# US 2022/0037660 A1 · Positive electrode active material and preparation method therefor, sodium ion battery, and apparatus comprising sodium ion battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0037660 A1
- Document ID: US20220037660A1
- Status: Published application
- Kind: A1
- Application number: 17/400,130
- Filed: 2021-08-12
- Published: 2022-02-03
- Earliest claimed: 2019-02-12
- Assignees: Contemporary Amperex Technology Co., Limited
- Applicants: Contemporary Amperex Technology Co., Limited
- Inventors: Jinyou Zhu; Yongsheng Guo; Chengdu Liang; Qian Liu; Wenguang Lin
- Web page: https://patentgrep.com/patent/US20220037660A1

## CPC

- C01G 49/0027: {containing one alkali metal}
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- C01G 49/0072: {containing manganese}
- C01G 53/51: containing sodium
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 10/054: Accumulators with insertion or intercalation of metals other than lithium, e.g. with magnesium or aluminium
- C01P 2002/52: containing elements as dopants
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/76: by a space-group or by other symmetry indications
- C01P 2002/78: by stacking-plane distances or stacking sequences
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/10: Solid density
- C01P 2006/11: Powder tap density
- C01P 2006/12: Surface area
- C01P 2006/40: Electric properties
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present application discloses a positive electrode active material satisfying the chemical formula LxNayMzCuαFeβMnγO2+δ−0.5ηXη and a preparation method therefor, a sodium ion battery and an apparatus including such battery, wherein L is a doping element at alkali metal site, M is a doping element at transition metal site, and X is a doping element at oxygen site, 0≤x<0.35, 0.65≤y≤1, 0<α≤0.3, 0<β≤0.5, 0<γ≤0.5, −0.03≤δ≤0.03, 0≤η≤0.1, z+α+β+γ=1, mx+y+nz+2α+3β+4γ=2(2+δ), m is the valence state of L, and n is the valence state of M; and the pH of the positive electrode active material is 10.5-13, wherein L is a doping element at alkali metal site, M is a doping element at transition metal site, and X is a doping element at oxygen site.

## Claims

### Claim 1

A positive electrode active material satisfying the chemical formula LxNayMzCuαFeβMnγO2+δ−0.5ηXη, wherein
L is a doping element at alkali metal site and selected from one or more of Li+, K+, Mg2+, Ca2+ and Zn2+;
M is a doping element at transition metal site and selected from one or more of Li+, Ni2+, Mg2+, Mn2+, Zn2+, Ca2+, Ca2+, Ba2+, Sr2+, Mn3+, Al3+, B3+, Cr3+, V3+, Zr4+, Ti4+, Sn4+, V4+, Mo4+, Mo5+, Ru4+, Nb5+, Si4+, Nb6+, Mo6+ and Te6+;
X is a doping element at oxygen site and selected from one or more of F−, Cl−, Br− and I−,
0≤x<0.35, 0.65≤y≤1, 0<α≤0.3, 0<β≤0.5, 0<γ≤0.5, −0.03≤δ≤0.03, 0≤η≤0.1, and z+α+β+γ=1, and mx+y+nz+2α+3β+4γ=2(2+δ), m is the valence state of L, and n is the valence state of M; and
the positive electrode active material has a pH value of from 10.5 to 13.

### Claim 2 (depends on 1)

The positive electrode active material according to claim 1, wherein the positive electrode active material has a pH value of from 11.5 to 12.5.

### Claim 3 (depends on 1)

The positive electrode active material according to claim 1, wherein an interlayer spacing d003 between two crystal planes (003) of the positive electrode active material is from 5.20 Å to 5.70 Å, optionally from 5.40 Å to 5.50 Å.

### Claim 4 (depends on 1)

The positive electrode active material according to claim 1, wherein the positive electrode active material has a space group of R3m.

### Claim 5 (depends on 1)

The positive electrode active material according to claim 1, wherein the positive electrode active material has a mean particle size Dv50 of from 2 μm to 25 μm, optionally from 5 μm to 15 μm,

### Claim 6 (depends on 1)

The positive electrode active material according to claim 1, wherein the positive electrode active material has a particle size Dv99 of from 15 μm to 80 μm, optionally from 20 m to 60 am.

### Claim 7 (depends on 1)

The positive electrode active material according to claim 1, wherein the positive electrode active material has a mean particle size Dv50 of from 2 μm to 25 μm, optionally from 5 μm to 15 μm; and
the positive electrode active material has a particle size Dv99 of from 15 μm to 80 μm, optionally from 20 μm to 60 μm.

### Claim 8 (depends on 1)

The positive electrode active material according to claim 1, wherein the positive electrode active material has a specific surface area of from 0.5 m2/g to 7.0 m2/g, optionally from 0.8 m2/g to 3.0 m2/g.

### Claim 9 (depends on 1)

The positive electrode active material according to claim 1, wherein the positive electrode active material has a tapped density of from 1.5 g/cm3 to 3.0 g/cm3, optionally from 1.8 g/cm3 to 2.8 g/cm3.

### Claim 10 (depends on 1)

The positive electrode active material according to claim 1, wherein the positive electrode active material has a compacted density of from 3.0 g/cm3 to 5.0 g/cm3 at a pressure of 8 t, optionally from 3.5 g/cm3 to 4.5 g/cm3.

### Claim 11 (depends on 1)

A method for preparing the positive electrode active material according to claim 1, comprising the following steps:
mixing a L source, Na source, M source, Cu source, Fe source, Mn source and X source in a preset proportion, and then conducting a thermal treatment in an oxygen-containing atmosphere to obtain a sodium transition metal oxide;
washing the sodium transition metal oxide with a washing solution, wherein the washing solution has a pH value of from 3 to 13, optionally from 6 to 12;
re-washing the washed sodium transition metal oxide with deionized water; and
drying the re-washed sodium transition metal oxide to obtain the positive electrode active material.

### Claim 12 (depends on 1)

A sodium-ion battery, comprising the positive electrode active material according to claim 1.

### Claim 13 (depends on 12)

An apparatus, comprising the sodium-ion battery according to claim 12.