# US 2022/0045308 A1 · Fabrication method of positive electrode for secondary battery and secondary battery including the positive electrode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0045308 A1
- Document ID: US20220045308A1
- Status: Published application
- Kind: A1
- Application number: 17/395,141
- Filed: 2021-08-05
- Published: 2022-02-10
- Earliest claimed: 2020-08-05
- Assignees: SK Innovation Co., Ltd.
- Applicants: SK Innovation Co., Ltd.
- Inventors: Byoung Wook JO; Byung Chan KANG; Yong Hee KANG; Sung Jun PARK; Hyo Sung LIM
- Web page: https://patentgrep.com/patent/US20220045308A1

## CPC

- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/622: {being polymers}
- H01M 10/04: Construction or manufacture in general (H01M10/058, H01M10/12, H01M10/28, H01M10/38 take precedence)
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention provides a fabrication method of a positive electrode for a secondary battery, including: (a) heating a slurry composition for a positive electrode containing a positive electrode active material, a binder, and a solvent to a temperature lower than a boiling point (17:0) of the solvent; (b) applying the heated slurry composition for a positive electrode onto current collector; and (c) cooling the applied slurry composition for a positive electrode.

## Claims

### Claim 1

A fabrication method of a positive electrode for a secondary battery, comprising:
(a) heating a slurry composition for a positive electrode containing a positive electrode active material, a binder, and a solvent to a temperature lower than a boiling point (Tb) of the solvent;
(b) applying the heated slurry composition for a positive electrode onto a current collector; and
(c) cooling the applied slurry composition for a positive electrode.

### Claim 2 (depends on 1)

The fabrication method of a positive electrode for a secondary battery of claim 1, wherein a solid in the slurry composition for a positive electrode is contained in an amount of more than 74 parts by weight and 90 parts by weight or less based on 100 parts by weight of the slurry composition for a positive electrode.

### Claim 3 (depends on 1)

The fabrication method of a positive electrode for a secondary battery of claim 1, wherein a viscosity (A1) of the slurry composition for a positive electrode before being heated is 13,000 to 80,000 cP.

### Claim 4 (depends on 1)

The fabrication method of a positive electrode for a secondary battery of claim 1, wherein a temperature (T) of the heating of the slurry composition for a positive electrode satisfies the following Relational Equation 1:
0.3Tb<T<0.9Tb [Relational Equation 1]
wherein Tb is the boiling point of the solvent.

### Claim 5 (depends on 1)

The fabrication method of a positive electrode for a secondary battery of claim 1, wherein the cooling is performed at a temperature of 10 to 30° C. for 1 to 60 seconds.

### Claim 5 (depends on 7)

The fabrication. method of a positive electrode for a secondary battery of claim 7, wherein the drying is performed at a temperature of 110° C. or more and less than 145° C. for 20 to 150 seconds.

### Claim 6 (depends on 1)

The fabrication method of a positive electrode for a secondary battery of claim 1, wherein the slurry composition a positive electrode satisfies the following Relational Equations 2 and 3:
1.3≤A1/A2≤12 [Relational Equation 2]
1.1≤A3/A2≤10 [Relational Equation 3]
wherein A1 is a viscosity of the slurry composition for a positive electrode before being heated. A2 is a viscosity of the heated slurry composition for a positive electrode, and A3 is a viscosity of the cooled slurry composition for a positive electrode.

### Claim 7 (depends on 1)

The fabrication method of a positive electrode for a secondary battery of claim 1, further comprising (d) drying the cooled slurry composition for a positive electrode.

### Claim 9

A positive electrode for a secondary battery, fabricated by a fabrication method of a positive electrode for a secondary battery including: (a) heating a slurry composition for a positive electrode containing a positive electrode active material, a binder, and a solvent to a temperature lower than a boiling point (Tb) of the solvent;
(b) applying the heated slurry composition for a positive electrode onto a current collector; and (c) cooling the applied slurry composition. for a positive electrode, the positive electrode comprising:
the current collector; and
a positive electrode active material layer formed on the current collector and containing a positive electrode active material, a conductive material, and a binder.

### Claim 10 (depends on 9)

The positive electrode for a secondary battery of claim 9, wherein an adhesive force of the positive electrode active material layer to the current collector is 0.35 N/cm or more.

### Claim 11 (depends on 9)

The positive electrode for a secondary battery of claim 9, wherein in the positive electrode, a difference between a maximum loading value and a minimum loading value of the positive electrode active material layer at five or more positions having regular intervals in a length direction is 10% or less of a total loading average value.

### Claim 12

A secondary battery comprising:
a positive electrode;
a negative electrode;
a separator positioned between. the positive electrode and the negative electrode; and
an electrolyte,
wherein the positive electrode is fabricated by a fabrication method of a positive electrode for a secondary battery including: (a) heating a slurry composition for a positive electrode containing a positive electrode active material, a binder, and a solvent to a temperature lower than a boiling point (Tb) of the solvent; (b) applying the heated slurry composition for a positive electrode onto a current collector; and (c) cooling the applied slurry composition for a positive electrode, and
the positive electrode includes:
the current collector; and
a positive electrode active material layer formed on the current collector and containing a positive electrode active material, a conductive material, and a binder.