# US 2022/0090284 A1 · Treatment Methods And Solutions For Improving Adhesion Of Gold Electroplating On Metal Surfaces

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0090284 A1
- Document ID: US20220090284A1
- Status: Published application
- Kind: A1
- Application number: 17/479,569
- Filed: 2021-09-20
- Published: 2022-03-24
- Earliest claimed: 2020-09-21
- Assignees: Hutchinson Technology Incorporated
- Applicants: Hutchinson Technology Incorporated
- Inventors: Paul V. Pesavento; Collin M. Grove; Douglas P. Riemer
- Web page: https://patentgrep.com/patent/US20220090284A1

## CPC

- C25D 5/36: of iron or steel
- C23F 1/00: Etching metallic material by chemical means (manufacture of printing surfaces B41C; manufacture of printed circuits H05K)
- C23F 1/28: for etching iron group metals
- C23F 17/00: Multi-step processes for surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by subclass C21D or C22F or class C25 (coating for obtaining at least two superposed coatings either by methods not provided for in a single one of main groups C23C2/00 - C23C26/00, or by combinations of methods providedfor in subclasses C23C and C25D, C23C28/00)
- C23G 1/19: Iron or steel
- C25D 3/48: of gold
- C23F 1/32: Alkaline compositions (C23F1/42 takes precedence)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- C23G: CLEANING OR DE-GREASING OF METALLIC MATERIAL BY CHEMICAL METHODS OTHER THAN ELECTROLYSIS

## Abstract

Treatment solutions and methods for improving adhesion of gold electroplating onto metal surfaces are provided herein. More specifically, the disclosure relates to micro-etching stainless steel surfaces using to remove any organic contamination and chromium oxide formed on the surface, neutralize and strip the surface of any iron content, and repassivate the surface with a thin chromium oxide layer, prior to gold electroplating of the stainless steel surfaces.

## Claims

### Claim 1

A method of treating stainless steel surfaces, comprising:
etching at least a portion of one or more stainless steel surfaces with an etchant solution comprised of potassium permanganate (KMnO4) and sodium hydroxide (NaOH); and
subsequently neutralizing the at least portion of one or more stainless steel surfaces with a neutralizer solution comprised of ascorbic acid and citric acid.

### Claim 2 (depends on 1)

The method of claim 1 wherein the concentration of potassium permanganate in the etchant solution is between about 0.1 M and 0.4 M, and the sodium hydroxide is added until the etchant solution has a pH greater than 12.5.

### Claim 3 (depends on 1)

The method of claim 1 wherein the concentration of ascorbic acid in the neutralizer solution is between about 75 g/L and 250 g/L, and the concentration of citric acid is between about 50 g/L and 200 g/L.

### Claim 4 (depends on 1)

The method of claim 1 wherein the at least portion of one or more stainless steel surfaces is exposed to the etchant solution for a period of time between 1 second and 5 minutes.

### Claim 5 (depends on 1)

The method of claim 1 wherein the at least portion of one or more stainless steel surfaces is exposed to the etchant solution at a temperature between 5.0 and 85 degrees Celsius.

### Claim 6 (depends on 1)

The method of claim 1 wherein the at least portion of one or more stainless steel surfaces is exposed to the neutralizer solution for a period of time between 1 and 300 seconds.

### Claim 7 (depends on 1)

The method of claim 1 wherein the at least portion of one or more stainless steel surfaces is exposed to the neutralizer solution at a temperature between 25 and 85 degrees Celsius.

### Claim 8 (depends on 1)

The method of claim 1, wherein the etching step dissolves chromium metal and converts chromium oxide, present on the at least one or more portions of the stainless steel surface, to a soluble form.

### Claim 9

A method of electroplating gold onto a stainless steel surface, the method comprising:
treating at least a portion of one or more surfaces of stainless steel by exposing the stainless steel surface to a solution comprising potassium permanganate (KMnO4) and sodium hydroxide (NaOH);
subsequently neutralizing the portion of one or more surfaces of stainless steel by exposing the stainless steel surface to a solution comprised of ascorbic acid and citric acid;
exposing the portion of one or more surfaces of stainless steel to an oxygen plasma cleaning process and a wet cleaning process solution;
immersing the stainless steel in a gold electroplating solution; and
applying a voltage between an anode within the gold electroplating solution and the stainless steel surface to generate a current from the anode to the stainless steel surface to electroplate gold from the gold electroplating solution onto the stainless steel surface.

### Claim 10 (depends on 9)

The method of claim 9, wherein the treating step dissolves chromium metal and converts chromium oxide to a soluble form.

### Claim 11 (depends on 9)

The method of claim 9, wherein the concentration of potassium permanganate in the etchant solution is between about 0.1 M and 0.4 M, and the sodium hydroxide is added until the etchant solution has a pH greater than 12.5.

### Claim 12 (depends on 9)

The method of claim 9, wherein the concentration of ascorbic acid in the neutralizer solution is between about 75 g/L and 250 g/L, and the concentration of citric acid is between about 50 g/L and 200 g/L.

### Claim 13 (depends on 9)

The method of claim 9, wherein the at least portion of one or more stainless steel surfaces is exposed to the etchant solution for a period of time between 1 and 300 seconds.

### Claim 14 (depends on 9)

The method of claim 9, wherein the at least portion of one or more stainless steel surfaces is exposed to the etchant solution at a temperature between 5.0 and 85 degrees Celsius.

### Claim 15 (depends on 9)

The method of claim 9, wherein the at least portion of one or more stainless steel surfaces is exposed to the neutralizer solution for a period of time between 1 and 300 seconds.

### Claim 16 (depends on 9)

The method of claim 9, wherein the at least portion of one or more stainless steel surfaces is exposed to the neutralizer solution at a temperature between 25 and 85 degrees Celsius.

### Claim 17 (depends on 9)

The method of claim 9, wherein the gold electroplating solution includes:
a gold (III) cyanide compound, the gold (III) cyanide compound being one of potassium gold (III) cyanide, ammonium gold (III) cyanide, and sodium gold (III) cyanide;
a chloride compound, the chloride compound being one of potassium chloride, ammonium chloride, and sodium chloride; and hydrochloric acid,
wherein if the gold (III) cyanide compound is potassium gold (III) cyanide, then the chloride compound is potassium chloride; if the gold (III) cyanide compound is ammonium gold (III) cyanide, then the chloride compound is ammonium chloride, and if the gold (III) cyanide compound is sodium gold (III) cyanide, then the chloride compound is sodium chloride.

### Claim 18 (depends on 9)

The method of claim 9, wherein the method deposits gold on a stainless steel surface of a disk drive head suspension, flexure, an optical image stabilization suspension, or a medical device.