# US 2022/0212295 A1 · Method for joining metal parts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0212295 A1
- Document ID: US20220212295A1
- Status: Published application
- Kind: A1
- Application number: 17/606,566
- Filed: 2020-05-08
- Published: 2022-07-07
- Earliest claimed: 2019-05-29
- Assignees: Alfa Laval Corporate AB
- Applicants: Alfa Laval Corporate AB
- Inventors: Per SJÖDIN; Kristian WALTER; Axel KNUTSSON
- Web page: https://patentgrep.com/patent/US20220212295A1

## CPC

- B23K 35/3606: {Borates or B-oxides}
- B23K 1/0012: {Brazing of heat exchangers}
- B23K 1/008: Soldering within a furnace (B23K1/012 takes precedence)
- B23K 1/19: taking account of the properties of the materials to be soldered
- B23K 1/20: Preliminary treatment of work or areas to be soldered, e.g. in respect of a galvanic coating
- B23K 20/026: {with diffusion of soldering material}
- B23K 20/16: with interposition of special material to facilitate connection of the parts, e.g. material for absorbing or producing gas
- B23K 20/227: with ferrous layer
- B23K 20/233: without ferrous layer
- B23K 20/24: Preliminary treatment
- B23K 35/001: {Interlayers, transition pieces for metallurgical bonding of workpieces}
- B23K 35/004: {at least one of the workpieces being of a metal of the iron group}
- B23K 35/0244: {Powders, particles or spheres; Preforms made therefrom}
- B23K 35/025: {Pastes, creams or slurries}
- B23K 35/30: with the principal constituent melting at less than 1550°C
- B23K 35/3086: {containing Ni or Mn}
- B23K 35/3617: {B-compounds}
- B23K 2101/14: Heat exchangers
- B23K 2101/18: Sheet panels
- B23K 2103/05: {Stainless steel}
- B23K 2103/26: {Alloys of Nickel and Cobalt and Chromium}
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A method for joining a first metal part with a second metal part, the metal parts having a solidus temperature above 1100° C., includes applying a melting depressant composition on a surface of the first metal part, the melting depressant composition including a melting depressant component that includes at least 25 wt % boron and silicon for decreasing a melting temperature of the first metal part; bringing the second metal part into contact with the melting depressant composition at a contact point on said surface; heating the first and second metal parts to a temperature above 1100° C.; and allowing a melted metal layer of the first metal component to solidify, such that a joint is obtained at the contact point. The boron at least partly originates from a boron compound selected from any of the following compounds: boric acid, borax, titanium diboride and boron nitride. The melting depressant composition and related products are also described.

## Claims

### Claim 1

A method for joining a first metal part with a second metal part, the metal parts having a solidus temperature above 1100° C., the method comprising
applying a melting depressant composition at least on a surface of the first metal part, the melting depressant composition comprising
a melting depressant component comprising at least 25 wt % boron and silicon in total for decreasing a melting temperature of the first metal part, and
optionally, a binder component for facilitating the applying of the melting depressant composition on the surface,
bringing the second metal part into contact with the melting depressant composition at a contact point on said surface,
heating the first and second metal parts to a temperature above 1100° C., said surface of the first metal part thereby melting such that a surface layer of the first metal part melts and, together with the melting depressant component, forms a molten metal layer that is in contact with the second metal part at the contact point, and
allowing the molten metal layer to solidify, such that a joint is obtained at the contact point,
wherein the boron at least partly originates from a boron compound selected from any of the following compounds: boric acid, borax, titanium diboride, boron nitride and/or combinations thereof.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the boron originates from any of the boric acid, borax, titanium diboride, boron nitride and/or combinations thereof in an amount 15-100 wt %, or 50 to 100 wt %, based on the total weight of the boron.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the silicon originates from any of elemental silicon and silicon of a silicon compound selected from at least any of the following compounds: silicon carbide, silicon boride and ferrosilicon.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the melting depressant component comprises at least 40 wt % boron and silicon.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the melting depressant component comprises at least 85 wt % boron and silicon.

### Claim 6 (depends on 1)

The method according to any one of the preceding claims claim 1, wherein boron constitutes at least 10 wt % of the boron and silicon content of the melting depressant compound.

### Claim 7 (depends on 1)

The method according to claim 1, wherein silicon constitutes at least 55 wt % of the boron and silicon content of the melting depressant compound.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the melting depressant component comprises less than 50 wt % metallic elements.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the melting depressant component comprises less than 10 wt % metallic elements.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the first metal part comprises a thickness of 0.1-1.0, or 0.6 to 1.0, or 0.3 to 0.6 mm and the applying of the melting depressant composition comprises applying an average of 0.02-0.12 mg boron and silicon per mm2 on the surface of the first metal part.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the surface has an area that is larger than an area defined by the contact point on said surface, such that metal in the melted metal layer flows to the contact point when allowing the joint to form.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the first metal part comprises >50 wt % Fe, <13 wt % Cr, <1 wt % Mo, <1 wt % Ni and <3 wt % Mn.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the first metal part comprises >10 wt % Cr and >60 wt % Ni.

### Claim 14 (depends on 1)

A product comprising a first metal part that is joined with a second metal part according to the method of claim 1.

### Claim 15 (depends on 1)

A melting depressant composition for joining a first metal part with a second metal part according to the method of claim 1, the melting depressant composition comprising i) a melting depressant component that comprises at least 25 wt % boron and silicon for decreasing a melting temperature, and ii), optionally, a binder component for facilitating applying of the melting depressant composition on the first metal part, wherein the boron originates from a boron compound selected from any of the following compounds: boric acid, borax, titanium diboride and boron nitride.

### Claim 16 (depends on 2)

The method according to claim 2, wherein the silicon originates from any of elemental silicon and silicon of a silicon compound selected from at least any of the following compounds: silicon carbide, silicon boride and ferrosilicon.

### Claim 17 (depends on 2)

The method according to claim 2, wherein the melting depressant component comprises at least 40 wt % boron and silicon.

### Claim 18 (depends on 3)

The method according to claim 3, wherein the melting depressant component comprises at least 40 wt % boron and silicon.

### Claim 19 (depends on 2)

The method according to claim 2, wherein the melting depressant component comprises at least 85 wt % boron and silicon.

### Claim 20 (depends on 3)

The method according to claim 3, wherein the melting depressant component comprises at least 85 wt % boron and silicon.