# US 2022/0045266 A1 · Mram structure and method of fabricating the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0045266 A1
- Document ID: US20220045266A1
- Status: Published application
- Kind: A1
- Application number: 17/006,923
- Filed: 2020-08-31
- Published: 2022-02-10
- Earliest claimed: 2020-08-05
- Assignees: United Microelectronics Corp.
- Applicants: United Microelectronics Corp.
- Inventors: Da-Jun Lin; Min-Hua Tsai; Tai-Cheng Hou; Fu-Yu Tsai; Bin-Siang Tsai
- Web page: https://patentgrep.com/patent/US20220045266A1

## CPC

- H10N 50/80: Constructional details
- H10B 61/00: Magnetic memory devices, e.g. magnetoresistive RAM [MRAM] devices
- H10N 50/01: Manufacture or treatment
- H10N 50/10: Magnetoresistive devices
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

An MRAM structure includes a dielectric layer. A first MRAM, a second MRAM and a third MRAM are disposed on the dielectric layer, wherein the second MRAM is disposed between the first MRAM and the third MRAM, and the second MRAM includes an MTJ. Two gaps are respectively disposed between the first MRAM and the second MRAM and between the second MRAM and the third MRAM. Two tensile stress pieces are respectively disposed in each of the two gaps. A first compressive stress layer surrounds and contacts the sidewall of the MTJ entirely. A second compressive stress layer covers the openings of each of the gaps and contacts the two tensile material pieces.

## Claims

### Claim 1

A magnetic random access memory (MRAM) structure, comprising:
a dielectric layer;
a first MRAM, a second MRAM and a third MRAM disposed on the dielectric layer, wherein the second MRAM is disposed between the first MRAM and the third MRAM, and the second MRAM comprises a magnetic tunneling junction (MTJ);
two gaps respectively disposed between the first MRAM and the second MRAM and between the second MRAM and the third MRAM;
two tensile stress pieces respectively disposed in each of the two gaps;
a first compressive stress layer surrounding and contacting the sidewall of the MTJ entirely; and
a second compressive stress layer covering the openings of each of the gaps and contacting the two tensile material pieces.

### Claim 2 (depends on 1)

The MRAM structure of claim 1, wherein an absolute value of a tensile stress in each of the two tensile stress pieces is the same as an absolute value of a tensile stress in the first compressive stress layer or a difference between the absolute value of the tensile stress in each of the two tensile stress pieces and the absolute value of the tensile stress in the first compressive stress layer is smaller than a predetermined ratio.

### Claim 3 (depends on 1)

The MRAM structure of claim 1, wherein the first compressive stress layer covers a sidewall of the first MRAM entirely, a sidewall of the second MRAM entirely and a sidewall of the third MRAM entirely.

### Claim 4 (depends on 1)

The MRAM structure of claim 1, wherein the first compressive stress layer covers a top surface of the first MRAM, a top surface of the second MRAM and a top surface of a third MRAM.

### Claim 5 (depends on 1)

The MRAM structure of claim 1, wherein there is no compressive stress in a sidewall of the MTJ.

### Claim 6 (depends on 1)

The MRAM structure of claim 1, wherein the two tensile stress pieces comprise silicon oxide, the first compressive stress layer comprises silicon nitride, and the second compressive stress layer comprises silicon nitride.

### Claim 7 (depends on 1)

The MRAM structure of claim 1, wherein the first compressive stress layer covers a bottom of each of the two tensile material pieces.

### Claim 8 (depends on 1)

The MRAM structure of claim 1, wherein a thickness of the second compressive stress layer is not greater than a thickness of the first compressive stress layer.

### Claim 9 (depends on 1)

The MRAM structure of claim 1, wherein a thickness of the first compressive stress layer is not smaller than 50 angstroms.

### Claim 10

A method of fabricating a magnetic random access memory (MRAM) structure, comprising:
providing a dielectric layer, wherein a first MRAM, a second MRAM and a third MRAM are disposed on the dielectric layer, the second MRAM are disposed between the first MRAM and the third MRAM, two gaps are respectively disposed between the first MRAM and the second MRAM and between the second MRAM and the third MRAM and the second MRAM comprises a magnetic tunneling junction (MTJ);
forming a first compressive stress layer covering the first MRAM, the second MRAM, the third MRAM and the dielectric layer;
forming a tensile stress material layer covering the first compressive stress layer and filling in the two gaps;
removing the tensile stress material layer outside of the two gaps to form two tensile stress pieces in each of the two gaps; and
forming a second compressive stress layer covering an opening of each of the two gaps and contacting the two tensile stress pieces.

### Claim 11 (depends on 10)

The method of fabricating the MRAM structure of claim 10, further comprising before forming the tensile stress material layer, etching back the first compressive stress layer.

### Claim 12 (depends on 11)

The method of fabricating the MRAM structure of claim 11, wherein during the steps of etching back the first compressive stress layer, the first compressive stress layer on a top surface of the first MRAM, on a top surface of the second MRAM and on a top surface of the third MRAM is removed.

### Claim 13 (depends on 12)

The method of fabricating the MRAM structure of claim 12, wherein the first compressive stress layer is etched back to remove the first compressive stress layer on a bottom of each of the two gaps.

### Claim 14 (depends on 10)

The method of fabricating the MRAM structure of claim 10, wherein an absolute value of a tensile stress in each of the two tensile stress pieces is the same as an absolute value of a tensile stress in the first compressive stress layer or a difference between the absolute value of the tensile stress in each of the two tensile stress pieces and the absolute value of the tensile stress in the first compressive stress layer is smaller than a predetermined ratio.

### Claim 15 (depends on 10)

The method of fabricating the MRAM structure of claim 10, wherein after forming the two tensile stress pieces, there is no compressive stress in a sidewall of the MTJ.

### Claim 16 (depends on 10)

The method of fabricating the MRAM structure of claim 10, wherein a thickness of the second compressive stress layer is not greater than a thickness of the first compressive stress layer.

### Claim 17 (depends on 10)

The method of fabricating the MRAM structure of claim 10, wherein a thickness of the first compressive stress layer is not smaller than 50 angstroms.

### Claim 18

A magnetic random access memory (MRAM) structure, comprising:
a dielectric layer;
a plurality of MRAMs disposed on the dielectric layer and the plurality of MRAMs arranged in one row, wherein the plurality of MRAMs comprise an end MRAM disposed at an end of the row;
a dummy MRAM disposed on the dielectric layer and at one side of the end MRAM;
a gap disposed between the end MRAM and the dummy MRAM;
a first compressive stress layer contacting a sidewall of the gap;
a tensile stress piece disposed within the gap;
a second compressive stress layer covering an opening of the gap and contacting the tensile stress piece; and
a plurality of metal interconnections respectively contacting each of the plurality of MRAMs.

### Claim 19 (depends on 18)

The MRAM structure of claim 18, wherein each of the plurality of the metal interconnections comprises a first metal interconnection and a second metal interconnection respectively electrically connecting to a top electrode and a bottom electrode of each of the plurality of MRAMs, and the dummy MRAM only electrically connects to one of the first metal interconnection and the second metal interconnection.

### Claim 20 (depends on 18)

The MRAM structure of claim 18, wherein the tensile tress piece comprises silicon oxide, the first compressive stress layer comprises silicon nitride, and the second compressive stress layer comprises silicon nitride.