# US 2022/0045317 A1 · Cathode active material, method for preparing same, and lithium secondary battery comprising same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0045317 A1
- Document ID: US20220045317A1
- Status: Published application
- Kind: A1
- Application number: 17/275,883
- Filed: 2019-09-16
- Published: 2022-02-10
- Earliest claimed: 2018-09-12
- Assignees: Posco; Research Institute of Industrial Science & Technology; Posco Chemical Co., Ltd
- Applicants: Posco; Research Institute of Industrial Science & Technology; Posco Chemical Co., Ltd.
- Inventors: Kwon Young Choi; Sang Hyuk Lee; Jong Il Park; Jung Hoon Song; Sang Cheol Nam
- Web page: https://patentgrep.com/patent/US20220045317A1

## CPC

- C01G 53/84: Hydroxides
- C01G 53/42: containing alkali metals, e.g. LiNiO2
- H01M 4/366: {as layered products}
- H01M 4/483: {for non-aqueous cells (H01M4/485 takes precedence)}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/52: containing elements as dopants
- C01P 2004/03: obtained by SEM
- C01P 2004/04: obtained by TEM, STEM, STM or AFM
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/84: one phase coated with the other
- C01P 2006/40: Electric properties
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A positive active material, a manufacturing method thereof, and a lithium secondary battery including the same are disclosed, and a positive active material including lithium metal oxide particles in a secondary particle form including primary particles, wherein the secondary particle surface includes planar primary particles with a narrow angle of 70 to 90° from among angles between a c axis of the primary particles and a straight line connecting a virtual point of a center of the primary particle and a center point of the secondary particle may be provided.

## Claims

### Claim 1

A positive active material including lithium metal oxide particles in a secondary particle form including primary particles,
wherein the secondary particle surface includes planar primary particles with a narrow angle of 60 to 90° from among angles between a c axis of the primary particles and a straight line connecting a virtual point of a center of the primary particle and a center point of the secondary particle.

### Claim 2 (depends on 1)

The positive active material of claim 1, wherein
with respect to the area of 100 area % formed by a circle of 50% reference of a radius of the secondary particles at the center point of the secondary particle,
an area occupied by the planar primary particles is equal to or greater than 20 area %.

### Claim 3 (depends on 2)

The positive active material of claim 2, wherein
with respect to the area 100 area % formed by a circle of 50% reference of a radius of the secondary particles at the center point of the secondary particle,
an average length of the planar primary particles existing in the area is 750 nm to 1.25 μm.

### Claim 4 (depends on 1)

The positive active material of claim 1, wherein
an inside of the secondary particle includes acicular primary particles with a narrow angle of equal to or greater than 0° and less than 70° from among angles between a c axis of the primary particles and a straight line connecting a virtual point of a center of the primary particle and a center point of the secondary particle.

### Claim 5 (depends on 1)

The positive active material of claim 1, wherein
a content of nickel from among metals in the secondary particle is equal to or greater than 80 mol %.

### Claim 6

A method for manufacturing a positive active material, comprising:
obtaining a metal precursor by inputting a metallic salt aqueous solution into a co-precipitation reactor; and
obtaining a positive active material by mixing the metal precursor and a raw lithium material and baking the same,
wherein, in the obtaining of a metal precursor by inputting a metallic salt aqueous solution into a co-precipitation reactor,
a pH condition is changes within a range of a reaction end time of 1 to 30 time % with respect to an entire reaction time of 100 time %.

### Claim 7 (depends on 6)

The method of claim 6, wherein
a difference between a reaction start pH and a reaction end pH in the obtaining of a metal precursor by inputting a metallic salt aqueous solution into a co-precipitation reactor is 0.1 to 0.8.

### Claim 8 (depends on 6)

The method of claim 6, wherein
the pH condition rises by 0.1 to 0.8 within a range of the reaction end time of 1 to 30 time % for the entire reaction time of 100 time %.

### Claim 9 (depends on 8)

The method of claim 8, wherein
the rising speed of the pH condition is 0.0016 to 0.0133 pH/min.

### Claim 10 (depends on 1)

A lithium secondary battery comprising:
a positive electrode including a positive active material according to claim 1;
a negative electrode including a negative active material; and
an electrolyte positioned between the positive electrode and the negative electrode.