# US 2022/0044927 A1 · Deposition of low-stress boron-containing layers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0044927 A1
- Document ID: US20220044927A1
- Status: Published application
- Kind: A1
- Application number: 16/987,704
- Filed: 2020-08-07
- Published: 2022-02-10
- Earliest claimed: 2020-08-07
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Huiyuan Wang; Rick Kustra; Bo Qi; Abhijit Basu Mallick; Kaushik Alayavalli; Jay D. Pinson
- Web page: https://patentgrep.com/patent/US20220044927A1

## CPC

- H10P 14/668: {the materials being characterised by the deposition precursor materials}
- C23C 16/32: Carbides
- C23C 16/342: {Boron nitride}
- C23C 16/345: {Silicon nitride}
- C23C 16/36: Carbonitrides
- C23C 16/401: {containing silicon}
- C23C 16/4586: {Elements in the interior of the support, e.g. electrodes, heating or cooling devices}
- C23C 16/46: characterised by the method used for heating the substrate (C23C16/48, C23C16/50 take precedence)
- C23C 16/463: {Cooling of the substrate}
- C23C 16/50: using electric discharges {(generation and control of plasma in discharge tubes for surface treatment H01J37/32, H01J37/34)}
- C23C 16/5096: {Flat-bed apparatus}
- C23C 16/52: Controlling or regulating the coating process {(C23C16/45557, C23C16/279 take precedence)}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/3416: {Nitrides}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 72/0402: {Apparatus for fluid treatment (H10P72/0441, H10P72/0448 take precedence)}
- H10P 72/0421: {for drying etching}
- H10P 72/0432: {mainly by conduction}
- H10P 72/0454: {surrounding a central transfer chamber}
- H10P 72/0471: {comprising at least one ion or electron beam chamber}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3444: {P-type}
- H10P 14/6681: {the precursor containing a compound comprising Si}
- H10P 14/68: Organic materials, e.g. photoresists
- H10P 14/6923: {the material being boron or phosphorus doped silicon oxides, e.g. BPSG, BSG or PSG}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Examples of the present technology include semiconductor processing methods to form boron-containing materials on substrates. Exemplary processing methods may include delivering a deposition precursor that includes a boron-containing precursor to a processing region of a semiconductor processing chamber. A plasma may be formed from the deposition precursor within the processing region of the semiconductor processing chamber. The methods may further include depositing a boron-containing material on a substrate disposed within the processing region of the semiconductor processing chamber, where the substrate is characterized by a temperature of less than or about 50° C. The as-deposited boron-containing material may be characterized by a surface roughness of less than or about 2 nm, and a stress level of less-than or about −500 MPa. In some embodiments, a layer of the boron-containing material may function as a hardmask.

## Claims

### Claim 1

A semiconductor processing method comprising:
delivering a deposition precursor comprising a boron-containing precursor to a processing region of a semiconductor processing chamber;
forming a plasma of the deposition precursor within the processing region of the semiconductor processing chamber; and
depositing a boron-containing material on a substrate disposed within the processing region of the semiconductor processing chamber, wherein the substrate is characterized by a temperature of less than or about 50° C.

### Claim 2 (depends on 1)

The semiconductor processing method of claim 1, wherein the method further comprises delivering an inert precursor to the processing region of the semiconductor processing chamber, wherein a flow rate ratio of the inert precursor to the deposition precursor is greater than about 10:1.

### Claim 3 (depends on 2)

The semiconductor processing method of claim 2, wherein the inert precursor comprises at least one of helium or argon.

### Claim 4 (depends on 1)

The semiconductor processing method of claim 1, wherein the semiconductor processing chamber is characterized by a pressure of less than or about 100 mTorr.

### Claim 5 (depends on 1)

The semiconductor processing method of claim 1, wherein the deposition precursor further comprises a boron-containing precursor.

### Claim 6 (depends on 1)

The semiconductor processing method of claim 1, wherein the deposition precursor further comprises at least one of a silicon-containing precursor or a nitrogen-containing precursor.

### Claim 7 (depends on 1)

The semiconductor processing method of claim 1, wherein the boron-containing material comprises at least one of boron carbide, boron-nitride, boron-carbon-nitride, boron-containing silicon, boron-containing silicon oxide, boron-and-boron-containing silicon oxide, or boron-containing silicon nitride.

### Claim 8 (depends on 1)

The semiconductor processing method of claim 1, wherein the plasma is a bias plasma formed at a bias power is greater than 2000 Watts.

### Claim 9

A semiconductor processing method comprising:
delivering a deposition precursor comprising a boron-containing precursor to a processing region of a semiconductor processing chamber;
applying a bias power to a substrate disposed within the processing region of the semiconductor processing chamber, wherein the bias power is greater than or about 3000 Watts;
forming a plasma of the deposition precursor within the processing region of the semiconductor processing chamber; and
depositing a boron-containing material on the substrate.

### Claim 10 (depends on 9)

The semiconductor processing method of claim 9, wherein the substrate is characterized by a temperature of less than or about 50° C.

### Claim 11 (depends on 9)

The semiconductor processing method of claim 9, wherein the deposition precursor further comprises an inert precursor.

### Claim 12 (depends on 11)

The semiconductor processing method of claim 11, wherein a flow rate ratio of the inert precursor to the boron-containing precursor is greater than or about 10:1.

### Claim 13 (depends on 9)

The semiconductor processing method of claim 9, wherein the bias power is greater than or about 4000 Watts.

### Claim 14

A semiconductor processing method comprising:
delivering a boron-containing precursor to a processing region of a semiconductor processing chamber;
forming a plasma of the boron-containing precursor within the processing region of the semiconductor processing chamber; and
depositing a boron-containing material on a substrate disposed within the processing region of the semiconductor processing chamber, wherein the boron-containing material is characterized by an as-deposited surface roughness of less than or about 2 nm.

### Claim 15 (depends on 14)

The semiconductor processing method of claim 14, wherein the substrate is characterized by a temperature of less than or about 50° C.

### Claim 16 (depends on 14)

The semiconductor processing method of claim 14, wherein the processing method further comprises:
delivering an inert precursor to the processing region of the semiconductor processing chamber, wherein a flow rate ratio of the inert precursor to the boron-containing precursor is greater than about 10:1; and
applying a bias power to the substrate during the deposition of the boron-containing material, wherein the bias power is greater than or about 3000 Watts.

### Claim 17 (depends on 14)

The semiconductor processing method of claim 14, wherein the boron-containing material is characterized by an as-deposited stress that is less than or about −500 MPa.

### Claim 18 (depends on 14)

The semiconductor processing method of claim 14, wherein the boron-containing material further comprises carbon atoms, and wherein greater than or about 60% of the carbon atoms have sp3 hybridized bonds.

### Claim 19 (depends on 14)

The semiconductor processing method of claim 14, wherein the boron-containing material comprises less than or about 25 mol % hydrogen.

### Claim 20 (depends on 14)

The semiconductor processing method of claim 14, wherein the boron-containing material comprises at least one of boron carbide, boron-nitride, boron-carbon-nitride, boron-containing silicon, boron-containing silicon oxide, boron-and-boron-containing silicon oxide, or boron-containing silicon nitride.