# US 2022/0045323 A1 · Positive electrode active material for lithium ion secondary battery, method of manufacturing positive electrode active material for lithium ion secondary battery, and lithium ion secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0045323 A1
- Document ID: US20220045323A1
- Status: Published application
- Kind: A1
- Application number: 17/310,805
- Filed: 2020-02-26
- Published: 2022-02-10
- Earliest claimed: 2019-02-26
- Assignees: Sumitomo Metal Mining Co., Ltd.
- Applicants: Sumitomo Metal Mining Co., Ltd.
- Inventors: Takahiro TOMA; Takahiro OGAWA; Yoshiyuki MATSUURA; Kazuomi RYOSHI
- Web page: https://patentgrep.com/patent/US20220045323A1

## CPC

- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- C01G 53/42: containing alkali metals, e.g. LiNiO2
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/366: {as layered products}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- C01P 2002/54: one element only
- C01P 2004/51: Particles with a specific particle size distribution
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/84: one phase coated with the other
- C01P 2006/11: Powder tap density
- C01P 2006/12: Surface area
- C01P 2006/40: Electric properties
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A positive electrode active material for a lithium ion secondary battery contains a lithium metal composite oxide. The lithium metal composite oxide includes lithium (Li), nickel (Ni), cobalt (Co), and an element M (M) in a mass ratio of Li:Ni:Co:M=1+a:1−x−y:x:y (wherein −0.05≤a≤0.50, 0≤x≤0.35, 0≤y≤0.35, and the element M is at least one element selected from Mg, Ca, Al, Si, Fe, Cr, Mn, V, Mo, W, Nb, Ti, Zr, and Ta), wherein a thickness of a NiO layer is 200 nm or less when a particle of the lithium metal composite oxide during charging at 4.3 V (vs. Li+/Li) is observed by STEM-EDS, and wherein a specific surface area is 0.7 m2/g or more and 2.0 m2/g or less.

## Claims

### Claim 1

A positive electrode active material for a lithium ion secondary battery containing a lithium metal composite oxide, the lithium metal composite oxide comprising:
lithium (Li), nickel (Ni), cobalt (Co), and an element M in a mass ratio of Li:Ni:Co:M=1+a:1−x−y:x:y (wherein −0.05≤a≤0.50, 0≤x≤0.35, 0≤y≤0.35, and the element M is at least one element selected from Mg, Ca, Al, Si, Fe, Cr, Mn, V, Mo, W, Nb, Ti, Zr, and Ta),
wherein a thickness of a NiO layer is 200 nm or less when a particle of the lithium metal composite oxide during charging at 4.3 V (vs. Li+/Li) is observed by Scanning Transmission Electron Microscope-Electron Dispersive X-Ray Spectrometer, and
wherein a specific surface area of the positive electrode active material for a lithium ion secondary battery is 0.7 m2/g or more and 2.0 m2/g or less.

### Claim 2 (depends on 1)

The positive electrode active material for a lithium ion secondary battery according to claim 1, wherein a mean volume particle diameter (MV) is 5 μm or more and 20 μm or less in a particle size distribution by a laser diffraction scattering method.

### Claim 3 (depends on 1)

The positive electrode active material for a lithium ion secondary battery according to claim 1, wherein the element M is either uniformly distributed inside secondary particles of the lithium metal composite oxide or uniformly coated on surfaces of the secondary particles, or both.

### Claim 4

A method of manufacturing a positive electrode active material for a lithium ion secondary battery, comprising:
a drying step of heating a metal composite hydroxide at 105° C. or higher and 120° C. or lower to obtain a dried metal composite hydroxide;
a mixing step of mixing the dried metal composite hydroxide with a lithium compound to form a lithium mixture; and
a firing step of firing the lithium mixture formed in the mixing step at a temperature of 650° C. or higher and 900° C. or lower in an oxidizing atmosphere;
wherein the metal composite hydroxide contains nickel (Ni), cobalt (Co), and an element M in a mass ratio of Ni:Co:M=1−x−y:x:y (wherein 0≤x≤0.35, 0≤y≤0.35, and the element M is at least one element selected from Mg, Ca, Al, Si, Fe, Cr, Mn, V, Mo, W, Nb, Ti, Zr, and Ta), and
wherein a specific surface area of a positive electrode active material for the lithium ion secondary battery obtained after the firing step is 0.7 m2/g or more and 2.0 m2/g or less.

### Claim 5 (depends on 1)

A lithium ion secondary battery having a positive electrode containing the positive electrode active material for the lithium ion secondary battery of claim 1.

### Claim 6 (depends on 2)

A lithium ion secondary battery having a positive electrode containing the positive electrode active material for the lithium ion secondary battery of claim 2.

### Claim 7 (depends on 3)

A lithium ion secondary battery having a positive electrode containing the positive electrode active material for the lithium ion secondary battery of claim 3.