# US 2022/0064814 A1 · Zinc electrolyte devoid of boric acid and ammonium for the electrodeposition of zinc coatings

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0064814 A1
- Document ID: US20220064814A1
- Status: Published application
- Kind: A1
- Application number: 17/312,812
- Filed: 2019-12-09
- Published: 2022-03-03
- Earliest claimed: 2018-12-12
- Assignees: Dr.-lng. Max Schlötter GmbH & Co. KG
- Applicants: Dr.-lng. Max Schlötter GmbH & Co. KG
- Inventors: Ralph Krauss; Vera Lipp; Ingo Messerschmid
- Web page: https://patentgrep.com/patent/US20220064814A1

## CPC

- C25D 21/14: Controlled addition of electrolyte components
- C25D 3/22: of zinc
- C25D 3/565: {containing more than 50% by weight of zinc}
- C25D 5/48: After-treatment of electroplated surfaces
- C25D 5/50: by heat-treatment
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

The invention relates to an aqueous electrolyte devoid of boric acid and ammonium for the electrodeposition of zinc coatings and to a method for producing such an electrolyte. The electrolyte comprises (a) Zn2+ in a concentration of 15 to 70 g/L; (b) Cl− in a concentration of 100 to 200 g/L; (c) K+ and/or Na+ in a total concentration of 0.75 to 6.0 mol/L; (d) acetate in a concentration of 5.0 to 45 g/L; (e) glycine and/or alanine in a total concentration of 0.5 to 30 g/L; and (f) water. The electrolyte has a pH of 4.5 to 6.5. In a preferred variant, the electrolyte contains (g) nicotinic acid and/or (h) ethoxylated thiodiglycol. The invention also relates to a method for producing a component having a zinc coating, which uses the electrolyte.

## Claims

### Claim 1

An aqueous electrolyte devoid of boric acid and ammonium for the electrodeposition of zinc coatings, comprising:
(a) Zn2+ in a concentration of 15 to 70 g/L;
(b) Cl− in a concentration of 100 to 200 g/L;
(c) K+ and/or Na+ in a total concentration of 0.75 to 6.0 mol/L;
(d) acetate in a concentration of 5.0 to 45 g/L;
(e) glycine and/or alanine in a total concentration of 0.5 to 30 g/L; and
(f) water;
wherein the electrolyte has a pH of 4.5 to 6.5.

### Claim 2 (depends on 1)

The electrolyte according to claim 1, wherein the concentration of Zn2+ in the electrolyte is 20 to 60 g/L, preferably 25 to 50 g/L, more preferably 30 to 40 g/L and most preferably 35 g/L.

### Claim 3 (depends on 1)

The electrolyte according to claim 1, wherein the concentration of Cl− in the electrolyte is 120 to 190 g/L, preferably 130 to 180 g/L and more preferably 160 g/L.

### Claim 4 (depends on 1)

The electrolyte according to claim 1, wherein the electrolyte contains K+ and the concentration of K+ is 0.75 to 6.0 mol/L, preferably 2.7 to 4.8 mol/L and more preferably 3.3 to 4.1 mol/L.

### Claim 5 (depends on 1)

The electrolyte according to claim 1, wherein the concentration of acetate in the electrolyte is 7.5 to 30 g/L, preferably 10 to 20 g/L, most preferably 12 g/L.

### Claim 6 (depends on 1)

The electrolyte according to claim 1, wherein the total concentration of glycine and/or alanine in the electrolyte is in the range of 0.5 to 20 g/L, preferably 1.0 to 10 g/L, more preferably 1.5 to 5 g/L and most preferably 2.5 g/L.

### Claim 7 (depends on 1)

The electrolyte according to claim 1, wherein the electrolyte contains
(a) Zn2+ in a concentration of 20 to 60 g/L;
(b) Cl− in a concentration of 120 to 190 g/L;
(c) K+ in a concentration of 2.7 to 4.8 mol/L and 0 to 0.5 mol/L Nat;
(d) acetate in a concentration of 7.5 to 30 g/L; and
(e) glycine and/or alanine in a total concentration of 0.5 to 20 g/L.

### Claim 8 (depends on 1)

The electrolyte according to claim 1, wherein the electrolyte additionally contains (g) nicotinic acid in a concentration of 0.01 to 2.0 g/L, preferably 0.05 to 1.0 g/L, more preferably 0.08 to 0.5 g/L, most preferably 0.1 g/L.

### Claim 9 (depends on 1)

The electrolyte according to claim 1, wherein the electrolyte additionally contains (h) ethoxylated thiodiglycol, with an average of at least 20 structural units derived from ethylene oxide, in a concentration of 0.3 to 10 g/L, preferably 0.5 to 5 g/L, more preferably 1.0 to 3.5 g/L and most preferably 2.1 g/L.

### Claim 10 (depends on 1)

The electrolyte according to claim 1, wherein the electrolyte contains
(g) nicotinic acid in a concentration of 0.05 to 1.0 g/L, and/or
(h) ethoxylated thiodiglycol, with an average of at least 20 structural units derived from ethylene oxide, in a concentration of 0.5 to 5 g/L.

### Claim 11 (depends on 1)

A method for producing an aqueous electrolyte according to claim 1, comprising the steps of:
A) forming an aqueous solution of
(a′) zinc chloride and/or zinc acetate;
(b′) potassium chloride and/or sodium chloride;
(c′) at least one of potassium acetate, sodium acetate and acetic acid;
(d′) at least one from the group consisting of glycine, a salt thereof, alanine and a salt thereof; and
(e′) optionally nicotinic acid or a salt thereof; and
(f′) optionally ethoxylated thiodiglycol, with an average of at least 20 structural units derived from ethylene oxide; and
B) optionally setting the pH to 4.5 to 6.5 by adding hydrochloric acid or by adding potassium hydroxide and/or sodium hydroxide, which can be added as solids or in the form of an aqueous solution.

### Claim 12 (depends on 1)

A method for producing a component having a zinc coating, comprising the electrodeposition of zinc on a metal component from an electrolyte according to claim 1.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the metal component comprises or consists of iron or an iron alloy.

### Claim 14 (depends on 12)

The method according to claim 12, wherein deposition occurs at a temperature of 20 to 50° C., preferably 25 to 40° C., and
a current density of 0.2 to 10 A/dm2, preferably 0.5 to 6 A/dm2, is used for the deposition.

### Claim 15 (depends on 12)

The method according to claim 12, wherein after the electrodeposition the component having a zinc coating is subjected to a passivation treatment.

### Claim 16 (depends on 12)

The method according to claim 12, wherein after the electrodeposition the component having a zinc coating is annealed, optionally before or after a passivation treatment.