# US 2022/0204821 A1 · Adhesive agent and method for producing adhesive agent

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0204821 A1
- Document ID: US20220204821A1
- Status: Published application
- Kind: A1
- Application number: 17/696,084
- Filed: 2022-03-16
- Published: 2022-06-30
- Earliest claimed: 2019-09-27
- Assignees: Kaneka Corporation
- Applicants: Kaneka Corporation
- Inventors: Nobuyoshi Maizuru
- Web page: https://patentgrep.com/patent/US20220204821A1

## CPC

- C09J 163/00: Adhesives based on epoxy resins; Adhesives based on derivatives of epoxy resins
- C08F 291/02: on to elastomers
- C08L 33/04: Homopolymers or copolymers of esters {(C08L43/04 takes precedence)}
- C08L 51/04: grafted on to rubbers
- C09J 133/04: Homopolymers or copolymers of esters {(C09J143/04 takes precedence)}
- C09J 151/00: Adhesives based on graft polymers in which the grafted component is obtained by reactions only involving carbon-to-carbon unsaturated bonds (based on ABS polymers C09J155/02); Adhesives based on derivatives of such polymers
- C09J 2409/00: Presence of diene rubber
- C09J 2433/00: Presence of (meth)acrylic polymer
- C09J 2463/00: Presence of epoxy resin
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

An adhesive agent that is favorable in terms of peeling form, adhesive strength, and viscosity is provided. The adhesive agent contains an epoxy resin (A), fine polymer particles (B), and a non-crosslinked acrylic resin (C). With respect to 100 parts by mass of the epoxy resin (A), 1 part by mass to 100 parts by mass of fine polymer particles (B) and 1 part by mass to 100 parts by mass of a non-crosslinked acrylic resin (C) are contained in the adhesive agent. The fine polymer particles (B) contain a rubber-containing graft copolymer that includes (i) an elastic body containing a specific material and (ii) a graft part containing a specific material.

## Claims

### Claim 1

An adhesive agent comprising:
an epoxy resin (A); and
with respect to 100 parts by mass of the epoxy resin (A), 1 part by mass to 100 parts by mass of fine polymer particles (B) and 1 part by mass to 100 parts by mass of a non-crosslinked acrylic resin (C),
the fine polymer particles (B) containing a rubber-containing graft copolymer that includes an elastic body and a graft part grafted to the elastic body,
the elastic body containing at least one selected from the group consisting of diene-based rubbers, (meth)acrylate-based rubbers, and organosiloxane-based rubbers,
the graft part containing a polymer that contains, as one or more structural units, the one or more structural units derived from at least one type of monomer selected from the group consisting of aromatic vinyl monomers, vinyl cyanide monomers, and (meth)acrylate monomers,
the non-crosslinked acrylic resin (C) forming a domain in a cured product that is obtained by curing the adhesive agent, and
the fine polymer particles (B) having an average particle size that is larger than a longitudinal dimension of the domain.

### Claim 2 (depends on 1)

The adhesive agent as set forth in claim 1, wherein the fine polymer particles (B) are contained in an amount of 50% by weight to 99% by weight and the non-crosslinked acrylic resin (C) is contained in an amount of 1% by weight to 50% by weight, where 100% by weight represents a total amount of the fine polymer particles (B) and the non-crosslinked acrylic resin (C).

### Claim 3 (depends on 1)

The adhesive agent as set forth in claim 1, wherein the non-crosslinked acrylic resin (C) has a weight average molecular weight of not more than 100,000.

### Claim 4 (depends on 1)

The adhesive agent as set forth in claim 1, wherein the non-crosslinked acrylic resin (C) has a glass transition temperature of not higher than 80° C.

### Claim 5 (depends on 1)

The adhesive agent as set forth in claim 1, wherein the non-crosslinked acrylic resin (C) is a liquid having a viscosity of not more than 1,000,000 mPa·s at 25° C.

### Claim 6

A method for producing an adhesive agent, comprising:
a mixing step of mixing 100 parts by mass of an epoxy resin (A) and a powdery and/or granular material containing 1 part by mass to 100 parts by mass of fine polymer particles (B) and 1 part by mass to 100 parts by mass of a non-crosslinked acrylic resin (C), wherein
the fine polymer particles (B) contain a rubber-containing graft copolymer that includes an elastic body and a graft part grafted to the elastic body,
the elastic body contains at least one selected from the group consisting of diene-based rubbers, (meth)acrylate-based rubbers, and organosiloxane-based rubbers, and
the graft part contains a polymer that contains, as one or more structural units, the one or more structural units derived from at least one type of monomer selected from the group consisting of aromatic vinyl monomers, vinyl cyanide monomers, and (meth)acrylate monomers.

### Claim 7 (depends on 6)

A method as set forth in claim 6, further comprising, before the mixing step, a powdery and/or granular material preparing step of preparing the powdery and/or granular material containing 1 part by mass to 100 parts by mass of the fine polymer particles (B) and 1 part by mass to 100 parts by mass of the non-crosslinked acrylic resin (C).

### Claim 8 (depends on 6)

The method as set forth in claim 6, wherein the non-crosslinked acrylic resin (C) forms a domain in a cured product that is obtained by curing the adhesive agent.

### Claim 9 (depends on 8)

The method as set forth in claim 8, wherein the fine polymer particles (B) have an average particle size that is larger than a longitudinal dimension of the domain.

### Claim 10 (depends on 7)

The method as set forth in claim 7, wherein a force required to break a block of the powdery and/or granular material is not more than 30000 Pa, wherein:
the block is a block obtained by applying, to the powdery and/or granular material which is being allowed to stand, a load of 6.3 kg at 60° C. for 2 hours by placing a 6.3 kg weight on 30 g of the powdery and/or granular material contained in a cylindrical container having a diameter of 50 mm, and