# US 2022/0093466 A1 · Epitaxial high-k etch stop layer for backside reveal integration

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0093466 A1
- Document ID: US20220093466A1
- Status: Published application
- Kind: A1
- Application number: 17/481,512
- Filed: 2021-09-22
- Published: 2022-03-24
- Earliest claimed: 2020-09-24
- Assignees: Tokyo Electron Limited
- Applicants: Tokyo Electron Limited
- Inventors: Robert D. Clark
- Web page: https://patentgrep.com/patent/US20220093466A1

## CPC

- H10P 95/11: {Separation of active layers from substrates}
- H10D 86/0214: {using temporary substrates}
- H10P 50/246: {of Group III-V materials}
- H10P 50/283: {by chemical means}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 88/01: {Manufacture or treatment}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A backside reveal method includes providing a semiconductor material substrate, depositing an epitaxial high-k etch stop layer on the semiconductor material substrate, forming an integrated circuit device layer on the epitaxial high-k etch stop layer, and attaching a carrier substrate to a front side of the integrated circuit device layer. The method further includes removing a portion of a thickness of the semiconductor material substrate to leave a remaining portion of the thickness of the semiconductor material substrate, removing, by a first selective etching, the remaining portion of the semiconductor material substrate, and removing, by a second selective etching, the epitaxial high-k etch stop layer to expose a backside of the integrated circuit device layer. The epitaxial high-k etch stop layer has good lattice match and high etch selectivity relative to the semiconductor material substrate.

## Claims

### Claim 1

A backside reveal method, comprising:
providing a semiconductor material substrate;
depositing an epitaxial high-k etch stop layer on the semiconductor material substrate,
forming an integrated circuit device layer on the epitaxial high-k etch stop layer;
attaching a carrier substrate to a front side of the integrated circuit device layer;
removing a portion of a thickness of the semiconductor material substrate to leave a remaining portion of the thickness of the semiconductor material substrate;
removing, by a first selective etching, the remaining portion of the semiconductor material substrate; and
removing, by a second selective etching, the epitaxial high-k etch stop layer to expose a backside of the integrated circuit device.

### Claim 2 (depends on 1)

The method of claim 1, wherein forming the integrated circuit device layer includes
depositing an epitaxial semiconductor material layer on the epitaxial high-k etch stop layer; and
patterning the epitaxial semiconductor material layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the integrated circuit device layer contains transistor structures that include channel bodies, gate/source/drain regions of transistor devices, or both.

### Claim 4 (depends on 1)

The method of claim 1, wherein the epitaxial high-k etch stop layer includes a mixed metal oxide, a mixed metal oxynitride, or a mixed metal nitride.

### Claim 5 (depends on 1)

The method of claim 1, wherein the epitaxial high-k etch stop layer contains at least one of Scandium (Sc), Yttrium (Y), and an element from the lanthanide series.

### Claim 6 (depends on 4)

The method of claim 4, wherein the mixed metal oxide has the chemical formula Ln1xLn2yO(x+y)3/2, and wherein Ln1 and Ln2 are selected from Scandium (Sc), Yttrium (Y), and the lanthanide series.

### Claim 7 (depends on 4)

The method of claim 4, wherein the mixed metal oxide has the chemical formula LnxGfyOz, wherein Ln is selected from Sc, Y, and the lanthanide series, and Gf is a Group 4 element selected from Titanium (Ti), Zirconium (Zr), Hafnium (Hf), and mixtures thereof.

### Claim 8 (depends on 4)

The method of claim 4, wherein the mixed metal oxide has the chemical formula TixMyOz, and where M is selected from Hf, Zr, and mixtures thereof.

### Claim 9 (depends on 4)

The method of claim 4, wherein the mixed metal oxide has the chemical formula LnxAlyO(x+y)3/2, and wherein Ln is selected from Sc, Y, the lanthanide series, and mixtures thereof.

### Claim 10 (depends on 4)

The method of claim 4, wherein the mixed metal oxide has the chemical formula AlxGfyOz, where Gf is a Group 4 element selected from Ti, Zr, Hf, and mixtures thereof.

### Claim 11 (depends on 1)

The method of claim 1, wherein the epitaxial high-k etch stop layer has less than 1% lattice mismatch to semiconductor material substrate.

### Claim 12 (depends on 1)

The method of claim 1, wherein removing the portion of the thickness of the semiconductor material substrate includes mechanical grinding.

### Claim 13 (depends on 1)

The method of claim 1, wherein removing the portion of the thickness of the semiconductor material substrate includes a Smart Cut™ process.

### Claim 14

A backside reveal method, comprising:
providing a semiconductor material substrate;
depositing an epitaxial high-k etch stop layer on the semiconductor material substrate,
forming an integrated circuit device layer on the epitaxial high-k etch stop layer;
attaching a carrier substrate to a front side of the integrated circuit device layer;
removing the semiconductor material substrate from the epitaxial high-k etch stop layer; and
removing, by selective etching, the epitaxial high-k etch stop layer to expose a backside of the integrated circuit device.

### Claim 15 (depends on 14)

The method of claim 14, wherein the epitaxial high-k etch stop layer includes a mixed metal oxide, a mixed metal oxynitride, or a mixed metal nitride.

### Claim 16 (depends on 14)

The method of claim 14, wherein the epitaxial high-k etch stop layer contains at least one of Scandium (Sc), Yttrium (Y), and an element from the lanthanide series.

### Claim 17 (depends on 14)

The method of claim 14, wherein the epitaxial high-k etch stop layer has less than 1% lattice mismatch to semiconductor material substrate.