: US20220235467A1
- Status: Published application
- Kind: A1
- Application number: 17/610,604
- Filed: 2020-05-15
- Published: 2022-07-28
- Earliest claimed: 2019-05-17
- Applicants: FundacióN Cidetec
- Inventors: Asier SALICIO PAZ; Eva GARCÍA LECINA; Egoitz LUIS MONASTERIO
- Web page: https://patentgrep.com/patent/US20220235467A1

## CPC

- C23C 18/36: using hypophosphites
- B32B 15/00: Layered products comprising {a layer of} metal
- C23C 18/1641: {Organic substrates, e.g. resin, plastic}
- C23C 18/1691: {Cooling, e g. forced or controlled cooling}
- C23C 18/2086: {with use of organic or inorganic compounds other than metals, first}
- C23C 18/285: {Sensitising or activating with tin based compound or composition}
- C23C 18/30: Activating {or accelerating or sensitising with palladium or other noble metal}
- C23C 18/40: using reducing agents
- C23C 18/44: using reducing agents
- C23C 18/52: using reducing agents for coating with metallic material not provided for in a single one of groups C23C18/32 - C23C18/50
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

It is provided a method for manufacturing a metal coated substrate by forming a metal coating on a surface of a substrate, comprising: immersing the substrate in a palladium/tin colloidal solution; immersing the substrate in an acid solution; carrying out electroless metal plating in order to obtain a continuous film-coated substrate, and subjecting the metal coating to a cryogenic treatment step in order to make it permeable to electromagnetic waves, the cryogenic treatment step being carried out by cooling the substrate with liquid nitrogen. It is also provided a metal coated substrate obtainable by the mentioned method and an article of manufacture made of the metal coated substrate.

## Claims

### Claim 1

A method for manufacturing a metal coated substrate by forming a metal coating on a surface of a substrate, the method comprising:
a) carrying out a sensitization step by:
immersing the substrate in a colloidal palladium/tin colloidal solution;
immersing the substrate in a tin aqueous solution and, thereafter, in a palladium aqueous solution, or vice versa; or
depositing on the substrate a silver nucleus by immersion or a spray method;
b) immersing the substrate in an acid solution;
c) optionally, immersing the substrate in a PdCl solution;
d) carrying out electroless metal plating by immersing the substrate in a metal electrolyte solution to form a metal coating on the surface of the substrate in order to obtain a continuous film-coated substrate, wherein the metal electrolyte solution comprises a source of metal cations, a complexing agent and a reducing agent, and wherein electroless metal plating is carried out for 5 to 300 seconds, and the metal coating formed has a thickness from 50 to 175 nm; and
e) subjecting the metal coating to a cryogenic treatment step by cooling the continuous film-coated substrate with liquid nitrogen for 10 to 600 seconds;
wherein the substrate is either transparent to electromagnetic waves in the radio domain or has a higher permeability to electromagnetic waves than the metal coating.

### Claim 2 (depends on 1)

The method according to claim 1, wherein step a) is carried out for 5 to 20 min.

### Claim 3 (depends on 1)

The method according to claim 1, wherein electroless metal plating is carried out for 10 to 30 seconds, and the metal coating formed has a thickness from 75 to 150 nm.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the metal coated substrate provides an attenuation for electromagnetic waves in the frequency range from 70 MHz to 85 MHz lower than 7 dB as measured by using a quasi-optical bench with focusing lens attached and equipped with vector network analyzer Keysight PNA-X E3861 attached with VDI frequency extender for W band.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the attenuation is from 0.1 to 6 dB.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the metal coating is selected from the group consisting of a nickel, a nickel alloy, a copper, a copper alloy, a silver, a silver alloy, a tin, and a tin alloy coating, and the metal cations are selected from the group consisting of nickel cations, copper cations, silver cations, tin cations, and mixtures thereof.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the metal coating is a nickel coating, or a nickel alloy coating, and the metal cations are nickel cations.

### Claim 8

(canceled)

### Claim 9 (depends on 1)

The method according to claim 1, wherein the substrate is polycarbonate.

### Claim 10 (depends on 1)

The method according to claim 1, wherein step a) is carried out for 5 to 20 min, and wherein in step d) the metal electrolyte solution is a nickel electrolyte solution, the reducing agent is a hypophosphite alkali metal salt, and electroless plating is carried out at a temperature from 40 to 80° C. in an electroless nickel electrolyte solution at a pH range from 4 to 10 in order to obtain a coating with a phosphorus content from 1 to 25 wt % related to the total weight coating.

### Claim 11 (depends on 1)

The method according to claim 1, wherein step a) is carried out for 12 to 17 min, and wherein in step d) the metal electrolyte solution is a nickel electrolyte solution, the reducing agent is a hypophosphite alkali metal salt, and electroless plating is carried out for 5 to 20 seconds at a temperature from 65 to 75° C. in a nickel electrolyte solution at a pH of 6 to 7 in order to obtain a coating with a phosphorus content from 1 to 4 wt % related to the total weight coating.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the coating has a structure containing crystallites having a size of up to 10 nm calculated using the Scherrer's equation by X-ray diffraction with CuKα radiation (λ=1.5418 Å) in the Bragg Brentano geometry.

### Claim 13 (depends on 1)

The method according to claim 1, wherein step a) is carried out for 12 to 17 min, and wherein in step d) the metal electrolyte solution is a nickel electrolyte solution, the reducing agent is a hypophosphite alkali metal salt, and electroless plating is is carried out for 15 to 60 seconds at a temperature from 40 to 60° C. in a nickel electrolyte solution at a pH of 8 to 10 in order to obtain a coating with a phosphorus content from 10 to 25 wt % related to the total weight coating.

### Claim 14 (depends on 1)

A metal coated substrate obtainable by the method as defined in claim 1, wherein the metal coated substrate provides an attenuation for electromagnetic waves in the frequency range from 70 MHz to 85 MHz lower than 7 dB as measured by using a quasi-optical bench with focusing lens attached and equipped with vector network analyzer Keysight PNA-X E3861 attached with VDI frequency extender for W band.

### Claim 15 (depends on 14)

A method for concealing radar antennas, sensors, image recording systems, or illumination systems, the method comprising providing a metal coated substrate as defined in claim 14.

### Claim 16 (depends on 14)

An article of manufacture made of the metal coated substrate of claim 14.

### Claim 17 (depends on 16)

The article of manufacture of claim 16 comprising a radar antenna.

### Claim 18 (depends on 16)

The article of manufacture of claim 16 comprising a sensor.

### Claim 19

(canceled)

### Claim 20 (depends on 16)

The article of manufacture of claim 16 for image recording.

### Claim 21 (depends on 20)

The article of manufacture of claim 20 that is an automotive reversing camera.

### Claim 22 (depends on 16)

The article of manufacture of claim 16 for illumination applications.