# US 2022/0068649 A1 · Bcd ic with gate etch and self-aligned implant integration

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0068649 A1
- Document ID: US20220068649A1
- Status: Published application
- Kind: A1
- Application number: 17/411,431
- Filed: 2021-08-25
- Published: 2022-03-03
- Earliest claimed: 2020-08-27
- Applicants: Texas Instruments Incorporated
- Inventors: Mona M. Eissa; Jason R. Heine; Pushpa Mahalingam; Henry Litzmann Edwards; James Robert Todd; Alexei Sadovnikov
- Web page: https://patentgrep.com/patent/US20220068649A1

## CPC

- H10P 30/22: using masks
- H10D 30/0227: {having both lightly-doped source and drain extensions and source and drain regions self-aligned to the sides of the gate, e.g. lightly-doped drain [LDD] MOSFET or double-diffused drain [DDD] MOSFET}
- H10D 30/0281: {of lateral DMOS [LDMOS] FETs}
- H10D 30/65: Lateral DMOS [LDMOS] FETs
- H10D 62/393: {Body regions of DMOS transistors or IGBTs (cell layout of DMOS H10D62/127)}
- H10D 64/516: {the thicknesses being non-uniform}
- H10D 84/0109: {the at least one component covered by H10D12/00 or H10D30/00 being a MOS device}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/401: {Combinations of FETs or IGBTs with BJTs}
- H10D 30/601: {having lightly-doped drain or source extensions, e.g. LDD IGFETs or DDD IGFETs (lightly doped source or drain extensions for TFTs H10D30/6715)}
- H10D 62/371: {Inactive supplementary semiconductor regions, e.g. for preventing punch-through, improving capacity effect or leakage current}
- H10D 64/015: {removing at least parts of gate spacers, e.g. disposable spacers}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method of fabricating an IC includes providing a substrate including a semiconductor surface having well diffusions for a plurality of devices including bipolar, complementary metal oxide semiconductor (CMOS), and double-diffused MOS (DMOS) devices. A polysilicon layer is deposited on a dielectric layer over the semiconductor surface, an anti-reflective coating (ARC) layer is formed on the polysilicon layer, and a photoresist pattern is formed on the ARC layer. The ARC layer is etched in areas exposed by the photoresist pattern to define areas including gate areas having the ARC layer on the polysilicon layer. The photoresist pattern is removed. Polysilicon etching is performed in areas lacking the ARC layer to form polysilicon gates having a remaining ARC portion of the ARC layer thereon. A self-aligned ion implant uses the remaining ARC portion as an additional implant blocking layer for the polysilicon gates, and the remaining ARC portion is stripped.

## Claims

### Claim 1

A method of fabricating an integrated circuit (IC), comprising:
depositing a polysilicon layer on a dielectric layer over a semiconductor substrate;
forming an anti-reflective coating (ARC) layer on the polysilicon layer;
forming a photoresist pattern on the ARC layer;
etching the ARC layer in areas exposed by the photoresist pattern to define areas including gate areas having the ARC layer on the polysilicon layer;
removing the photoresist pattern;
etching the polysilicon layer in areas lacking the ARC layer to form polysilicon gates having a remaining ARC portion of the ARC layer thereon;
performing at least one self-aligned ion implantation using the remaining ARC portion as an additional implant blocking layer for the polysilicon gates, and
stripping the remaining ARC portion.

### Claim 2 (depends on 1)

The method of claim 1, further comprising before stripping the remaining ARC portion forming a spacer on sidewalls of the polysilicon gates and then performing an additional ion implant.

### Claim 3 (depends on 1)

The method of claim 1, wherein after the etching of the polysilicon layer i) a thickness of the remaining ARC portion is at least 50% of a thickness of the ARC layer before the etching of the polysilicon layer, and ii) the remaining ARC portion is at a sidewall taper angle of at least 80 degrees relative to a top surface of the polysilicon gates.

### Claim 4 (depends on 1)

The method of claim 1, wherein the etching of the polysilicon layer comprises a plasma etch configured for etching polysilicon.

### Claim 5 (depends on 1)

The method of claim 1, wherein the IC includes at least one laterally diffused metal oxide semiconductor (LDMOS) device.

### Claim 6 (depends on 1)

The method of claim 1, wherein a thickness of the ARC layer immediately following the forming the ARC layer on the polysilicon layer is in a range from 800 to 2,500 Å, and wherein the ARC layer comprises silicon nitride.

### Claim 7 (depends on 1)

The method of claim 1, wherein the forming of the ARC layer comprises forming a bottom ARC layer and then forming a top ARC layer on the bottom ARC layer that is a different material compared to the bottom ARC layer.

### Claim 8 (depends on 7)

The method of claim 7, wherein the bottom ARC layer comprises silicon rich silicon nitride, and wherein the top ARC layer comprises silicon nitride.

### Claim 9 (depends on 1)

The method of claim 1, further comprising trimming the photoresist pattern to narrow a line width.

### Claim 10 (depends on 1)

The method of claim 1, further comprising before the etching of the ARC layer:
obtaining critical dimensions (CDs) of the photoresist pattern for a plurality of wafers in a wafer lot each having a plurality of the IC die;
trimming the photoresist pattern of selected first ones of the plurality of wafers as test wafers with trim times based on the CDs for each of the test wafers;
polysilicon etching the test wafers after trimming the photoresist pattern;
measuring a gate CD of the test wafers after the polysilicon etching of the test wafers;
using the gate CDs of the test wafers to calculate adjusted trim times for remaining others of the plurality of wafers in the wafer lot;
selecting at least one wafer from the remaining others of the plurality of wafers for the polysilicon etching and then measuring a post etch CD, and
using the post etch CD to select a trim time for a trimming of the photoresist pattern for a next lot of wafers.

### Claim 11

A method of fabricating an integrated circuit (IC), comprising:
providing a substrate including a semiconductor surface having well diffusions for a plurality of devices, the plurality of devices including bipolar, complementary metal oxide semiconductor (CMOS), and double-diffused MOS (DMOS) devices;
depositing a polysilicon layer on a dielectric layer over the semiconductor surface;
forming anti-reflective coating (ARC) layers on the polysilicon layer comprising forming a bottom ARC layer and then forming a top ARC layer on the bottom ARC layer that is a different material compared to the bottom ARC layer;
forming a photoresist pattern on the top ARC layer;
etching the ARC layers in areas exposed by the photoresist pattern to define areas including gate areas having the ARC layers on the polysilicon layer;
removing the photoresist pattern;
etching the polysilicon layer in areas lacking the ARC layers to form polysilicon gates having a remaining ARC portion of the ARC layer thereon, wherein a thickness of the remaining ARC portion is at least 50% of a thickness of the ARC layers before the etching of the polysilicon layer, and wherein the remaining ARC portion is at a sidewall taper angle of at least 80 degrees relative to a top surface of the polysilicon gates;
performing at least one self-aligned ion implantation using the remaining ARC portion as an additional implant blocking layer for the polysilicon gates,
forming a spacer on sidewalls of the polysilicon gates and then performing an additional ion implant, and
stripping the remaining ARC portion.

### Claim 12 (depends on 11)

The method of claim 11, wherein the bottom ARC layer comprises silicon rich silicon nitride, and wherein the top ARC layer comprises silicon nitride.

### Claim 13 (depends on 11)

The method of claim 11, wherein a total thickness of the bottom and the top ARC layers immediately following the forming the ARC layers is in a range from 800 to 2,500 Å.

### Claim 14 (depends on 11)

The method of claim 11, further comprising trimming the photoresist pattern to narrow a line width.

### Claim 15 (depends on 14)

The method of claim 14, further comprising before the etching of the ARC layer:
obtaining critical dimensions (CDs) of the photoresist pattern for a plurality of wafers in a wafer lot each having a plurality of the IC die;
trimming the photoresist pattern of selected first ones of the plurality of wafers as test wafers with trim times based on the CDs for each of the test wafers;
polysilicon etching the test wafers after trimming the photoresist pattern;
measuring a gate CD of the test wafers after the polysilicon etching of the test wafers;
using the gate CDs of the test wafers to calculate adjusted trim times for the remaining others of the plurality of wafers in the wafer lot;
selecting at least one wafer from the remaining others of the plurality of wafers for the polysilicon etching and then measuring a post etch CD, and
using the post etch CD to select a trim time for a trimming of the photoresist pattern for a next lot of wafers.

### Claim 16 (depends on 11)

The method of claim 11, wherein the DMOS devices include at least one laterally diffused metal oxide semiconductor (LDMOS) device.

### Claim 17 (depends on 11)

The method of claim 11, wherein the etching of the polysilicon layer comprises a plasma etch configured for etching polysilicon.

### Claim 18

An integrated circuit (IC), comprising:
a complementary metal oxide semiconductor (CMOS) device including a polysilicon gate layer that has a thickness less than 1,500 Å which is on a gate dielectric layer, with a source and drain structure, having a drawn channel length of less than (<) 0.8 μm;
a double diffused MOSFET (DMOS) device having a gate stack with the polysilicon gate layer on the gate dielectric layer, and having a drift region separating a drain region from a source region with an effective channel length (Leff) of less than (<) 0.4 μm defined as a spacing between the drift region and the source region, and
a bipolar device including at least one diffusion common to at least one of the CMOS devices and the DMOS device.

### Claim 19 (depends on 18)

The IC of claim 18, wherein the thickness of the polysilicon gate layer is less than 1,300 Å.

### Claim 20 (depends on 18)

The IC of claim 18, wherein the DMOS device includes at least one laterally diffused metal oxide semiconductor (LDMOS) device.