# US 2022/0204357 A1 · Method for the production of a gallate solution

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0204357 A1
- Document ID: US20220204357A1
- Status: Published application
- Kind: A1
- Application number: 17/574,470
- Filed: 2022-01-12
- Published: 2022-06-30
- Earliest claimed: 2019-07-12
- Assignees: Obshchestvo S Ogranichennoy Otvetstvennost'yu "Obedinennaya Kompaniya Rusal Inzhenerno-Tekhnologiche
- Applicants: Obshchestvo S Ogranichennoy Otvetstvennost'yu "Obedinennaya Kompaniya Rusal Inzhenerno-Tekhnologiche
- Inventors: Aleksandr Aleksandrovich Damaskin; Aleksandr Gennadievich Suss; Maksim Nikolaevich Pechenkin; Anna Aleksandrovna Damaskina
- Web page: https://patentgrep.com/patent/US20220204357A1

## CPC

- C01G 15/003: {Preparation involving a liquid-liquid extraction, an adsorption or an ion-exchange}
- C22B 58/00: Obtaining gallium or indium {(treatment or purification of solutions by liquid-liquid extraction, by ion-exchange or by adsorption C22B3/20)}
- C22B 3/08: Sulfuric acid {, other sulfurated acids or salts thereof}
- C22B 3/22: by physical processes, e.g. by filtration, by magnetic means {, or by thermal decomposition} (treatment or purification of solutions by liquid-liquid extraction C22B3/26)
- C22B 3/24: by adsorption on solid substances, e.g. by extraction with solid resins
- C22B 3/44: by chemical processes (treatment or purification of solutions by liquid-liquid extraction C22B3/26, by ion-exchange extraction C22B3/42)
- Y02P 10/20: Recycling
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The gallate solution is obtained from an alkaline gallium-containing solution. Gallium is sorbed from a recycled solution on a divinylbenzene polymer-based ionite, gallium is desorbed with a solution of sulfuric acid to obtain a gallium-containing eluate, followed by concentration of gallium by converting it to a solid phase by neutralisation of the eluate with a caustic solution with precipitation of a gallium hydroxide precipitate at a given temperature. Thickening and filtration of the precipitate are carried out with its further dissolution in a caustic solution until a given concentration of gallium in the solution is obtained. The method allows to increase the concentration of gallium by converting it to the solid phase when neutralising acidic eluates with an alkaline solution, which simplifies the concentration process and reduces the number of technological operations and, as a result, reduces the cost of gallium production.

## Claims

### Claim 1

A method for obtaining a gallate solution from an alkaline gallium-containing solution, which differs from a prototype, the method comprising:
sorption of gallium from a recycled solution on a divinylbenzene polymer-based ionite,
desorption of gallium with a solution of sulfuric acid to obtain a gallium-containing eluate,
concentrating gallium by converting said gallium to a solid phase based on neutralising the gallium-containing eluate with a caustic solution with precipitation of a precipitate of gallium hydroxide at a given temperature,
thickening and filtering the precipitate of gallium hydroxide; and
dissolving the filtered precipitate of gallium hydroxide in a caustic solution until a given concentration of gallium in the caustic solution is obtained.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the concentration of the solution of sulfuric acid is 1-10 wt. %.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the concentration of the caustic solution is 50-500 g/dm3 of Na2O.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the gallate solution is generated at a temperature of 60-80° C.

### Claim 5 (depends on 1)

The method according to claim 1, further comprises at least:
a cooling stage before sorption of a previously generated spent liquor, or
a cooling stage after preparation of the gallate solution.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the cooling stage is carried out to a temperature below 20° C.

### Claim 7 (depends on 5)

The method according to claim 5, wherein impurity components are filtered out during the cooling stage.

### Claim 8 (depends on 1)

The method according to claim 1, wherein after the thickening and filtering, a resulting neutral solution is further processed to generate alumina.

### Claim 9 (depends on 1)

The method according to claim 1, wherein after the thickening and filtering:
combining a resulting neutral solution with neutralised effluents from a mud disposal area in an open water circulation system, and
sending the combined neutral solution and the neutralised effluents to an alumina production stage.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the precipitation of the gallium hydroxide precipitate is carried out at a temperature of 40-95° C.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the minimum concentration of gallium obtained in the gallate solution is 20 g/dm3.

### Claim 12 (depends on 1)

The method according to claim 1, wherein converting said gallium to the solid phase by neutralising the gallium-containing eluate with the caustic solution is carried out to a pH of 6.8-7.2.

### Claim 13 (depends on 1)

The method according to claim 1, wherein a solution of alumina is used as the alkaline gallium-containing solution.

### Claim 14

A gallate solution generated by processing an alkaline gallium-containing solution, the processing comprising:
sorption of gallium from a recycled solution on a divinylbenzene polymer-based ionite,
desorption of gallium with a solution of sulfuric acid to obtain a gallium-containing eluate,
concentrating gallium by converting said gallium to a solid phase based on neutralising the gallium-containing eluate with a caustic solution with precipitation of a precipitate of gallium hydroxide at a given temperature,
thickening and filtering the precipitate of gallium hydroxide; and
dissolving the filtered precipitate of gallium hydroxide in a caustic solution until a given concentration of gallium in the caustic solution is obtained.

### Claim 15 (depends on 1)

The method according to claim 1, wherein:
the concentration of the solution of sulfuric acid is 1-10 wt. %;
the concentration of the caustic solution is 50-500 g/dm3 of Na2O; and
the minimum concentration of gallium obtained in the gallate solution is 20 g/dm3.

### Claim 16 (depends on 1)

The method according to claim 1, further comprises at least one of:
a first cooling stage before sorption of a previously generated spent liquor, and
a second cooling stage after preparation of the gallate solution.

### Claim 17 (depends on 16)

The method according to claim 16, wherein:
one or more of the first cooling stage and the cooling stage is carried out to a temperature below 20° C.,
the preparation of a gallate solution is carried out at a temperature of 60-80° C., and
the precipitation of the gallium hydroxide precipitate is carried out at a temperature of 40-95° C.

### Claim 18 (depends on 16)

The method according to claim 16, wherein impurity components are filtered out during one or more of the first cooling stage or the second cooling stage.

### Claim 19 (depends on 1)

The method according to claim 1, wherein after the thickening and filtering, a resulting neutral solution is further processed to generate alumina.

### Claim 20 (depends on 1)

The method according to claim 1, wherein after the thickening and filtering:
combining a resulting neutral solution with neutralised effluents from a mud disposal area in an open water circulation system, and
sending the combined neutral solution and the neutralised effluents to an alumina production stage.