# US 2022/0045333 A1 · Current collector for lithium ion battery and manufacturing method of the current collector

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0045333 A1
- Document ID: US20220045333A1
- Status: Published application
- Kind: A1
- Application number: 17/417,024
- Filed: 2020-09-03
- Published: 2022-02-10
- Earliest claimed: 2019-11-01
- Assignees: Gunze Limited; Apb Corporation
- Applicants: Gunze Limited; APB Corporation
- Inventors: Kazuaki ONISHI; Masahiro UCHIMARU; Ryosuke KUSANO; Sonomi FUKUYAMA; Shun KUDOH; Yasuhiro TSUDO; Hideaki HORIE
- Web page: https://patentgrep.com/patent/US20220045333A1

## CPC

- H01M 4/668: {Composites of electroconductive material and synthetic resins}
- C23C 26/00: Coating not provided for in groups C23C2/00 - C23C24/00
- C23C 28/00: Coating for obtaining at least two superposed coatings either by methods not provided for in a single one of groups C23C2/00 - C23C26/00 or by combinations of methods provided for in subclasses C23C and C25C or C25D
- H01M 4/0433: {Molding}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 4/663: {containing carbon or carbonaceous materials as conductive part, e.g. graphite, carbon fibres}
- H01M 4/667: {in the form of layers, e.g. coatings}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A current collector for a lithium ion battery includes a first conductive resin layer and a second conductive resin layer. The first conductive resin layer includes a first conductive filler. The second conductive resin layer is formed on the first conductive resin layer and includes a second conductive filler. The first conductive filler is a conductive carbon. The second conductive filler contains at least one kind of metal element selected from the group consisting of platinum, gold, silver, copper, nickel, and titanium. A volume % of the second conductive filler in the second conductive resin layer on a first surface side, which is a first conductive resin layer side, is higher than that on the second surface side that is opposite to the first conductive resin layer.

## Claims

### Claim 1

A current collector for a lithium ion battery comprising:
a first conductive resin layer containing a first conductive filler; and
a second conductive resin layer that is formed on the first conductive resin layer and contains a second conductive filler,
wherein the first conductive filler is a conductive carbon,
the second conductive filler contains at least one kind of metal element selected from the group consisting of platinum, gold, silver, copper, nickel, and titanium,
a surface of the first conductive resin layer on a side opposite to the second conductive resin layer is a first surface,
a surface of the second conductive resin layer on a side opposite to the first conductive resin layer is a second surface,
a volume % of the second conductive filler in the second conductive resin layer on the first conductive resin layer side is higher than that on the second surface side,
a specific heat capacity Cp in a 40° C. environment is at least 0.9 mJ/mg·° C. and at most 2.2 mJ/mg·° C., and
a surface resistance value of the second surface is at least 1Ω/□ and at most 2 Ω/□.

### Claim 2 (depends on 1)

The current collector for a lithium ion battery according to claim 1, further comprising a metal coating layer formed on the second surface.

### Claim 3 (depends on 1)

The current collector for a lithium ion battery according to claim 1, wherein a surface resistance value of the first surface is at least 0.9Ω/□ and at most 8Ω/□.

### Claim 4 (depends on 1)

The current collector for a lithium ion battery according to claim 1, wherein a thickness of the first conductive resin layer is 80% or less of a sum of the thickness of the first conductive resin layer and a thickness of the second conductive resin layer.

### Claim 5

A manufacturing method of a current collector for a lithium ion battery, comprising:
a step of forming a first conductive resin layer containing a first conductive filler; and
a step of forming a second conductive resin layer containing a second conductive filler, on the first conductive resin layer,
wherein the first conductive filler is a conductive carbon,
the second conductive filler includes at least one kind of metal element selected from the group consisting of platinum, gold, silver, copper, nickel, and titanium,
a surface of the first conductive resin layer on a side opposite to the second conductive resin layer is a first surface,
a surface of the second conductive resin layer on a side opposite to the first conductive resin layer is a second surface,
a volume % of the second conductive filler in the second conductive resin layer on the first conductive resin layer side is higher than that on the second surface side,
the manufacturing method further comprises a step of controlling a specific heat capacity Cp in a 40° C. environment of the current collector for a lithium ion battery and a surface resistance value of the second surface to target values by adjusting the volume % of the second conductive filler in the second conductive resin layer,
the target value of the specific heat capacity is at least 0.9 mJ/mg·° C. and at most 2.2 mJ/mg·° C., and
the target value of the surface resistance value of the second surface is at least 1Ω/□ and at most 2Ω/□.

### Claim 6 (depends on 2)

The current collector for a lithium ion battery according to claim 2, wherein a surface resistance value of the first surface is at least 0.9Ω/□ and at most 8Ω/□.

### Claim 7 (depends on 2)

The current collector for a lithium ion battery according to claim 2, wherein a thickness of the first conductive resin layer is 80% or less of a sum of the thickness of the first conductive resin layer and a thickness of the second conductive resin layer.

### Claim 8 (depends on 3)

The current collector for a lithium ion battery according to claim 3, wherein a thickness of the first conductive resin layer is 80% or less of a sum of the thickness of the first conductive resin layer and a thickness of the second conductive resin layer.