# US 2022/0064054 A1 · Crystallized glass of three-dimensional shape, chemically strengthened glass of three-dimensional shape, and method for producing crystallized glass of three-dimensional shape and chemically strengthened glass of three-dimensional shape

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0064054 A1
- Document ID: US20220064054A1
- Status: Published application
- Kind: A1
- Application number: 17/525,554
- Filed: 2021-11-12
- Published: 2022-03-03
- Earliest claimed: 2018-02-27
- Assignees: AGC Inc.
- Applicants: AGC Inc.
- Inventors: Qing LI; Kenji IMAKITA; Akio KOIKE; Eriko MAEDA
- Web page: https://patentgrep.com/patent/US20220064054A1

## CPC

- C03C 3/076: with 40% to 90% silica, by weight {(C03C3/045 takes precedence)}
- C03C 10/0027: {containing SiO2, Al2O3, Li2O as main constituents}
- C03B 23/023: by bending
- C03B 23/0252: {by gravity only, e.g. sagging (C03B23/035 takes precedence)}
- C03B 23/0302: {between opposing full-face shaping moulds}
- C03B 23/0357: {by suction without blowing, e.g. with vacuum or by venturi effect}
- C03B 32/02: Thermal crystallisation, e.g. for crystallising glass bodies into glass-ceramic articles {(C03B27/012 takes precedence)}
- C03C 1/004: {Refining agents (refining C03B5/225)}
- C03C 3/085: containing an oxide of a divalent metal
- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 4/0028: {for crystal glass, e.g. lead-free crystal glass}
- C03C 10/0054: {containing PbO, SnO2, B2O3}
- C03C 21/00: Treatment of glass, not in the form of fibres or filaments, by diffusing ions or metals in the surface
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 2204/00: Glasses, glazes or enamels with special properties
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

The present invention provides crystallized glass of three-dimensional shape for easily producing chemically strengthened glass of three-dimensional shape that resists damage and has exceptional transparency. This crystallized glass of three-dimensional shape: contains crystals; has light transmittance in terms of a thickness of 0.8 mm of 80% or higher; and contains 45-74% SiO2, 1-30% Al2O3, 1-25% Li2O, 0-10% Na2O, 0-5% K2O, a total of 0-15% of SnO2 and/or ZrO2, and 0-12% P2O5, these amounts expressing the oxide-based mass percentage.

## Claims

### Claim 1

A crystallized glass for a cover glass for a mobile device, comprising a petalite crystal and a lithium disilicate crystal,
having an average transmittance of a light at a wavelength of 380 nm to 780 nm of 80% or more in terms of a thickness of 0.8 mm, and
having a Young's modulus of 90 GPa or more.

### Claim 2 (depends on 1)

The crystallized glass according to claim 1, wherein the Young's modulus is 100 GPa or more.

### Claim 3 (depends on 1)

The crystallized glass according to claim 1, wherein the average transmittance is 85% or more.

### Claim 4 (depends on 1)

The crystallized glass according to claim 1, having a fracture toughness value of 0.8 MPa·m1/2 or more.

### Claim 5 (depends on 1)

The crystallized glass according to claim 1, having a haze value in terms of a thickness of 0.8 mm of 1% or less.

### Claim 6 (depends on 1)

The crystallized glass according to claim 1, having a Vickers hardness of 680 or more.

### Claim 7 (depends on 1)

The crystallized glass according to claim 1, having a Vickers hardness of 700 or more.

### Claim 8 (depends on 1)

The crystallized glass according to claim 1, comprising, in mass % on an oxide basis:
from 45 to 74% of SiO2; and
from 4 to 11.2% of Li2O.

### Claim 9 (depends on 1)

The crystallized glass according to claim 1, comprising, in mass % on an oxide basis, from 5 to 8% of Al2O3.

### Claim 10 (depends on 1)

The crystallized glass according to claim 1, comprising, in mass % on an oxide basis, from 1 to 10% in total of either one or more of SnO2 and ZrO2.

### Claim 11 (depends on 1)

The crystallized glass according to claim 1, comprising, in mass % on an oxide basis, from 1 to 7% of P2O5.

### Claim 12 (depends on 1)

The crystallized glass according to claim 1, being a chemically strengthened glass having a compressive stress layer on a surface thereof

### Claim 13 (depends on 1)

The crystallized glass according to claim 1, having an average thermal expansion coefficient at 50° C. to 350° C. of 10×10−7° C. or more and 160×10−7° C. or less.

### Claim 14 (depends on 1)

The crystallized glass according to claim 1, comprising no lithium metasilicate as a result of identification of a precipitated crystal by measurement of powder X-ray diffractometry under the following conditions.
Measurement method for powder X-ray diffractometry:
Measurement apparatus: SmartLab manufactured by Rigaku Corporation
X-Ray: CuKα radiation
Measurement Range: 2θ=from 10° to 80°
Speed: 10°/min
Step: 0.02°

### Claim 15 (depends on 1)

The crystallized glass according to claim 1, being a chemically strengthened glass.

### Claim 16 (depends on 15)

The crystallized glass according to claim 15, having m1 of −50 MPa/μm or less, m2 of −5 MPa/μm or more and −0.3 MPa/μm or less, and m3 of −5 MPa/μm or more and −0.3 MPa/μm or less,
wherein m1 is an inclination of a stress profile from a surface of the crystallized glass to a depth DOL1, represented by the following expression (1):
m1=(CS−CS/2)/(0−DOL1) (1)
where CS is a compressive stress value at the surface of the crystallized glass, DOL is a depth of the compressive stress at which the compressive stress value is zero, and DOL1 is a depth at which the compressive stress value is CS/2,
wherein m2 is an inclination of the stress profile from a depth DOL/4 to a depth DOL/2, represented by the following expression (2):
m2=(CS1−CS2)/(DOL/4−DOL/2) (2)
where CS1 is the compressive stress value at the depth DOL/4 from the surface of the crystallized glass, and CS2 is the compressive stress value at the depth DOL/2 from the surface of the crystallized glass, and
wherein m3 is an inclination of the stress profile from the depth DOL/2 to the depth DOL, represented by the following expression (3):
m3=(CS2−0)/(DOL/2−DOL) (3).

### Claim 17 (depends on 16)

The crystallized glass according to claim 16, having a ratio m2/m3 of the inclination m2 to the inclination m3 of 0.3 or more and 2 or less.

### Claim 18 (depends on 1)

The crystallized glass according to claim 1, being a three-dimensionally shaped crystallized glass.

### Claim 19

A production method of a crystallized glass for a cover glass for a mobile device, the method comprising:
heating a glass at a first treatment temperature of 540° C., at a second treatment temperature of 600° C., and at a third treatment temperature of 710° C. in this order for crystallizing the glass,
wherein the glass comprises, in mass % on an oxide basis:
from 45 to 74% of SiO2;
from 5 to 8% of Al2O3;
from 4 to 11.2% of Li2O;
from 1 to 10% in total of either one or more of SnO2 and ZrO2; and
from 1 to 7% of P2O5.

### Claim 20 (depends on 19)

The production method of a crystallized glass according to claim 19, wherein a treatment time for each of the first treatment temperature, the second treatment temperature, and the third treatment temperature is 4 hours.