# US 2022/0045066 A1 · Semiconductor structure and method of manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0045066 A1
- Document ID: US20220045066A1
- Status: Published application
- Kind: A1
- Application number: 17/411,103
- Filed: 2021-08-25
- Published: 2022-02-10
- Earliest claimed: 2020-08-05
- Assignees: Changxin Memory Technologies, Inc.
- Applicants: Changxin Memory Technologies, Inc.
- Inventors: Jingwen LU; Hai-Han Hung
- Web page: https://patentgrep.com/patent/US20220045066A1

## CPC

- H10B 12/0335: {Making a connection between the transistor and the capacitor, e.g. plug}
- H10B 12/312: {with a bit line higher than the capacitor}
- H10B 12/482: {Bit lines}
- H10D 62/115: {Dielectric isolations, e.g. air gaps}
- H10B: ELECTRONIC MEMORY DEVICES
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A semiconductor structure and a method of manufacturing the same are provided. The semiconductor structure includes a substrate, bit line structures and isolation walls located on side walls of the bit line structures, and capacitor contact holes. In the substrate, conductive contact regions are arranged. The conductive contact regions are exposed from the substrate. A plurality of discrete bit line structures are located on the substrate. Each of the isolation walls includes at least one isolation layer and a gap between the isolation layer and the bit line structure. Each of the capacitor contact holes is constituted by a region surrounded by the isolation walls between the adjacent bit line structures. The capacitor contact holes expose the conductive contact regions. A top width of the capacitor contact holes is larger than a bottom width thereof in a direction parallel to an arrangement direction of the bit line structures.

## Claims

### Claim 1

A semiconductor structure, comprising:
a substrate, in which conductive contact regions are arranged, wherein the conductive contact regions are exposed from the substrate;
bit line structures and isolation walls located on side walls of the bit line structures, wherein a plurality of discrete bit line structures are located on the substrate, and each of the isolation walls comprises at least one isolation layer and a gap between the isolation layer and the bit line structure; and
capacitor contact holes, each of which is constituted by a region surrounded by the isolation walls between the adjacent bit line structures, wherein the capacitor contact holes expose the conductive contact regions, and a top width of the capacitor contact holes is larger than a bottom width thereof in a direction parallel to an arrangement direction of the bit line structures.

### Claim 2 (depends on 1)

The semiconductor structure of claim 1, wherein at least one of the isolation layers has doping ions, a hardness of the isolation layer with the doping ions is larger than that of the isolation layer without the doping ions, or a dielectric constant of the isolation layer with the doping ions is smaller than that of the isolation layer without the doping ions.

### Claim 3 (depends on 2)

The semiconductor structure of claim 2, wherein the isolation layer comprises a silicon nitride layer and the doping ions comprise oxygen ions; or, the isolation layer comprises a silicon oxide layer and the doping ions comprise nitrogen ions.

### Claim 4 (depends on 2)

The semiconductor structure of claim 2, wherein the isolation wall comprises two isolation layers and the gap between the two isolation layers, the isolation layer away from the bit line structure has the doping ions, and a thickness of the isolation layer away from the bit line structure is smaller than that of the isolation layer close to the bit line structure in the direction parallel to the arrangement direction of the bit line structures.

### Claim 5 (depends on 1)

The semiconductor structure of claim 1, wherein the isolation wall comprises a first isolation layer, the gap, and a second isolation layer arranged in sequence, a material of the first isolation layer comprises at least one of silicon nitride or silicon oxynitride, and a material of the second isolation layer comprises at least one of silicon nitride or silicon oxynitride.

### Claim 6 (depends on 1)

The semiconductor structure of claim 1, further comprising: a sealing layer, which is connected to the bit line structure and the isolation layer, and is configured to seal a top of the gap, wherein a top surface height of the isolation layer connected to the sealing layer is lower than that of the bit line structure in a direction perpendicular to a surface of the substrate.

### Claim 7 (depends on 1)

The semiconductor structure of claim 1, wherein the bit line structure has a chamfer on a top thereof, and the chamfer is 5°-35°.

### Claim 8

A method of manufacturing a semiconductor structure, comprising:
providing a substrate in which conductive contact regions are arranged, wherein the conductive contact regions are exposed from the substrate;
forming a plurality of discrete bit line structures on the substrate, wherein a top width of the bit line structures is smaller than a bottom width thereof in a direction parallel to an arrangement direction of the bit line structures;
forming a sacrificial layer on a side wall of each of the bit line structures, and an isolation layer on a side, away from the bit line structure, of the sacrificial layer; and
removing the sacrificial layer to form an isolation wall, wherein the isolation wall comprises the isolation layer and a gap between the isolation layer and the bit line structure, and a capacitor contact hole is constituted by a region surrounded by the isolation walls between the adjacent bit line structures.

### Claim 9 (depends on 8)

The method of manufacturing the semiconductor structure of claim 8, wherein the forming the bit line structure comprises:
forming a plurality of discrete initial bit line structures, wherein a top width of the initial bit line structures is larger than or equal to a bottom width thereof in a direction parallel to the initial bit line structures; and
performing a dry etching process with an etching angle on the initial bit line structure to form the bit line structure with a chamfer on a top thereof, wherein the chamfer is the same as the etching angle and is 5°-35°.

### Claim 10 (depends on 8)

The method of manufacturing the semiconductor structure of claim 8, wherein the forming the sacrificial layer and the isolation layer comprises:
forming a sacrificial film on the side wall of each of the bit line structures, wherein the sacrificial film comprises a first isolation portion close to the bit line structure and a second isolation portion away from the bit line structure; and
doping the second isolation portion with doping ions to form the sacrificial layer located at the first isolation portion and the isolation layer located at the second isolation portion, wherein a hardness of the isolation layer is larger than that of the sacrificial layer.

### Claim 11 (depends on 10)

The method of manufacturing the semiconductor structure of claim 10, wherein a material of the sacrificial film comprises silicon oxide and the doping ions comprise nitrogen ions.

### Claim 12 (depends on 10)

The method of manufacturing the semiconductor structure of claim 10, wherein forming the isolation wall comprises:
forming a silicon nitride layer on the side wall of each of the bit line structures, wherein the silicon nitride layer comprises a first isolation portion close to the bit line structure and a second isolation portion away from the bit line structure;
doping the second isolation portion of the silicon nitride layer with oxygen ions;
forming a silicon oxide layer on a side wall of the silicon nitride layer away from the bit line structure, wherein the silicon oxide layer comprises the first isolation portion close to the bit line structure and the second isolation portion away from the bit line structure;
doping the second isolation portion of the silicon oxide layer with nitrogen ions; and
removing the first isolation portion of the silicon oxide layer to form the gap.

### Claim 13 (depends on 12)

The method of manufacturing the semiconductor structure of claim 12, wherein a temperature of the oxygen ions during doping the oxygen ions is 800° C.-1000° C., and a temperature of the nitrogen ions during doping the nitrogen ions is 600° C.-800° C.

### Claim 14 (depends on 8)

The method of manufacturing the semiconductor structure of claim 8, wherein before the sacrificial layer is etched, the capacitor contact hole is filled to form a support structure which is in contact with a side wall of the isolation layer away from the bit line structure, and the support structure is removed after the sacrificial layer is etched.

### Claim 15 (depends on 8)

The method of manufacturing the semiconductor structure of claim 8, wherein a sealing layer for sealing a top opening of the gap is formed by a deposition process, after the gap is formed.