# US 2022/0044924 A1 · Semiconductor structure processing method and manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0044924 A1
- Document ID: US20220044924A1
- Status: Published application
- Kind: A1
- Application number: 17/403,447
- Filed: 2021-08-16
- Published: 2022-02-10
- Earliest claimed: 2020-08-05
- Assignees: Changxin Memory Technologies, Inc.
- Applicants: Changxin Memory Technologies, Inc.
- Inventors: Ning XI; Meng ZHU
- Web page: https://patentgrep.com/patent/US20220044924A1

## CPC

- B08B 7/0014: {by incorporation in a layer which is removed with the contaminants}
- H10P 70/20: {Cleaning during device manufacture}
- B08B 3/08: the liquid having chemical or dissolving effect
- H10B 12/00: Dynamic random access memory [DRAM] devices
- H10P 50/642: {Chemical etching}
- H10P 50/691: {for Group IV materials or Group III-V materials}
- H10P 72/00: Handling or holding of wafers, substrates or devices during manufacture or treatment thereof
- H10P 76/204: {of organic photoresist masks}
- H10P 95/00: Generic processes or apparatus for manufacture or treatments not covered by the other groups of this subclass
- B08B: CLEANING IN GENERAL; PREVENTION OF FOULING IN GENERAL
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

This application relates to a semiconductor structure processing method, including: providing a semiconductor layer including a pattern, where a trench is located amongst the pattern; cleaning the pattern using a rinse liquid, where the rinse liquid fills the trench after the cleaning; forming a flexible layer, where the flexible layer displaces the rinse liquid and fills the trench, and covers a surface of the semiconductor layer; and hardening the flexible layer and subsequently removing the flexible layer.

## Claims

### Claim 1

A semiconductor structure processing method, comprising:
providing a semiconductor layer comprising a pattern, wherein a trench is located amongst the pattern;
cleaning the pattern using a rinse liquid, wherein the rinse liquid fills the trench after the cleaning;
forming a flexible layer, wherein the flexible layer displaces the rinse liquid and fills the trench, and covers a surface of the semiconductor layer; and
hardening the flexible layer and subsequently removing the flexible layer.

### Claim 2 (depends on 1)

The semiconductor structure processing method according to claim 1, wherein providing the semiconductor layer comprising the pattern comprises:
forming a photoresist layer on the surface of the semiconductor layer;
exposing and developing the photoresist layer to form a patterned mask layer; and
etching the semiconductor layer based on the patterned mask layer.

### Claim 3 (depends on 1)

The semiconductor structure processing method according to claim 1, wherein hardening the flexible layer and subsequently removing the flexible layer further comprises:
hardening the flexible layer through a heating process; and
removing the flexible layer through an ashing process.

### Claim 4 (depends on 3)

The semiconductor structure processing method according to claim 3, after hardening the flexible layer through the heating process and before removing the flexible layer through the ashing process, further comprising:
drying the flexible layer through a drying process.

### Claim 5 (depends on 1)

The semiconductor structure processing method according to claim 1, wherein the flexible layer comprises an upper flexible layer and a lower flexible layer, wherein the lower flexible layer is formed in the trench, and the upper flexible layer is formed on an upper surface of the pattern and the lower flexible layer.

### Claim 6 (depends on 5)

The semiconductor structure processing method according to claim 5, wherein removing the flexible layer through the ashing process further comprises:
removing the upper flexible layer through the ashing process in an oxygen-containing atmosphere; and
removing the lower flexible layer through the ashing process in an oxygen-free atmosphere.

### Claim 7 (depends on 6)

The semiconductor structure processing method according to claim 6, wherein the oxygen-free atmosphere comprises at least one of a hydrogen atmosphere, a nitrogen atmosphere, or a mixture of hydrogen and nitrogen atmospheres, and the lower flexible layer is removed through the ashing process in the oxygen-free atmosphere.

### Claim 8 (depends on 6)

The semiconductor structure processing method according to claim 6, wherein removing the upper flexible layer through the ashing process in the oxygen-containing atmosphere further comprises:
obtaining a thickness of the upper flexible layer;
determining an amount of oxygen required to be contained in an oxygen-containing gas based on the thickness of the upper flexible layer; and
removing the upper flexible layer through the ashing process using the oxygen-containing gas containing the required amount of oxygen.

### Claim 9 (depends on 8)

The semiconductor structure processing method according to claim 8, wherein obtaining the thickness of the upper flexible layer further comprises:
measuring an overall thickness of the flexible layer;
obtaining a depth of the trench; and
obtaining the thickness of the upper flexible layer based on the overall thickness of the flexible layer and the depth of the trench.

### Claim 10 (depends on 8)

The semiconductor structure processing method according to claim 8, wherein removing the upper flexible layer through the ashing process using the oxygen-containing gas containing the required amount of oxygen further comprises: a flow rate of the oxygen-containing gas ranges from 8000 sccm to 15000 sccm, and an ashing time of the ashing process ranges from 10s to 60s.

### Claim 11 (depends on 1)

The semiconductor structure processing method according to claim 1, wherein cleaning the pattern using the rinse liquid comprises:
cleaning the pattern; and
drying the pattern using isopropanol, wherein
the rinse liquid filled in the trench is the isopropanol.

### Claim 12 (depends on 2)

The semiconductor structure processing method according to claim 2, before cleaning the pattern, further comprising:
removing an etching residue through the ashing process.

### Claim 13 (depends on 1)

The semiconductor structure processing method according to claim 1, wherein forming the flexible layer comprises:
forming the flexible layer on the semiconductor layer through spin coating, wherein a spin coating speed of the flexible layer ranges from 800 rpm to 1500 rpm.

### Claim 14 (depends on 1)

The semiconductor structure processing method according to claim 1, wherein the semiconductor layer is selected from a group consisting of a substrate, a conductive or semi-conductive layer made of a doped semiconductor material, a non-conductive layer made of a non-doped semiconductor material, and an isolation layer.

### Claim 15 (depends on 1)

The semiconductor structure processing method according to claim 1, wherein the pattern and the trench comprise an aspect ratio of larger than 9.

### Claim 16 (depends on 1)

A semiconductor structure manufacturing method, comprising:
providing a semiconductor layer;
performing patterning processing on the semiconductor layer to form a pattern on the semiconductor layer, wherein a trench is located amongst the pattern; and
processing the semiconductor layer based on the semiconductor structure processing method according to claim 1.

### Claim 17 (depends on 14)

The semiconductor structure manufacturing method according to claim 14, wherein the patterning processing is performed on the semiconductor layer through an etching process, wherein the etching process leaves behind an etching residue in the trench after the etching, further comprising: removing the etching residue through an ashing process before cleaning the pattern.

### Claim 18 (depends on 1)

The semiconductor structure processing method according to claim 1, wherein the semiconductor layer is selected from a group consisting of a substrate, a conductive or semi-conductive layer made of a doped semiconductor material, and an isolation layer.

### Claim 19 (depends on 1)