# US 2022/0037658 A1 · Positive Electrolyte Active Material for Secondary Battery, Preparation Method Thereof, and Lithium Secondary Battery Including Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0037658 A1
- Document ID: US20220037658A1
- Status: Published application
- Kind: A1
- Application number: 17/279,759
- Filed: 2019-10-21
- Published: 2022-02-03
- Earliest claimed: 2018-10-26
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Sang Min Park; Ji Hye Kim; Tae Gu Yoo; Wang Mo Jung; Gi Beom Han
- Web page: https://patentgrep.com/patent/US20220037658A1

## CPC

- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- C01G 53/50: of the type (MnO2)n-, e.g. Li(NixMn1-x)O2 or Li(MyNixMn1-x-y)O2
- C01G 53/502: containing lithium and cobalt
- C01G 53/504: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.5, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.5
- C01G 53/506: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.8, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.8
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/54: one element only
- C01P 2002/60: Compounds characterised by their crystallite size
- C01P 2002/88: by thermal analysis data, e.g. TGA, DTA, DSC
- C01P 2004/03: obtained by SEM
- C01P 2004/50: Agglomerated particles
- C01P 2006/12: Surface area
- C01P 2006/32: Thermal properties
- C01P 2006/37: Stability against thermal decomposition
- C01P 2006/40: Electric properties
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A lithium composite transition metal oxide includes nickel (Ni), cobalt (Co), and manganese (Mn), wherein the lithium composite transition metal oxide includes two or more kinds of first dopants selected from the group consisting of Zr, Al, V, Co, and Mg and two or more kinds of second dopants selected from the group consisting of Ti, Y, Sr, Nb, Ba, and Ca, and particles of the lithium composite transition metal oxide has a crystallite size of 170-300 nm.

## Claims

### Claim 1

A positive electrode active material for a secondary battery, the material being a lithium composite transition metal oxide including nickel (Ni), cobalt (Co), and manganese (Mn), wherein
the lithium composite transition metal oxide includes two or more kinds of first dopants selected from the group consisting of Zr, Al, V, Co, and Mg and two or more kinds of second dopants selected from the group consisting of Ti, Y, Sr, Nb, Ba, and Ca, and
particles of the lithium composite transition metal oxide has a crystallite size of 170 nm to 300 nm.

### Claim 2 (depends on 1)

The positive electrode active material of claim 1, wherein an average number of primary particles in secondary particles on a cross-section is 20 or less, wherein the average number is calculated by etching the particles of the lithium composite transition metal oxide into the cross-section using a focused ion beam (FIB) device, and calculating the average number when 20 or more secondary particle cross-sections are observed using a scanning electron microscope (FE-SEM).

### Claim 3 (depends on 1)

The positive electrode active material of claim 1, wherein the first dopants are contained in the total content of 2,000 ppm to 6,000 ppm.

### Claim 4 (depends on 1)

The positive electrode active material of claim 1, wherein the second dopants are contained in the total content of 500 ppm to 3,000 ppm.

### Claim 5 (depends on 1)

The positive electrode active material of claim 1, wherein the particles of the lithium composite transition metal oxide have a specific surface area of 0.2 m2/g to 0.7 m2/g.

### Claim 6 (depends on 2)

The positive electrode active material of claim 2, wherein the particles of the lithium composite transition metal oxide have an average number of primary particles in secondary particles on a cross-section of 10 or less.

### Claim 7 (depends on 1)

The positive electrode active material of claim 1, wherein the lithium composite transition metal oxide has a nickel (Ni) content of 60 mol % or greater in a total content of metals excluding Li (lithium).

### Claim 8 (depends on 1)

The positive electrode active material of claim 1, wherein the lithium composite transition metal oxide has a nickel (Ni) content of less than 60 mol % in the total content of metals excluding Li (lithium).

### Claim 9

A method for preparing a positive electrode active material for a secondary battery, the method comprising:
mixing a positive electrode active material precursor including nickel (Ni), cobalt (Co), and manganese (Mn), a lithium raw material, and at least two kinds of first dopant raw materials selected from the group consisting of Zr, Al, V, Co, and Mg, and subjecting the mixture to primary firing; and
after the primary firing, mixing at least two kinds of second dopant raw materials selected from the group consisting of Ti, Y, Sr, Nb, Ba, and Ca, and subjecting the mixture to secondary firing, wherein
particles of a lithium composite transition metal oxide having a crystallite size of 170 nm to 300 nm are formed through the primary firing and the secondary firing.

### Claim 10 (depends on 9)

The method of claim 9, wherein when the positive electrode active material precursor has a nickel (Ni) content of 60 mol % or greater in a total content of metals, the primary firing is performed at 800° C. to 1,000° C.

### Claim 11 (depends on 9)

The method of claim 9, wherein when the positive electrode active material precursor has a nickel (Ni) content of less than 60 mol % in the total content of metals, the primary firing is performed at 900° to 1,100° C.

### Claim 12 (depends on 9)

The method of claim 9, wherein when the positive electrode active material precursor has a nickel (Ni) content of 60 mol % or greater in the total content of metals, the secondary firing is performed at 600° C. to 950° C.

### Claim 13 (depends on 9)

The method of claim 9, wherein when the positive electrode active material precursor has a nickel (Ni) content of less than 60 mol % in the total content of metals, the secondary firing is performed at 700° C. to 1,050° C.

### Claim 14 (depends on 9)

The method of claim 9, wherein an average number of primary particles in secondary particles on a cross-section is 20 or less, wherein the average number is calculated by etching the particles of the lithium composite transition metal oxide formed through the primary firing and the secondary firing into the cross-sections using a focused ion beam (FIB) device, and when 20 or more secondary particle cross-sections are observed using a scanning electron microscope (FE-SEM), calculating the average number of primary particles in the secondary particles on the cross-section.

### Claim 15 (depends on 9)

The method of claim 9, wherein the first dopant raw materials are mixed such that a total content of the first dopants based on the total weight of the positive electrode active material is 2,000 ppm to 6,000 ppm.

### Claim 16 (depends on 9)

The method of claim 9, wherein the second dopant raw materials are mixed such that a total content of the second dopants based on the total weight of the positive electrode active material is 500 ppm to 3,000 ppm.

### Claim 17 (depends on 1)

A positive electrode comprising the positive electrode active material according to claim 1.

### Claim 18 (depends on 17)

A lithium secondary battery comprising the positive electrode according claim 17.