# US 2022/0037696 A1 · Pre-lithiated polyphenylene sulfide, polyphenylene sulfide-based solid electrolyte membrane, battery electrode sheet, quasi-solid-state lithium ion battery and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0037696 A1
- Document ID: US20220037696A1
- Status: Published application
- Kind: A1
- Application number: 17/413,960
- Filed: 2020-11-20
- Published: 2022-02-03
- Earliest claimed: 2019-11-21
- Assignees: Jiangsu University
- Applicants: Jiangsu University
- Inventors: Haitao ZHOU; Hongquan GAO; Jianchun WU; Chongchen YU; Menghao LIU; Dong HOU
- Web page: https://patentgrep.com/patent/US20220037696A1

## CPC

- H01M 10/0565: Polymeric materials, e.g. gel-type or solid-type
- C08G 75/02: Polythioethers
- C08G 75/0204: Polyarylenethioethers
- C08G 75/0254: using metal sulfides
- C08G 75/14: Polysulfides
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2300/0082: Organic polymers
- H01M 2300/0085: Immobilising or gelification of electrolyte
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for manufacturing a pre-lithiated polyphenylene sulfide with a high solid solubility of lithium includes: placing NMP, Li2S, and LiOH into a high-pressure reactor to obtain a mixture, and heating the mixture to 150-250° C. for a high-temperature dehydration for 2-5 h, and then cooling the mixture to 100° C. and adding p-DCB to the mixture for a reaction at 150-250° C. for 80-200 min; dropwise adding hydrochloric acid in an identical amount as that of the LiOH neutralize LiOH, and removing NMP and H2O by evaporation or sublimation, to obtain a dry mixed powder; and to the dry mixed powder, adding a chloride ion complexing agent to obtain a mixture, stirring the mixture to homogeneity, and placing the mixture in a sealed reactor for a reaction at 150-250° C. for 80-200 min, followed by washing and drying, to obtain the pre-lithiated polyphenylene sulfide.

## Claims

### Claim 1

A method for manufacturing a pre-lithiated polyphenylene sulfide with a high solid solubility of lithium, comprising the following steps:
placing N-methylpyrrolidone (NMP), lithium sulfide (Li2S), and lithium hydroxide (LiOH) into a high-pressure reactor with a stirring function to obtain a first mixture, and heating the first mixture to 150-250° C. for a high-temperature dehydration for 2-5 h, and then cooling the first mixture to 100° C. and adding 1,4-dichlorobenzene (p-DCB) to the first mixture for a first reaction at 150-250° C. for 80-200 min;
dropwise adding hydrochloric acid in an identical amount as an amount of the LiOH on a molar basis to neutralize the LiOH, and removing the NMP and H2O by an evaporation or sublimation, to obtain a dry mixed powder; and
to the dry mixed powder, adding a chloride ion complexing agent to obtain a second mixture, stirring the second mixture to homogeneity, and placing the second mixture in a sealed reactor for a second reaction at 150-250° C. for 80-200 min, followed by washing and drying, to obtain the pre-lithiated polyphenylene sulfide with the high solid solubility of lithium.

### Claim 2 (depends on 1)

The method for manufacturing the pre-lithiated polyphenylene sulfide according to claim 1, wherein
the Li2S is formed by a high-temperature reaction of a lithium metal powder with a sulfur powder or the Li2S is formed by a carbothermal reduction reaction of lithium sulfate (Li2SO4).

### Claim 3 (depends on 1)

The method for manufacturing the pre-lithiated polyphenylene sulfide according to claim 1, wherein
the NMP, the Li2S, and the LiOH are at a molar ratio of 1-5:1:0.05-0.2.

### Claim 4 (depends on 1)

The method for manufacturing the pre-lithiated polyphenylene sulfide according to claim 1, wherein
the Li2S and the p-DCB are at a molar ratio of 1.3-0.8:1.

### Claim 5 (depends on 1)

The method for manufacturing the pre-lithiated polyphenylene sulfide according to claim 1, wherein
the evaporation or sublimation comprises a hot-air drying method, a rotary evaporation method, and a freeze-drying method, to maximize a retention of solid-phase components and only remove the NMP and the H2O.

### Claim 6 (depends on 1)

The method for manufacturing the pre-lithiated polyphenylene sulfide according to claim 1, wherein
the chloride ion complexing agent is an organic metal-ion-free complexing agent, and
the chloride ion complexing agent is preferably calixcrown ether, caliximidazole, calixpyrrole, or calixarene.

### Claim 7 (depends on 1)

The method for manufacturing the pre-lithiated polyphenylene sulfide according to claim 1, wherein
the chloride ion complexing agent is added in an amount on the molar basis, wherein the amount of the chloride ion complexing agent is 0.01-0.2 times an amount of the p-DCB.

### Claim 8

(canceled)

### Claim 9 (depends on 1)

A pre-lithiated polyphenylene sulfide prepared by the method according to claim 1.

### Claim 10

A method for preparing an isotropic polyphenylene sulfide-based solid electrolyte membrane, comprising the following steps:
mixing a pre-lithiated polyphenylene sulfide powder and polytetrafluoroethylene (PTFE) uniformly in a mixer under a temperature condition where the PTFE is in a glassy state, to obtain a mixed powder, and air-grinding the mixed powder with a supersonic gas to allow a molecular chain of the PTFE to extend and open and form a physical adhesion with the pre-lithiated polyphenylene sulfide powder, without a chemical reaction;
then removing the supersonic gas in the mixed powder through an extruder to form a continuous cake-like wide strip, followed by hot pressing the continuous cake-like wide strip into a pre-lithiated polyphenylene sulfide membrane material with a hot roll at a temperature lower than 150° C., and winding the pre-lithiated polyphenylene sulfide membrane material up; and
preparing the isotropic polyphenylene sulfide-based solid electrolyte membrane.

### Claim 11

(canceled)

### Claim 12

(canceled)

### Claim 13 (depends on 10)

The method for preparing the isotropic polyphenylene sulfide-based solid electrolyte membrane according to claim 10, wherein
the pre-lithiated polyphenylene sulfide powder and the PTFE are mixed uniformly in the mixer at a temperature controlled below 10° C. for a mixing time of 0.5-4 h.

### Claim 14

(canceled)

### Claim 15 (depends on 10)

A polyphenylene sulfide-based solid electrolyte membrane prepared by the method according to claim 10.

### Claim at position 16

16-26. (canceled)

### Claim 27 (depends on 15)

The polyphenylene sulfide-based solid electrolyte membrane according to claim 15, wherein
the pre-lithiated polyphenylene sulfide powder and the PTFE are mixed uniformly in the mixer at a temperature controlled below 10° C. for a mixing time of 0.5-4 h.