# US 2022/0037651 A1 · Methods and systems for salt-rinse surface doping of electrode materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0037651 A1
- Document ID: US20220037651A1
- Status: Published application
- Kind: A1
- Application number: 17/443,805
- Filed: 2021-07-27
- Published: 2022-02-03
- Earliest claimed: 2020-07-30
- Assignees: A123 Systems, Inc.
- Applicants: A123 Systems LLC
- Inventors: Lei Liu; Kitae Kim; Lixin Wang; Anil Parmar; Bryan Kim; Chloe Harrison; Andrew Millonig; Derek Johnson; Eunsung Lee; Taehwan Yu
- Web page: https://patentgrep.com/patent/US20220037651A1

## CPC

- H01M 4/366: {as layered products}
- C01G 53/502: containing lithium and cobalt
- C01G 53/504: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.5, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.5
- C01G 53/506: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.8, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.8
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0435: {Rolling or calendering}
- H01M 4/049: {Manufacturing of an active layer by chemical means}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- C01P 2002/52: containing elements as dopants
- C01P 2004/80: Particles consisting of a mixture of two or more inorganic phases
- C01P 2006/40: Electric properties
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Methods and systems are provided for salt-rinse surface doping of electrode materials for lithium-ion batteries. In one example, a method may include dissolving a dopant salt in a solvent to form a dopant salt rinse solution, rinsing an electrode active material with the dopant salt rinse solution to form a coated electrode active material, and heating the coated electrode active material to form a doped electrode active material. In some examples, a surface region of the doped electrode active material may include a uniform distribution of dopants from the dopant salt rinse solution. In this way, the electrode active material may be rinsed and doped via the dopant salt rinse solution in a single-stage process.

## Claims

### Claim 1

A method, comprising:
dissolving a dopant salt in a rinsing solvent to form a dopant salt rinse solution;
rinsing an electrode active material with the dopant salt rinse solution to obtain a uniformly surface-coated electrode active material; and
heating the uniformly surface-coated electrode active material to form a uniformly surface-doped electrode active material.

### Claim 2 (depends on 1)

The method of claim 1, wherein rinsing the electrode active material with the dopant salt rinse solution to obtain the uniformly surface-coated electrode active material comprises:
mixing the electrode active material with the dopant salt rinse solution to form a mixture;
filtering the mixture to isolate a filtrate; and
drying the filtrate.

### Claim 3 (depends on 1)

The method of claim 1, wherein the dopant salt comprises cations of any one of Al, Mg, Mn, Co, Ni, Ti, Zr, Sn, Cu, Ca, La, Ce, Y, Nd, W, Na, K, V, Nb, Mo, Fe, Zn, F, Cl, Br, S, Se, P, Sb, Si, Ge, Ga, and B, or a combination thereof.

### Claim 4 (depends on 1)

The method of claim 1, wherein the dopant salt comprises cations of any one of Al, Mg, Mn, Co, Ni, Ti, Zr, W, F, and B, or a combination thereof.

### Claim 5 (depends on 3)

The method of claim 3, wherein a surface region of the uniformly surface-doped electrode active material comprises a uniform distribution of the cations.

### Claim 6 (depends on 3)

The method of claim 3, wherein the cations are included in the uniformly surface-doped electrode active material at 0.1 to 2 mol %.

### Claim 7 (depends on 1)

The method of claim 1, wherein cations of Mn and/or cations of Co are included in the dopant salt, and wherein the cations are included in the uniformly surface-doped electrode active material at 0.1 to 15 mol %.

### Claim 8 (depends on 1)

The method of claim 1, wherein the dopant salt comprises one or more dopant oxides, one or more dopant acetates, one or more dopant nitrides, one or more dopant sulfates, one or more dopant fluorides, one or more dopant nitrates, one or more dopant phosphides, one or more dopant sulfides, one or more dopant iodides, one or more dopant phosphates, one or more dopant carbonates, one or more dopant oxalates, one or more dopant acetylacetones, or a combination thereof.

### Claim 9 (depends on 1)

The method of claim 1, wherein the electrode active material comprises one or more lithium insertion electrode materials.

### Claim 10 (depends on 1)

The method of claim 1, wherein the electrode active material is a cathode active material comprising stoichiometric NMC, lithium-rich NMC, NCA, NCMA, LNO, spinel LMO, spinel LNMO, LFP, or a combination thereof.

### Claim 11 (depends on 1)

The method of claim 1, wherein the uniformly surface-doped electrode active material is NMC or doped NMC.

### Claim 12 (depends on 1)

The method of claim 1, wherein the electrode active material is an anode active material comprising LTO, graphite, graphene, silicon, a silicon oxide, a tin oxide, or a combination thereof.

### Claim 13 (depends on 1)

The method of claim 1, wherein the rinsing solvent comprises water, ethanol, methanol, isopropanol, acetone, acetone nitrile, ethyl acetate, ethylene glycol, or a combination thereof.

### Claim 14

A method, comprising:
dissolving a metal salt in a rinsing solvent to form an aqueous rinse solution; and thereafter
mixing a cathode active material with the aqueous rinse solution to form a mixture; and thereafter,
without any further rinsing:
isolating a coated cathode active material from the mixture;
heating the coated cathode active material to obtain a surface-doped cathode active material; and
forming a cathode slurry comprising the surface-doped cathode active material.

### Claim 15 (depends on 14)

The method of claim 14, wherein mixing the cathode active material with the aqueous rinse solution comprises:
dissolving a residual lithium salt on a surface of the cathode active material; and
precipitating a dopant precipitate on the surface of the cathode active material while producing a product salt, where the dopant precipitate is formed from a cation of the metal salt and an anion of the residual lithium salt, where a product salt is formed from lithium and an anion of the metal salt is soluble in the rinsing solvent, and where the dopant precipitate has a lower solubility in the rinsing solvent than each of the residual lithium salt and the product salt.

### Claim 16 (depends on 14)

The method of claim 14, wherein the metal salt is a salt of any one of Al, Mg, Mn, Co, Ni, Ti, Zr, W, F, and B, or a combination thereof.

### Claim 17 (depends on 14)

The method of claim 14, wherein the cathode active material comprises an NMC having a molar content of nickel of 60% or greater of a total molar content of nickel, manganese, and cobalt.

### Claim 18

A doped cathode material, comprising:
NMC; and
a dopant comprising an ion of any one of Al, Mg, Mn, Co, Ni, Ti, Zr, Sn, Cu, Ca, La, Ce, Y, Nd, W, Na, K, V, Nb, Mo, Fe, Zn, F, Cl, Br, S, Se, P, Sb, Si, Ge, Ga, and B, or a combination thereof,
wherein the dopant is uniformly doped into a surface region of the NMC, and
wherein less than 10000 ppm of residual lithium salts are present at a surface of the doped cathode material.

### Claim 19 (depends on 18)

The doped cathode material of claim 18, wherein the dopant is more uniformly doped into the surface region of the NMC than via a dry surface doping process.

### Claim 20 (depends on 18)

The doped cathode material of claim 18, wherein the dopant comprises a metal ion having an ionic radius of 50 pm or greater.