# US 2022/0090229 A1 · Austenitic stainless steel containing niobium and manufacturing method of the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0090229 A1
- Document ID: US20220090229A1
- Status: Published application
- Kind: A1
- Application number: 17/537,707
- Filed: 2021-11-30
- Published: 2022-03-24
- Earliest claimed: 2018-11-13
- Assignees: Korea Advanced Institute of Science and Technology
- Applicants: Korea Advanced Institute of Science and Technology
- Inventors: Chang-Heui JANG; Ji Ho SHIN; Byeong Seo KONG; Ho-Sub KIM; Hyeon Bae LEE
- Web page: https://patentgrep.com/patent/US20220090229A1

## CPC

- C21D 9/46: for sheet metals
- C21D 6/004: {containing Cr and Ni}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 6/02: Hardening by precipitation
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C21D 2211/001: Austenite
- C21D 2211/004: Dispersions; Precipitations
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The austenitic stainless steel containing niobium according to an exemplary embodiment of the present invention includes: 16 to 26 wt. % of chromium (Cr), 8 to 22 wt. % of nickel (Ni), 0.02 to 0.1 wt. % of carbon (C), 0.2 to 1 wt. % of niobium (Nb), 0.015 to 0.025 wt. % of titanium (Ti), 0.004 to 0.01 wt. % of nitrogen (N), and 0.5 to 2 wt. % of manganese (Mn), wherein the austenitic stainless steel containing niobium has an austenitic matrix structure, a fine niobium carbide and a fine titanium nitride are precipitated in the austenitic matrix structure, and the fine niobium carbide is uniformly dispersed in the austenitic matrix structure.

## Claims

### Claim 1

A manufacturing method of an austenitic stainless steel containing niobium, the manufacturing method comprising:
a melting and casting step of melting mixed steel material and casting the melted mixed steel material to form cast steel material having an austenitic matrix structure, the mixed steel material including 16 to 26 wt. % of chromium (Cr), 8 to 22 wt. % of nickel (Ni), 0.02 to 0.1 wt. % of carbon (C), 0.2 to 1 wt. % of niobium (Nb), 0.015 to 0.025 wt. % of titanium (Ti), 0.004 to 0.01 wt. % of nitrogen (N), and 0.5 to 2 wt. % of manganese (Mn),
a step of deriving a non-recrystallization temperature by evaluating a high temperature deformation behavior of the cast steel material,
a step of performing a homogenizing heat treatment on the cast steel material,
a multi-pass hot rolling step of performing at least 1-pass hot rolling on the cast steel material at a temperature higher than the non-recrystallization temperature, and then performing at least 1-pass hot rolling on the cast steel material at a temperature lower than the non-recrystallization temperature; and
a step of precipitating a fine niobium carbide (NbC) in the austenitic matrix structure by performing a heat treatment on the hot-rolled cast steel material and then air-quenching the hot-rolled cast steel material,
wherein
the fine niobium carbide is uniformly dispersed in the austenitic matrix structure.

### Claim 2 (depends on 1)

The manufacturing method of claim 1, wherein:
in the multi-pass hot rolling step,
5- to 8-pass hot rolling is performed.

### Claim 3 (depends on 2)

The manufacturing method of claim 2, wherein:
3- to 5-pass hot rolling is performed at a temperature higher than the non-recrystallization temperature, and then 2- to 3-pass hot rolling is performed at a temperature lower than the non-recrystallization temperature.

### Claim 4 (depends on 3)

The manufacturing method of claim 3, wherein:
a running temperature of each pass is lowered by 20 to 30° C. while each pass of hot rolling is sequentially performed.

### Claim 5 (depends on 1)

The manufacturing method of claim 1, wherein:
in the melting and casting step,
a fine titanium nitride (TiN) is precipitated in the austenitic matrix structure.

### Claim 6 (depends on 1)

The manufacturing method of claim 1, wherein:
in the step of deriving the non-recrystallization temperature,
high temperature deformation behavior of the cast steel material is evaluated by a hot torsion test or a dynamic property test.