# US 2022/0093457 A1 · Etch Profile Control of Interconnect Structures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0093457 A1
- Document ID: US20220093457A1
- Status: Published application
- Kind: A1
- Application number: 17/542,609
- Filed: 2021-12-06
- Published: 2022-03-24
- Earliest claimed: 2017-04-28
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Allen Ke; Yi-Wei Chiu; Hung Jui Chang; Yu-Wei Kuo
- Web page: https://patentgrep.com/patent/US20220093457A1

## CPC

- H10W 20/037: {the barrier, adhesion or liner layers being on top of a main fill metal}
- H10W 20/082: {the openings being tapered via holes}
- H10W 20/021: {of interconnections within wafers or substrates}
- H10W 20/075: {of multilayered thin functional dielectric layers}
- H10W 20/077: {on sidewalls or on top surfaces of conductors (H10W20/076 takes precedence)}
- H10W 20/087: {involving multiple stacked pre-patterned masks}
- H10W 20/088: {involving partial etching of via holes}
- H10W 20/42: Vias, e.g. via plugs
- H10W 20/47: comprising two or more dielectric layers having different properties, e.g. different dielectric constants
- H10W 70/042: {Etching}
- H10P 50/73: {using masks for insulating materials}
- H10W 72/9232: {with additional elements interposed between layers}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of forming a semiconductor structure includes forming an etch stop layer on a substrate, forming a metal oxide layer over the etch stop layer, and forming an interlayer dielectric (ILD) layer on the metal oxide layer. The method further includes forming a trench etch opening over the ILD layer, forming a capping layer over the trench etch opening, and forming a via etch opening over the capping layer.

## Claims

### Claim 1

A method, comprising:
patterning a first opening in a photoresist layer;
etching, via the first opening, a first silicon-based layer and a first organic layer below the photoresist layer to form a second opening in the first organic layer while removing the photoresist layer and the first silicon-based layer; and
etching, via the second opening, a capping layer, a second silicon-based layer, and a low temperature oxide (LTO) layer below the first organic layer to form a third opening in the second silicon-based layer and the LTO layer while removing the first organic layer and the capping layer, wherein the third opening exposes a portion of a second organic layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first silicon-based layer is formed by spin-coating siloxane on the first organic layer at a temperature between about 50° C. and about 200° C., and wherein etching the first silicon-based layer comprises etching the first silicon-based layer by a dry etch process using a gas mixture comprising fluorocarbon, nitrogen, and argon.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first organic layer is formed by spin-coating a polymer material on the capping layer at a temperature between about 100° C. and about 300° C., and wherein etching the first organic layer comprises etching the first organic layer by a dry etch process using a gas mixture comprising hydrogen, nitrogen, and argon.

### Claim 4 (depends on 1)

The method of claim 1, wherein the capping layer is formed on the second silicon-based layer by a chemical vapor deposition (CVD) process using a gas mixture comprising silane and oxygen at a temperature between about 200° C. and about 500° C., and wherein etching the capping layer comprises etching the capping layer by a dry etch process using fluorocarbon gas having a flow rate between about 100 sccm and about 400 sccm.

### Claim 5 (depends on 1)

The method of claim 1, wherein the second silicon-based layer is formed on the LTO layer by one of a CVD process and a physical vapor deposition (PVD) process using a gas mixture having elements of silicon, oxygen, and carbon, and wherein etching the second silicon-based layer comprises etching the second silicon-based layer by a dry etch process using a gas mixture comprising hydrofluorocarbon, oxygen, nitrogen, and argon.

### Claim 6 (depends on 1)

The method of claim 1, wherein the LTO layer is formed on the second organic layer by a CVD process using a gas mixture comprising silane and oxygen at a temperature between about 50° C. and about 200° C., and wherein etching the LTO layer comprises etching the LTO layer by a dry etch process using a gas mixture comprising between about 1% and about 20% fluorocarbon.

### Claim 7 (depends on 1)

The method of claim 1, further comprising spin-coating a polymer material on a substrate at a temperature between about 100° C. and about 300° C. to form the second organic layer.

### Claim 8

A method, comprising:
forming a first opening in a silicon-based layer and a low temperature oxide (LTO) layer;
etching, via the first opening, an organic layer below the LTO layer to form a second opening in the organic layer while removing the silicon-based layer and the LTO layer; and
etching, via the second opening, a nitrogen free anti-reflective layer (NFARL) and an interlayer dielectric (ILD) layer below the organic layer to form a third opening in the NFARL and the ILD layer while removing the organic layer.

### Claim 9 (depends on 8)

The method of claim 8, wherein etching the organic layer comprises etching the organic layer by a dry etch process using a gas mixture comprising between about 5% and about 20% hydrogen, and wherein a flow rate of hydrogen is between about 20 sccm and about 100 sccm.

### Claim 10 (depends on 8)

The method of claim 8, wherein the NFARL is formed on the LTO layer by a chemical vapor deposition (CVD) process using a gas mixture comprising silane and carbon dioxide, and wherein etching the NFARL comprises etching the NFARL by a dry etch process using a gas mixture comprising fluorocarbon, oxygen, nitrogen, and argon.

### Claim 11 (depends on 8)

The method of claim 8, wherein the ILD layer is a low-k dielectric material formed on a substrate by one of a CVD process and an atomic layer deposition (ALD) process, and wherein etching the ILD layer comprises etching the ILD layer by a dry etch process using a gas mixture comprising between about 5% and about 10% fluorocarbon.

### Claim 12

A method, comprising:
forming, between adjacent hard mask stacks, a first opening in a nitrogen free anti-reflective layer (NFARL) and an interlayer dielectric (ILD) layer, wherein each of the hard mask stacks comprises a first hard mask layer and a second hard mask layer;
etching, via the first opening, the NFARL and the ILD layer exposed outside the hard mask stacks to form a second opening in the ILD layer while removing the second hard mask layer;
etching, via the second opening, a metal oxide layer below the ILD layer to form a third opening in the ILD layer and the metal oxide layer while removing the first hard mask layer; and
etching, via the third opening, a liner and an etch stop layer (ESL) below the metal oxide layer to form a fourth opening in the ILD layer, the metal oxide layer, the liner, and the ESL while removing the NFARL, wherein the fourth opening exposes a portion of a conductive structure.

### Claim 13 (depends on 12)

The method of claim 12, wherein the first hard mask layer comprises silicon nitride, titanium nitride, and combinations thereof, and wherein the second hard mask layer comprises tetraethoxysilane and is formed by a chemical vapor deposition (CVD) process.

### Claim 14 (depends on 12)

The method of claim 12, wherein the hard mask stacks are formed by a photolithography patterning process and a chlorine based dry etch process.

### Claim 15 (depends on 12)

The method of claim 12, wherein etching the NFARL and the ILD layer comprises etching the NFARL and the ILD layer by a dry etch process at a temperature between about 10° C. and about 90° C. and at a pressure between about 15 mTorr and about 100 mTorr.

### Claim 16 (depends on 12)

The method of claim 12, wherein the metal oxide layer is formed on the liner by a CVD process, and wherein etching the metal oxide layer comprises etching the metal oxide layer by a wet etch process using hydrogen peroxide at a temperature between about 30° C. and about 100° C.

### Claim 17 (depends on 12)

The method of claim 12, wherein the liner comprises an oxygen doped carbide material and is formed on the ESL by one of a low pressure chemical vapor deposition (LPCVD) process, a plasma enhanced chemical vapor deposition (PECVD) process, and a CVD process, and wherein etching the liner comprises etching the liner by a dry etch process using a gas mixture comprising fluorocarbon, oxygen, carbon dioxide, nitrogen, and argon.

### Claim 18 (depends on 12)

The method of claim 12, wherein the ESL comprises silicon nitride, silicon oxide, and combinations thereof and is formed on the conductive structure by one of a LPCVD process, a PECVD process, a CVD process, an atomic layer deposition (ALD) process, and a high-aspect-ratio process (HARP), and wherein etching the ESL comprises etching the ESL by a dry etch process using a gas mixture comprising between about 1% and about 5% carbon dioxide.

### Claim 19 (depends on 12)

The method of claim 12, further comprising forming the conductive structure on a substrate, wherein the conductive structure comprises a contact structure, a metal line, and combinations thereof.

### Claim 20 (depends on 12)

The method of claim 12, further comprising forming an other conductive structure in the fourth opening, wherein the other conductive structure has a substantially vertical sidewall and is electrically coupled to the conductive structure.