# US 2022/0045324 A1 · Pressure-resistant positive active material and electrochemical energy storage apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0045324 A1
- Document ID: US20220045324A1
- Status: Published application
- Kind: A1
- Application number: 17/416,122
- Filed: 2019-11-25
- Published: 2022-02-10
- Earliest claimed: 2018-12-27
- Assignees: Contemporary Amperex Technology Co., Limited
- Applicants: Contemporary Amperex Technology Co., Limited
- Inventors: Rui DU; Yongchao LIU; Deyu ZHAO; Sihui WANG; Chongheng SHEN; Na LIU
- Web page: https://patentgrep.com/patent/US20220045324A1

## CPC

- H01M 4/364: {as mixtures}
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/366: {as layered products}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

This application relates to the field of battery technologies, and in particular, to a pressure-resistant positive active material and an electrochemical energy storage apparatus. The positive active material includes secondary particles composed of primary particles, and a quantity σ of primary particles per unit sphere area in a SEM graph of the secondary particles is 5/μm2 to 30/μm2. A single-particle pressure-resistant strength of the secondary particles is 60 MPa to 300 MPa. A molecular formula of the positive active material is LixNiyCozMkMepOrAm, where 0.95≤x≤1.05, 0≤y≤1, ≤z≤1, 0≤k≤1, 0≤p≤0.1, 1≤r≤2, 0≤m≤2, and m+r≤2. The positive active material in this application has a compact particle structure and a high single-particle pressure-resistant strength.

## Claims

### Claim 1

A positive active material, wherein the positive active material comprises secondary particles composed of primary particles, a quantity σ of primary particles per unit sphere surface area in a SEM profile of the secondary particles is 5/μm2 to 30/μm2, and a single-particle pressure-resistant strength of the secondary particles is 60 MPa to 300 MPa; and
a molecular formula of the positive active material is LixNiyCozMkMepOrAm, wherein 0.95≤x≤1.05, 0≤y≤1, 0≤z≤1, 0≤k≤1, 0≤p≤0.1, 1≤r≤2, 0≤m≤2, and m+r≤2, M is selected from Mn and/or Al, Me is selected from any one or a combination of Zr, Zn, Cu, Cr, Mg, Fe, V, Ti, Sr, Sb, Y, W, and Nb, and A is selected from any one or a combination of N, F, S, and Cl.

### Claim 2 (depends on 1)

The positive active material according to claim 1, wherein in the molecular formula of the positive active material, 0.70≤y≤0.95, 0≤z≤0.2, 0≤k≤0.2, and 0≤p≤0.05.

### Claim 3 (depends on 1)

The positive active material according to claim 1, wherein a powder compacted density of the positive active material is not less than 3.3 g/cm3.

### Claim 4 (depends on 1)

The positive active material according to claim 1, wherein the secondary particles have Dv10 of 2 μm to 8 μm, Dv50 of 5 μm to 18 μm, and Dv90 of 10 μm to 30 μm.

### Claim 5 (depends on 4)

The positive active material according to claim 4, wherein the secondary particles are obtained by stacking the primary particles in an extension direction of the primary particles; the primary particles are rod-shaped, cone-shaped, or needle-shaped; the primary particles are 100 nm to 1000 nm in length; the primary particles is 50 nm to 400 nm in radial cross-sectional width.

### Claim 6 (depends on 1)

The positive active material according to claim 1, wherein the secondary particles have a BET of 0.3 m2/g to 0.8 m2/g.

### Claim 7 (depends on 1)

The positive active material according to claim 1, wherein an inner coating layer is provided on the surface of at least a portion of the primary particles at non-outermost positions of the secondary particles, the inner coating layer comprises a coating element, and the coating element of the inner coating layer is selected from any one or a combination of Al, Ba, Zn, Ti, Co, W, Y, Si, Sn, B, and P.

### Claim 8 (depends on 1)

A positive electrode material, comprising the positive active material according to claim 1, wherein an outer coating layer is provided on the surface of the positive active material, the outer coating layer comprises a coating element, and the coating element of the outer coating layer is selected from any one or a combination of Al, Ba, Zn, Ti, Co, W, Y, Si, Sn, B, and P.

### Claim 9 (depends on 8)

The positive electrode material according to claim 8, wherein the outer coating layer is a continuous and/or discontinuous coating layer.

### Claim 10 (depends on 1)

A method for determining a quantity of primary particles per unit sphere surface area of secondary particles in the positive active material according to claim 1, comprising the steps of:
(1) selecting a positive active material sample whose particle size is an average secondary-particle size Dv50±20%, and conducting SEM-based testing on the sample, to obtain a 10K-times magnified SEM graph;
(2) based on the SEM graph obtained in step (1), calculating the quantity σ of primary particles per unit sphere surface area in the positive active material by using the following formula:
σ=(x1+x2)/2*(y1+y2)/2/(A/C*B/C)
wherein
x1 represents a quantity of primary particles in a horizontal direction on a lower edge of the 10K-times magnified SEM image of the secondary particles;
x2 represents a quantity of primary particles in a horizontal direction on an upper edge of the 10K-times magnified SEM image of the secondary particles;
y1 represents a quantity of primary particles in a longitudinal direction on a left edge of the 10K-times magnified SEM image of the secondary particles;
y2 represents a quantity of primary particles in a longitudinal direction on a right edge of the 10K-times magnified SEM image of the secondary particles;
A represents an actual measured horizontal length of the 10K-times magnified SEM image of the secondary particles, measured in mm;
B represents an actual measured longitudinal length of the 10K-times magnified SEM image of the secondary particles, measured in mm; and
C represents an actual measured length of the 10K-times magnified SEM image of the secondary particles, corresponding to a scale of 1 μm and measured in mm/μm; wherein
during calculation of the quantity of primary particles in the 10K-times magnified SEM image of the secondary particles, a primary particle with presence of a portion is counted as one primary particle.

### Claim 11 (depends on 1)

An electrochemical energy storage apparatus, comprising the positive active material according to claim 1.

### Claim 12 (depends on 4)

The positive active material according to claim 4, wherein the secondary particles are obtained by stacking the primary particles in an extension direction of the primary particles; the primary particles are rod-shaped, cone-shaped, or needle-shaped; and a ratio of a length to a radial cross-sectional width of the primary particles is 2 to 10.

### Claim 13 (depends on 9)

The positive electrode material according to claim 9, wherein the outer coating layer is a composite form of a continuous first coating layer and a discontinuous second coating layer.

### Claim 14 (depends on 9)

The positive electrode material according to claim 9, wherein a substance of the discontinuous coating layer is different from a substance of the continuous coating layer.

### Claim 15 (depends on 8)

A method for determining a quantity of primary particles per unit sphere surface area of secondary particles in the positive electrode material according to claim 8, comprising the steps of:
(1) selecting a positive active material sample whose particle size is an average secondary-particle size Dv50±20%, and conducting SEM-based testing on the sample, to obtain a 10K-times magnified SEM graph;
(2) based on the SEM graph obtained in step (1), calculating the quantity σ of primary particles per unit sphere surface area in the positive active material by using the following formula:
σ=(x1+x2)/2*(y1+y2)/2/(A/C*B/C)
wherein
x1 represents a quantity of primary particles in a horizontal direction on a lower edge of the 10K-times magnified SEM image of the secondary particles;
x2 represents a quantity of primary particles in a horizontal direction on an upper edge of the 10K-times magnified SEM image of the secondary particles;
y 1 represents a quantity of primary particles in a longitudinal direction on a left edge of the 10K-times magnified SEM image of the secondary particles;
y2 represents a quantity of primary particles in a longitudinal direction on a right edge of the 10K-times magnified SEM image of the secondary particles;
A represents an actual measured horizontal length of the 10K-times magnified SEM image of the secondary particles, measured in mm;
B represents an actual measured longitudinal length of the 10K-times magnified SEM image of the secondary particles, measured in mm; and
C represents an actual measured length of the 10K-times magnified SEM image of the secondary particles, corresponding to a scale of 1 μm and measured in mm/μm; wherein
during calculation of the quantity of primary particles in the 10K-times magnified SEM image of the secondary particles, a primary particle with presence of a portion is counted as one primary particle.

### Claim 16 (depends on 8)

An electrochemical energy storage apparatus, comprising the positive electrode material according to claim 8.