# US 2022/0045419 A1 · Three-dimensional graphene antenna and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0045419 A1
- Document ID: US20220045419A1
- Status: Published application
- Kind: A1
- Application number: 17/505,653
- Filed: 2021-10-20
- Published: 2022-02-10
- Earliest claimed: 2020-12-31
- Assignees: Xi'an Technological University
- Applicants: Xi'an Technological University
- Inventors: Huan Liu; Jijie Zhao; Jinmei Jia; Yuxuan Du; Shuai Wen; Minyu Bai; Fei Xie; Wanpeng Xie; Weiguo Liu
- Web page: https://patentgrep.com/patent/US20220045419A1

## CPC

- H01Q 1/368: {using carbon or carbon composite}
- C01B 32/184: Preparation
- H01Q 9/0407: {Substantially flat resonant element parallel to ground plane, e.g. patch antenna (dipole H01Q9/285; monopole H01Q9/40)}
- C01B 32/194: After-treatment
- C01B 2204/22: Electronic properties
- C01B 2204/24: Thermal properties
- H01Q: ANTENNAS, i.e. RADIO AERIALS (radiators or antennas for microwave heating H05B6/72)
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}

## Abstract

A three-dimensional graphene antenna includes a three-dimensional graphene radiation layer, a dielectric substrate, a metal layer and a feeder line. The three-dimensional graphene radiation layer is made from porous three-dimensional graphene. A preparation method of the porous three-dimensional graphene includes steps of preparing pressurized solid particles by pressurizing gas into solid micro particles, mixing the pressurized solid particles with a graphene oxide dispersion liquid, removing liquid nitrogen under high pressure and low temperature such that the graphene oxide flakes enwrap around the pressurized solid particles, obtaining a graphene oxide block containing the pressurized solid particles by extruding, sublimating the pressurized solid particles in the graphene oxide block into gas, forming holes in the graphene oxide block and annealing, thereby obtaining the three-dimensional graphene. The three-dimensional graphene has a porous three-dimensional conductive network structure, which is able to be in any shape without any pollution.

## Claims

### Claim 1

A three-dimensional graphene antenna, which comprises a three-dimensional graphene radiation layer (1), a dielectric substrate (3), a metal layer (4) and a feeder line (2), wherein the three-dimensional graphene radiation layer (1) is attached to a top surface of the dielectric substrate (3), the metal layer (4) is attached to a bottom surface of the dielectric substrate (3), the feeder line (2) is provided at one side of the three-dimensional graphene radiation layer (1) and on the dielectric substrate (3).

### Claim 2 (depends on 1)

The three-dimensional graphene antenna according to claim 1, wherein the three-dimensional graphene radiation layer (1) is made from porous three-dimensional graphene.

### Claim 3 (depends on 1)

The three-dimensional graphene antenna according to claim 1, wherein the dielectric substrate (3) is made from a low dielectric constant material with a dielectric constant lower than 2.7.

### Claim 4 (depends on 1)

A preparation method of the three-dimensional graphene antenna according to claim 1, wherein the preparation method comprises steps of:
(A) selecting a material with low dielectric constant as a dielectric substrate (3);
(B) preparing the three-dimensional graphene radiation layer (1) which comprises:
(B1) under low temperature and high pressure, pressurizing gas whose intermolecular force is greater than repulsive force into a solid, and crushing the solid into solid micro particles which are pressurized solid particles;
(B2) preparing graphene flakes with Hummers method, obtaining a graphene oxide dispersion liquid by distributing the graphene flakes in liquid nitrogen below −200° C. under the high pressure and the low temperature;
(B3) obtaining a mixed solution containing the pressurized solid particles and the graphene oxide flakes by adding the pressurized solid particles into the graphene oxide dispersion liquid, removing the liquid nitrogen in the mixed solution and the graphene oxide flakes enwrapping around the pressurized solid particles by increasing a temperature of the mixed solution under the high pressure, wherein the increased temperature is lower than a sublimation temperature of the pressurized solid particles, such that the pressurized solid particles exist stably, and obtaining a graphene oxide block containing the pressurized solid particles by extruding after all of the graphene oxide flakes in the mixed solution enwrapping around the pressurized solid particles; and
(B4) sublimating the pressurized solid particles in the graphene oxide block into gas by increasing a temperature and decreasing a pressure of the graphene oxide block, forming holes in the graphene oxide block, obtaining the porous three-dimensional graphene by annealing in a vacuum condition, and obtaining the three-dimensional graphene radiation layer (1) by transferring the porous three-dimensional graphene to the top surface of the dielectric substrate (3); and
(C) preparing the feeder line (2) and the metal layer (4), which comprises:
(C1) plating a layer of metal on the bottom surface of the dielectric substrate (3) as the metal layer (4), wherein a stable radiation field is formed between the metal layer (4) and the three-dimensional graphene radiation layer (1); and
(C2) depositing a metal strip as the feeder line (2) at one side of the three-dimensional graphene radiation layer (1) for transmitting signals produced by the radiation field, thereby obtaining the three-dimensional graphene antenna.

### Claim 5 (depends on 4)

The preparation method according to claim 4, wherein the low temperature is in a range of −30° C. and −100° C., and the high pressure is in a range of 0.3 Pa and 5 Pa.

### Claim 6 (depends on 4)

The preparation method according to claim 4, wherein the pressurized solid particles have a size in a range of 50 nm and 1 μm.

### Claim 7 (depends on 4)

The preparation method according to claim 4, wherein in the step (B3), the liquid nitrogen in the mixed solution is removed by increasing the temperature in a range of −200° C. and −120° C., which is able to ensure volatilization of the liquid nitrogen, and the solid micro particles formed by gas condensation do not volatilized.

### Claim 8 (depends on 4)

The preparation method according to claim 4, wherein a density of the holes is determined by a quantity of the solid micro particles in the graphene oxide dispersion liquid.

### Claim 9 (depends on 4)

The preparation method according to claim 4, wherein a size of each of the holes is determined by a size of each of the solid micro particles.