# US 2022/0045356 A1 · Method for producing lithium titanium phosphate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0045356 A1
- Document ID: US20220045356A1
- Status: Published application
- Kind: A1
- Application number: 17/415,127
- Filed: 2020-01-27
- Published: 2022-02-10
- Earliest claimed: 2019-01-29
- Assignees: Nippon Chemical Industrial Co., Ltd.
- Applicants: Nippon Chemical Industrial Co., Ltd.
- Inventors: Junya Fukazawa; Toru Hata; Takuma Kato
- Web page: https://patentgrep.com/patent/US20220045356A1

## CPC

- H01M 10/0562: Solid materials
- C01B 25/45: containing plural metal, or metal and ammonium
- C04B 35/447: based on phosphates {, e.g. hydroxyapatite}
- H01B 13/00: Apparatus or processes specially adapted for manufacturing conductors or cables
- H01M 10/052: Li-accumulators
- B01J 2/06: in a liquid medium
- C01P 2002/50: Solid solutions
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/82: by IR- or Raman-data
- C01P 2004/03: obtained by SEM
- C01P 2006/40: Electric properties
- H01M 2300/0068: inorganic
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

An X-ray diffractometrically single-phase lithium titanium phosphate can be obtained by an industrially advantageous method. Provided is a method for producing the lithium titanium phosphate having a NASICON structure represented by the following general formula (1): Li1+xMx(Ti1−yAy)2−x(PO4)3 (1), and provided is a method comprising a first step of preparing a raw material mixed slurry (1) comprising, at least, titanium dioxide, phosphoric acid and a surfactant, a second step of heat treating the raw material mixed slurry (1) to obtain a raw material heat-treated slurry (2), a third step of mixing the raw material heat-treated slurry (2) with a lithium source to obtain a lithium-containing raw material heat-treated slurry (3), a fourth step of subjecting the lithium-containing raw material heat-treated slurry (3) to a spray drying treatment to obtain a reaction precursor containing, at least, Ti, P and Li, and a fifth step of firing the reaction precursor.

## Claims

### Claim 1

A method for producing a lithium titanium phosphate having a NASICON structure represented by the following general formula (1):
Li1+xMx(Ti1−yAy)2−x(PO4)3 (1)
wherein 0≤x≤1.0 and 0 ≤y≤0.5; M denotes one or two or more divalent or trivalent metal elements selected from Al, Ga, Sc, Y, La, Fe, Cr, Ni, Mn, In and Co; and A denotes one or two or more tetravalent or pentavalent metal elements selected from Ge, Zr, V, Nb, Sn and Si,
the method comprising:
a first step of preparing a raw material mixed slurry (1) comprising at least titanium dioxide, phosphoric acid, a polycarboxylic acid surfactant and a solvent;
a second step of heat treating the raw material mixed slurry (1) to obtain a raw material heat-treated slurry (2);
a third step of mixing the raw material heat-treated slurry (2) with a lithium source to obtain a lithium-containing raw material heat-treated slurry (3);
a fourth step of subjecting the lithium-containing raw material heat-treated slurry (3) to a spray drying treatment to obtain a reaction precursor comprising at least Ti, P and Li; and a fifth step of firing the reaction precursor.

### Claim 2 (depends on 1)

The method for producing a lithium titanium phosphate according to claim 1, wherein in the first step (1), an M source (M denotes one or two or more divalent or trivalent metal elements selected from Al, Ga, Sc, Y, La, Fe, Cr, Ni, Mn, In and Co) and/or an A source (A denotes one or two or more tetravalent or pentavalent metal elements selected from Ge, Zr, V, Nb, Sn and Si) are further contained in the raw material mixed slurry (1).

### Claim 3 (depends on 1)

The method for producing a lithium titanium phosphate according to claim 1, wherein the heat-treated slurry (2) or the lithium-containing heat-treated slurry (3) is further mixed with an M source (M denotes one or two or more divalent or trivalent metal elements selected from Al, Ga, Sc, Y, La, Fe, Cr, Ni, Mn, In and Co) and/or an A source (A denotes one or two or more tetravalent or pentavalent metal elements selected from Ge, Zr, V, Nb, Sn and Si).

### Claim 4 (depends on 1)

The method for producing a lithium titanium phosphate according to claim 1, wherein the titanium dioxide is an anatase type.

### Claim 5

(canceled)

### Claim 6

(canceled)

### Claim 7 (depends on 1)

The method for producing a lithium titanium phosphate according to claim 1, wherein a temperature of the heat treatment in the second step is 50 to 120° C.

### Claim 8 (depends on 1)

The method for producing a lithium titanium phosphate according to claim 1, wherein the reaction precursor has a peak observed at around 975 cm−1 in Raman spectrometry.

### Claim 9 (depends on 1)

The method for producing a lithium titanium phosphate according to claim 1, wherein the M source is an Al-containing compound.

### Claim 10 (depends on 9)

The method for producing a lithium titanium phosphate according to claim 9, wherein the Al-containing compound is aluminum biphosphate.

### Claim 11 (depends on 1)

The method for producing a lithium titanium phosphate according to claim 1, wherein the M source is a Cr-containing compound.

### Claim 12 (depends on 11)

The method for producing a lithium titanium phosphate according to claim 11, wherein the Cr-containing compound is chromium phosphate.