# US 2022/0037653 A1 · Use of Silicon With Impurities In Silicon-Dominant Anode Cells

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0037653 A1
- Document ID: US20220037653A1
- Status: Published application
- Kind: A1
- Application number: 17/503,846
- Filed: 2021-10-18
- Published: 2022-02-03
- Earliest claimed: 2019-11-07
- Assignees: Enevate Corporation
- Applicants: Enevate Corporation
- Inventors: Ian Browne; Benjamin Park; Jill Renee Pestana
- Web page: https://patentgrep.com/patent/US20220037653A1

## CPC

- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/364: {as mixtures}
- H01M 4/622: {being polymers}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Systems and methods for use of silicon with impurities in silicon-dominant anode cells may include a cathode, an electrolyte, and an anode including an active material, where the anode active material includes silicon, and where an impurity level of the silicon may be more than 400 ppm. The impurity level of the silicon is more than 600 ppm. The impurity level may be for elements with an atomic number between 2 and 42. The silicon may have a purity of 99.90% or less. A resistance of the silicon when pressed into a 4 mm thick and 15 mm diameter pellet may be 25 kΩ or less. The active material may include silicon, carbon, and a pyrolyzed polymer on a metal current collector. The metal current collector may include a copper or nickel foil in electrical contact with the active material. The active material may include more than 50% silicon.

## Claims

### Claim 1

A battery, comprising:
a cathode;
an electrolyte; and
an anode comprising a pyrolyzed binder material and 50% or more silicon by weight, wherein an impurity level of the silicon is more than 400 ppm.

### Claim 2 (depends on 1)

The battery according to claim 1, wherein the impurity level of the silicon is more than 600 ppm.

### Claim 3 (depends on 2)

The battery according to claim 2, wherein the impurity level is for elements with an atomic number between 2 and 42.

### Claim 4 (depends on 1)

The battery according to claim 1, wherein the silicon has a purity of 99.90% or less.

### Claim 5 (depends on 1)

The battery according to claim 1, wherein a resistance of the silicon when pressed into a 4 mm thick and 15 mm diameter pellet is 25 kΩ or less.

### Claim 6 (depends on 1)

The battery according to claim 1, wherein:
the anode further comprises a metal current collector; and
the pyrolyzed binder material and the silicon are on a surface of the metal current collector.

### Claim 7 (depends on 6)

The battery according to claim 6, wherein the anode further comprises conductive carbon.

### Claim 8 (depends on 6)

The battery according to claim 6, wherein the metal current collector comprises a copper or nickel foil in electrical contact with the pyrolyzed binder material and the silicon.

### Claim 9 (depends on 1)

The battery according to claim 1, wherein the electrolyte comprises a liquid, solid, or gel.

### Claim 10 (depends on 1)

The battery according to claim 1, wherein the anode, the electrolyte, and the cathode form a lithium ion battery cell.

### Claim 11

A method comprising:
forming a mixture comprising a binder material and silicon particles;
costing a surface with the mixture; and
pyrolyzing the mixture to form an anode active material comprising a pyrolyzed binder material and 50% or more silicon by weight, wherein an impurity level of the silicon is more than 400 ppm.

### Claim 12 (depends on 11)

The method according to claim 11, wherein coating the surface comprises coating a surface of a metal current collector with the mixture.

### Claim 13 (depends on 11)

The method according to claim 11, wherein:
coating the surface comprises coating a surface of a substrate; and
the method further comprises drying the mixture on the substrate to form a film of the mixture, and peeling the film from the substrate.

### Claim 14 (depends on 11)

The method according to claim 11, wherein the anode active material comprises conductive carbon.

### Claim 15 (depends on 11)

The method according to claim 11, wherein the impurity level of the silicon is more than 600 ppm.

### Claim 16 (depends on 11)

The method according to claim 11, wherein the impurity level is for elements with an atomic number between 2 and 40.

### Claim 17 (depends on 11)

The method according to claim 11, wherein the silicon has a purity of 99.90% or less.

### Claim 18 (depends on 11)

The method according to claim 11, wherein a resistance of the silicon when pressed into a 4 mm thick and 15 mm diameter pellet is 25 kΩ or less.

### Claim 19 (depends on 11)

The method according to claim 11, wherein coating the surface comprises coating a copper or nickel foil.

### Claim 20 (depends on 11)

The method according to claim 11, further comprising forming a lithium ion battery cell comprising a cathode, an electrolyte, and anode active material.