# US 2022/0090248 A1 · Hot dip galvanized steel sheet and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0090248 A1
- Document ID: US20220090248A1
- Status: Published application
- Kind: A1
- Application number: 17/425,234
- Filed: 2020-02-06
- Published: 2022-03-24
- Earliest claimed: 2019-02-06
- Assignees: Nippon Steel Corporation
- Applicants: Nippon Steel Corporation
- Inventors: Takafumi YOKOYAMA; Hiroyuki KAWATA; Kunio HAYASHI; Yuji YAMAGUCHI; Satoshi UCHIDA
- Web page: https://patentgrep.com/patent/US20220090248A1

## CPC

- C22C 38/58: with more than 1.5% by weight of manganese
- C23C 2/12: Aluminium or alloys based thereon
- C21D 1/185: {from an intercritical temperature}
- C21D 1/19: by interrupted quenching
- C21D 1/20: Isothermal quenching, e.g. bainitic hardening
- C21D 1/25: Hardening, combined with annealing between 300 degrees Celsius and 600 degrees Celsius, i.e. heat refining ("Vergüten")
- C21D 1/26: Methods of annealing
- C21D 1/76: Adjusting the composition of the atmosphere
- C21D 8/00: Modifying the physical properties of ferrous metals or ferrous alloys by deformation combined with, or followed by, heat treatment (hardening articles or materials formed by forging or rolling with no further heating beyond that required for the formation C21D1/02)
- C21D 8/021: involving particular fabrication steps or treatments of ingots or slabs
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0436: {Cold rolling}
- C21D 9/46: for sheet metals
- C21D 9/48: deep-drawing sheets
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/008: {containing tin}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/10: containing cobalt
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/16: containing copper
- C22C 38/34: with more than 1.5% by weight of silicon
- C22C 38/38: with more than 1.5% by weight of manganese
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/52: with cobalt
- C22C 38/54: with boron
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- C23C 2/02: Pretreatment of the material to be coated, e.g. for coating on selected surface areas (C23C2/30 takes precedence)
- C23C 2/0224: {Two or more thermal pretreatments}
- C23C 2/024: {by cleaning or etching}
- C23C 2/06: Zinc or cadmium or alloys based thereon
- C23C 2/28: Thermal after-treatment, e.g. treatment in oil bath
- C23C 2/29: {Cooling or quenching}
- C23C 2/40: Plates; Strips
- C21D 2211/001: Austenite
- C21D 2211/002: Bainite
- C21D 2211/003: Cementite
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- C21D 2211/009: Pearlite
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)

## Abstract

Provided are a hot dip galvanized steel sheet comprising a base steel sheet wherein the base steel sheet has a predetermined composition and contains ferrite: 0% to 50%, retained austenite: 0% to 30%, tempered martensite: 5% or more, fresh martensite: 0% to 10%, and pearlite and cementite in total: 0% to 5%, remaining structures consist of bainite, when defining a region having a hardness of 90% or less of the hardness at a position of ¼ thickness to the base steel sheet side from an interface of the base steel sheet and a hot dip galvanized layer as a “soft layer”, there is a soft layer having a thickness of 10 μm or more at the base steel sheet side from the interface, the soft layer contains tempered martensite, and an increase rate in a thickness direction of an area % of tempered martensite from the interface to the inside of the base steel sheet inside the soft layer is 5.0%/pm or less, and a method for producing the same.

## Claims

### Claim 1

A hot dip galvanized steel sheet comprising a base steel sheet and a hot dip galvanized layer on at least one surface of the base steel sheet, wherein the base steel sheet has a chemical composition comprising, by mass %,
C: 0.050% to 0.350%,
Si: 0.10% to 2.50%,
Mn: 1.00% to 3.50%,
P: 0.050% or less,
S: 0.0100% or less,
Al: 0.001% to 1.500%,
N: 0.0100% or less,
O: 0.0100% or less,
Ti: 0% to 0.200%,
B: 0% to 0.0100%,
V: 0% to 1.00%,
Nb: 0% to 0.100%,
Cr: 0% to 2.00%,
Ni: 0% to 1.00%,
Cu: 0% to 1.00%,
Co: 0% to 1.00%,
Mo: 0% to 1.00%,
W: 0% to 1.00%,
Sn: 0% to 1.00%,
Sb: 0% to 1.00%,
Ca: 0% to 0.0100%,
Mg: 0% to 0.0100%,
Ce: 0% to 0.0100%,
Zr: 0% to 0.0100%,
La: 0% to 0.0100%,
Hf: 0% to 0.0100%,
Bi: 0% to 0.0100%,
REM other than Ce and La: 0% to 0.0100% and
a balance of Fe and impurities,
a steel microstructure at a range of ⅛ thickness to ⅜ thickness centered about a position of ¼ thickness from a surface of the base steel sheet contains, by area %,
ferrite: 0% to 50%,
retained austenite: 0% to 30%,
tempered martensite: 5% or more,
fresh martensite: 0% to 10%, and
pearlite and cementite in total: 0% to 5%,
when there are remaining structures, the remaining structures consist of bainite,
when defining a region having a hardness of 90% or less of the hardness at a position of ¼ thickness to the base steel sheet side from an interface of the base steel sheet and the hot dip galvanized layer as a “soft layer”, there is a soft layer having a thickness of 10 μm or more at the base steel sheet side from the interface,
the soft layer contains tempered martensite, and
an increase rate in a thickness direction of an area % of tempered martensite from the interface to the inside of the base steel sheet inside the soft layer is 5.0%/μm or less.

### Claim 2 (depends on 1)

The hot dip galvanized steel sheet according to claim 1, wherein the steel microstructure further contains, by area %, retained austenite: 6% to 30%.

### Claim 3 (depends on 1)

A method for producing the hot dip galvanized steel sheet according to claim 1, comprising a hot rolling step for hot rolling a slab having the chemical composition according to claim 1, a cold rolling step for cold rolling the obtained hot rolled steel sheet, and a hot dip galvanizing step for hot dip galvanizing the obtained cold rolled steel sheet, wherein
(A) the cold rolling step satisfies the conditions of the following (A1) and (A2):
(A1) a rolling line load satisfies the following formula (1) and cold rolling with a rolling reduction of 6% or more is performed one time or more:
13≤A/B≤35 (1)
(where A is the rolling line load (kgf/mm) and B is the tensile strength of the hot rolled steel sheet (kgf/mm2))
(A2) a total cold rolling reduction is 30 to 80%, and
(B) the hot dip galvanizing step comprises heating the steel sheet to first soak it, first cooling then second soaking the first soaked steel sheet, dipping the second soaked steel sheet in a hot dip galvanizing bath, second cooling the coated steel sheet, and heating the second cooled steel sheet then third soaking it, and further satisfies the conditions of the following (B1) to (B6):
(B1) in the heating of the steel sheet before the first soaking, an average heating rate from 650° C. to a maximum heating temperature of Ac1° C.+30° C. or more and 950° C. or less is 0.5° C./s to 10.0° C./s in an atmosphere satisfying the following formulas (2) and (3),
(B2) the steel sheet is held at the maximum heating temperature for 1 second to 1000 seconds (first soaking),
(B3) an average cooling rate in a temperature range of 700 to 600° C. at the first cooling is 10 to 100° C./s,
(B4) the first cooled steel sheet is held in a range of 300 to 600° C. for 80 seconds to 500 seconds in an atmosphere satisfying the following formulas (4) and (5) (second soaking),
(B5) the second cooling is performed down to Ms-50° C. or less, and
(B6) the second cooled steel sheet is heated to a temperature region of 200 to 420° C., then held in the temperature region for 5 to 500 seconds (third soaking).
−1.10 log(PH2O/PH2)≤−0.07 (2)
0.010≤PH2≤0.150 (3)
log(PH2 O/PH2)<−1.10 (4)
0.0010≤PH2≤0.1500 (5)
(where PH2 O represents the partial pressure of water vapor and PH2 represents the partial pressure of hydrogen).