# US 2022/0194811 A1 · Method for preparing two-dimensional ordered mesoporous nanosheets by inorganic salt interface-induced assembly

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0194811 A1
- Document ID: US20220194811A1
- Status: Published application
- Kind: A1
- Application number: 17/603,587
- Filed: 2020-03-09
- Published: 2022-06-23
- Earliest claimed: 2019-05-11
- Assignees: Fudan University
- Applicants: Fudan University
- Inventors: Yonghui DENG; Liangliang LIU; Yidong ZOU; Xuanyu YANG
- Web page: https://patentgrep.com/patent/US20220194811A1

## CPC

- C01B 33/126: {Preparation of silica of undetermined type}
- C01G 23/053: Producing by wet processes, e.g. hydrolysing titanium salts
- B32B 18/00: Layered products essentially comprising ceramics, e.g. refractory products
- C01B 32/15: Nano-sized carbon materials
- C01B 33/113: Silicon oxides; Hydrates thereof {(preparing monoxide by reduction of siliceous material C01B33/182)}
- C01F 7/30: Preparation of aluminium oxide or hydroxide by thermal decomposition or by hydrolysis or oxidation of aluminium compounds
- C01F 7/304: of organic aluminium compounds
- C01F 17/235: Cerium oxides or hydroxides
- C01F 17/32: oxide or hydroxide being the only anion, e.g. NaCeO2 or MgxCayEuO
- C01G 25/00: Compounds of zirconium
- C01G 25/02: Oxides
- C04B 38/0022: {obtained by a chemical conversion or reaction other than those relating to the setting or hardening of cement-like material or to the formation of a sol or a gel, e.g. by carbonising or pyrolysing preformed cellular materials based on polymers, organo-metallic or organo-silicon precursors}
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- C01P 2004/01: depicted by an image
- C01P 2004/20: extending in two dimensions, e.g. plate-like
- C01P 2004/24: Nanoplates, i.e. plate-like particles with a thickness from 1-100 nanometer
- C01P 2006/16: Pore diameter
- C04B 2111/00008: {Obtaining or using nanotechnology related materials}
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

A method for preparing two-dimensional (2D) ordered mesoporous nanosheets by inorganic salt interface-induced assembly includes the following steps: carrying out, by using a soluble inorganic salt as a substrate and an amphiphilic block copolymer as a template, uniform mass diffusion of a target precursor solution at an inorganic salt crystal interface through vacuum filtration or low-speed centrifugation; forming a single-layer ordered mesoporous structure by using the solvent evaporation-induced co-assembly (EICA) technology; and promoting, through gradient temperature-controlled Ostwald ripening, the evaporation and induced formation of an organic solvent, and removing the template in N2 to obtain a 2D single-layer ordered mesoporous nanosheet material. The assembled nanosheet material has a large pore size, regular spherical pores and orderly arrangement. By changing the type of the precursor, a variety of mesoporous metal oxides, metal elements, inorganic non-metal nanosheets are synthesized.

## Claims

### Claim 1

A method for preparing two-dimensional (2D) ordered mesoporous nanosheets by inorganic salt interface-induced assembly, comprising the following steps:
(1) preparing a nonmaterial precursor solution by using an amphiphilic block copolymer with a high molecular weight as a template;
(2) introducing the nanomaterial precursor solution into a soluble inorganic salt serving as a substrate; guiding mass diffusion of the nanomaterial precursor solution in the soluble inorganic salt by a physical means of suction filtration or low-speed centrifugation to realize a single-layer dispersion interface on a surface of the precursor solution, wherein the suction filtration is less than 0.03 MPa, and the low-speed centrifugation is less than 4.000 rpm;
(3) based on a principle of solvent evaporation-induced co-assembly (EICA), regulating a volatile organic solvent to evaporate at slow or medium-speed in a gradient temperature-controlled manner, to realize self-assembly of a molecular precursor and the amphiphilic block copolymer on a surface of the soluble inorganic salt;
(4) heating up to 300-600° C. in N2; carrying out high-temperature calcination for 2-3 h to remove the amphiphilic block copolymer and to obtain a layered 2D ordered mesoporous organic/inorganic hybrid composite; heating up to 430-630° C. in air in a muffle furnace; carrying out high-temperature calcination for 2-3 h to remove residual carbon and to obtain a highly ordered mesoporous structure; dissolving the soluble inorganic salt template with a large amount of deionized water to obtain a 2D single-layer ordered mesoporous nanosheet material.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the amphiphilic block copolymer is a high-molecular-weight polymer, and the high-molecular-weight polymer is one or more selected from the group consisting of a commercial polyether template, PEO-b-PS, PEO-PPO-PEO and PS-b-P4VP[P]; wherein the commercial polyether template comprises F127;
a target nanosheet raw material used is one or more selected from the group consisting of metal alkoxide, metal chloride, metal sulfate, acetylacetonate, inorganic non-metal precursor salt and phenolic formaldehyde resin;
the volatile organic solvent used by the nanomaterial precursor solution is one or more selected from the group consisting of tetrahydrofuran (THF) and ethanol.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the soluble inorganic salt used is selected from the group consisting of NaCl, KCl and K2SO4.

### Claim 4 (depends on 1)

The method according to claim 1, wherein when the volatile organic solvent is regulated in the gradient temperature-controlled manner, the solvent is gradiently and continuously evaporated at room temperature for 12-24 h, at 35-40° C. for 15-24 h and at 95-105° C. for 15-24 h.

### Claim 5

The method according to 4, wherein a heating rate of the high-temperature calcination is 1-5° C./min.

### Claim 6 (depends on 2)

The method according to claim 2, wherein a solution-phase assembly system of the 2D single-layer ordered mesoporous nanosheet material comprises 5-20 wt % of the target nanosheet raw material, 1-5 wt % of the amphiphilic block copolymer, 20-80 wt % of the soluble inorganic salt, and the balance being the volatile organic solvent.

### Claim 7 (depends on 1)

A 2D ordered mesoporous nanosheet material prepared by the method according to claim 1, wherein a mesoporous size is changeable, the molecular weight of the amphiphilic block copolymer is adjustable within 18-50 nm, and the number of nanosheet layers is adjusted to 1-5 by changing a solubility of the molecular precursor, a suction filtration time or a centrifugation speed.

### Claim 8 (depends on 2)

The method according to claim 2, wherein when the volatile organic solvent is regulated in the gradient temperature-controlled manner, the solvent is gradiently and continuously evaporated at room temperature for 12-24 h, at 35-40° C. for 15-24 h and at 95-105° C. for 15-24 h.

### Claim 9 (depends on 3)

The method according to claim 3, wherein when the volatile organic solvent is regulated in the gradient temperature-controlled manner, the solvent is gradiently and continuously evaporated at room temperature for 12-24 h, at 35-40° C. for 15-24 h and at 95-105° C. for 15-24 h.

### Claim 10 (depends on 4)

The method according to claim 4, wherein a solution-phase assembly system of the 2D single-layer ordered mesoporous nanosheet material comprises 5-20 wt % of a target nanosheet raw material, 1-5 wt % of the amphiphilic block copolymer, 20-80 wt % of the soluble inorganic salt, and the balance being the volatile organic solvent.

### Claim 11 (depends on 7)

The 2D ordered mesoporous nanosheet material according to claim 7, wherein the amphiphilic block copolymer is a high-molecular-weight polymer, and the high-molecular-weight polymer is one or more selected from the group consisting of a commercial polyether template, PEO-b-PS, PEO-PPO-PEO and PS-b-P4VP; wherein the commercial polyether template comprises F127;
a target nanosheet raw material used is one or more selected from the group consisting of metal alkoxide, metal chloride, metal sulfate, acetylacetonate, inorganic non-metal precursor salt and phenolic formaldehyde resin;
the volatile organic solvent used by the nanomaterial precursor solution is one or more selected from the group consisting of tetrahydrofuran (THF) and ethanol.

### Claim 12 (depends on 11)

The 2D ordered mesoporous nanosheet material according to claim 11, wherein the soluble inorganic salt used is selected from the group consisting of NaCl, KCl and K2SO4.

### Claim 13 (depends on 12)

The 2D ordered mesoporous nanosheet material according to claim 12, wherein when the volatile organic solvent is regulated in the gradient temperature-controlled mariner, the solvent is gradiently and continuously evaporated at room temperature for 12-24 h, at 35-40° C. for 15-24 h and at 95-105° C. for 15-24 h.

### Claim 14 (depends on 13)

The 2D ordered mesoporous nanosheet material to claim 13, wherein a heating rate of the high-temperature calcination is 1-5° C./min.

### Claim 15 (depends on 7)

The 2D ordered mesoporous nanosheet material according to claim 7, wherein a solution-phase assembly system of the single-layer 2D ordered mesoporous nanosheet material comprises 5-20 wt % of a target nanosheet raw material, 1-5 wt % of the amphiphilic block copolymer, 20-80 wt % of the soluble inorganic salt, and the balance being the volatile organic solvent.