# US 2022/0045105 A1 · Display device including polycrystalline silicon layer, method of manufacturing polycrystalline silicon layer, and method of manufacturing display device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0045105 A1
- Document ID: US20220045105A1
- Status: Published application
- Kind: A1
- Application number: 17/510,995
- Filed: 2021-10-26
- Published: 2022-02-10
- Earliest claimed: 2019-03-19
- Assignees: Samsung Display Co., Ltd.
- Applicants: Samsung Display Co., LTD.
- Inventors: Dong-Sung LEE; Jongoh SEO; Byung Soo SO; Dong-min LEE; Yeon Hee JEON; Jonghoon CHOI
- Web page: https://patentgrep.com/patent/US20220045105A1

## CPC

- H10D 86/60: wherein the TFTs are in active matrices
- H10P 14/36: {characterised by treatments done before the formation of the materials}
- H10D 30/0314: {of lateral top-gate TFTs comprising only a single gate}
- H10D 30/0321: {comprising silicon, e.g. amorphous silicon or polysilicon}
- H10D 30/6731: {Top-gate only TFTs}
- H10D 30/6745: {Polycrystalline or microcrystalline silicon}
- H10D 62/405: {Orientations of crystalline planes}
- H10D 86/0223: {comprising crystallisation of amorphous, microcrystalline or polycrystalline semiconductor materials}
- H10D 86/421: {having a particular composition, shape or crystalline structure of the active layer}
- H10P 14/2922: {being non-crystalline insulating materials, e.g. glass or polymers}
- H10P 14/3238: {being insulating materials}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3454: {Amorphous}
- H10P 14/3456: {Polycrystalline}
- H10P 14/3808: {using laser beams}
- H10P 14/3816: {Pulsed laser beam}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A display device may include a thin film transistor disposed on a substrate, and a display element electrically connected to the thin film transistor. The thin film transistor may include an active pattern including polycrystalline silicon, a gate insulation layer disposed on the active pattern, and a gate electrode disposed on the gate insulation layer. An average value of grain sizes of the active pattern may be in a range of about 400 nm to about 800 nm. An RMS value of a surface roughness of the active pattern may be about 4 nm or less. A method of manufacturing a polycrystalline silicon layer may include cleaning an amorphous silicon layer with hydrofluoric acid, rinsing the amorphous silicon layer with hydrogenated deionized water, and irradiating the amorphous silicon layer with a laser beam having an energy density of about 440 mJ/cm2 to about 490 mJ/cm2.

## Claims

### Claim 1

A method of manufacturing a polycrystalline silicon layer, comprising:
forming an amorphous silicon layer on a substrate;
cleaning the amorphous silicon layer with hydrofluoric acid;
rinsing the amorphous silicon layer with hydrogenated deionized water; and
irradiating the amorphous silicon layer with a laser beam having an energy density in a range of about 440 mJ/cm2 to about 490 mJ/cm2 to form the polycrystalline silicon layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein a thickness of the amorphous silicon layer is in a range of about 370 Å to about 500 Å.

### Claim 3 (depends on 1)

The method of claim 1, wherein the hydrofluoric acid includes a hydrogen fluoride in an amount of about 0.5%.

### Claim 4 (depends on 1)

The method of claim 1 wherein the cleaning the amorphous silicon layer is performed for a time period of about 60 seconds to about 120 seconds.

### Claim 5 (depends on 1)

The method of claim 1, wherein a hydrogen concentration of the hydrogenated deionized water is about 1.0 ppm.

### Claim 6 (depends on 1)

The method of claim 1, wherein a wavelength of the laser beam is about 308 nm.

### Claim 7 (depends on 1)

The method of claim 1, wherein a scan pitch of the laser beam is about 10 μm or less.

### Claim 8 (depends on 1)

The method of claim 1, wherein the forming the polycrystalline silicon layer includes forming grains in the polycrystalline silicon layer, an average size of the grains of the polycrystalline silicon layer is in a range of about 400 nm to about 800 nm.

### Claim 9 (depends on 1)

The method of claim 1, wherein the forming the polycrystalline silicon layer includes forming a rough surface of the polycrystalline silicon layer, a root-mean-square value of a roughness of the rough surface of the polycrystalline silicon layer is about 4 nm or less.

### Claim 10

A method of manufacturing a display device, comprising:
forming an amorphous silicon layer on a substrate;
cleaning the amorphous silicon layer with hydrofluoric acid;
rinsing the amorphous silicon layer with hydrogenated deionized water;
irradiating the amorphous silicon layer with a laser beam having an energy density in a range of about 440 mJ/cm2 to about 490 mJ/cm2 to form a polycrystalline silicon layer;
etching the polycrystalline silicon layer to form a polycrystalline silicon pattern;
forming an insulation layer on the polycrystalline silicon pattern;
forming a gate electrode on the insulation layer;
injecting an ion at a portion of the polycrystalline silicon pattern to form an active pattern; and
forming a display element on the gate electrode.

### Claim 11 (depends on 10)

The method of claim 10, wherein a scan pitch of the laser beam is about 10 μm or less.

### Claim 12 (depends on 10)

The method of claim 10, wherein the forming the display element comprises:
forming a first electrode on the gate electrode, the first electrode being electrically connected to the active pattern;
forming an emission layer on the first electrode; and
forming a second electrode on the emission layer.