# US 2022/0037553 A1 · Method for post-treating an absorber layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0037553 A1
- Document ID: US20220037553A1
- Status: Published application
- Kind: A1
- Application number: 17/276,458
- Filed: 2019-09-17
- Published: 2022-02-03
- Earliest claimed: 2018-09-22
- Assignees: (Cnbm) Bengbu Design & Research Institute for Glass Industry Co., Ltd
- Applicants: (Cnbm) Bengbu Design & Research Institute for Glass Industry Co., Ltd
- Inventors: Michael ALGASINGER; Thomas DALIBOR; Joerg PALM
- Web page: https://patentgrep.com/patent/US20220037553A1

## CPC

- H10F 71/128: {Annealing}
- H10F 77/126: {comprising only Group I-III-VI chalcopyrite materials, e.g. CuInSe2, CuGaSe2 or CuInGaSe2 [CIGS]}
- H10F 19/37: comprising means for obtaining partial light transmission through the integrated devices, or the assemblies of multiple devices, e.g. partially transparent thin-film photovoltaic modules for windows
- H10F 77/127: {comprising only Group IV-VI or only Group II-IV-VI chalcogenide materials, e.g. PbSnTe}
- H10F 77/45: Wavelength conversion means, e.g. by using luminescent material, fluorescent concentrators or up-conversion arrangements
- Y02E 10/52: PV systems with concentrators
- Y02E 10/541: CuInSe2 material PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for post-treating an absorber layer for photoelectric conversion of incident light into electric current. The method includes providing a chalcogen-containing absorber layer on a carrier, applying a post-treatment layer on a surface of the absorber layer, wherein the post-treatment material is not a buffer or component of a buffer, and thermally diffusing the post-treatment material into the absorber layer. A method for producing a layer system for the production of thin-film solar cells is also described.

## Claims

### Claim at position 1

-15. (canceled)

### Claim 16

A method for post-treating an absorber layer for photoelectric conversion of incident light into electric current, comprising:
providing a chalcogen-containing absorber layer on a carrier;
applying a post-treatment layer on a surface of the absorber layer, wherein the post-treatment layer contains at least one post-treatment material selected from the group consisting of a metal chalcogenide, an oxygen compound of a metal chalcogenide, and a hydrogen-oxygen compound of a metal chalcogenide; and
thermally diffusing the at least one post-treatment material into the absorber layer.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the post-treatment material is selected from the group consisting of an alkali sulfide, an alkaline earth sulfide, a hydrogen-oxygen compound of a metal chalcogenide with oxidation state IV, an oxygen compound of a metal chalcogenide with oxidation state IV, a hydrogen-oxygen compound of a metal chalcogenide with oxidation state VI, and an oxygen compound of a metal chalcogenide with the oxidation state VI.

### Claim 18 (depends on 17)

The method according to claim 17, wherein
the alkali sulfide is selected from the group consisting of Na2S, K2S, Rb2S and Cs2S;
the alkaline earth sulfide is selected from the group consisting of MgS, and CaS;
the hydrogen-oxygen compound of a metal chalcogenide with oxidation state IV is selected from the group consisting of NaHSO3, KHSO3, RbHSO3, and CsHSO3;
the oxygen compound of a metal chalcogenide with oxidation state IV is selected from the group consisting of Na2SO3, K2SO3, Rb2SO3, and Cs2SO3;
the hydrogen-oxygen compound of a metal chalcogenide with oxidation state VI is selected from the group consisting of NaHSO4, KHSO4, RbHSO4, and CsHSO4; and
the oxygen compound of a metal chalcogenide with oxidation state VI is selected from the group consisting of Na2SO4, K2SO4, Rb2SO4, Cs2SO4.

### Claim 19 (depends on 16)

The method according to claim 16, wherein the absorber layer has, after the thermally diffusing, a metal content in a range from 0.02 atomic % to 2.5 atomic %, based on a total amount of material of the absorber layer.

### Claim 20 (depends on 19)

The method according to claim 19, wherein the range is from 0.1 atomic % to 1.3 atomic %.

### Claim 21 (depends on 16)

The method according to claim 16, wherein the post-treatment layer contains exactly one post-treatment material selected from the group consisting of exactly one alkali chalcogenide, exactly one oxygen compound of an alkali chalcogenides, and exactly one hydrogen-oxygen compound of an alkali chalcogenide, wherein only one single alkali element is chemically bound in the post-treatment material.

### Claim 22 (depends on 16)

The method according to claim 16, wherein the at least one post-treatment material is applied on the surface of the absorber layer by a process selected from thermal evaporation, wet-chemical bath deposition, electron beam evaporation, sputtering, atomic layer deposition, and spray pyrolysis.

### Claim 23 (depends on 16)

The method according to claim 16, wherein the thermally diffusing comprises heating the post-treatment layer.

### Claim 24 (depends on 23)

The method according to claim 23, wherein the heating occurs in a temperature range from 70° C. to 700° C. with a heating time in a range from 1 min to 120 min.

### Claim 25 (depends on 24)

The method according to claim 24, wherein the temperature range is from 150° C. to 700° C.

### Claim 26 (depends on 23)

The method according to claim 23, wherein the heating occurs with an energy input in a range from 0.5 J/cm2 to 15 J/cm2.

### Claim 27 (depends on 26)

The method of claim 26, wherein the energy input is made of pulses with a pulse duration in a range from 0.2 msec to 20 msec.

### Claim 28 (depends on 16)

The method according to claim 16, wherein the absorber layer has a temperature in a range from 300° C. to 800° C. during application of the post-treatment layer.

### Claim 29 (depends on 16)

The method according to claim 16, wherein the thermally diffusing the at least one post-treatment material into the absorber layer is performed in a vacuumed environment.

### Claim 30 (depends on 16)

The method according to claim 16, wherein the thermally diffusing the at least one post-treatment material into the absorber layer is performed in an atmosphere containing at least one chalcogen or in a chalcogen-free atmosphere.

### Claim 31 (depends on 30)

The method according to claim 30, wherein the chalcogen-free atmosphere consists of inert gas.

### Claim 32 (depends on 16)

The method according to claim 16, further comprising removing the at least one post-treatment material from the surface of the absorber layer after the thermally diffusing.

### Claim 33 (depends on 16)

A method for producing a layer system for production of thin-film solar cells, comprising:
providing a carrier;
producing a back electrode layer on the carrier;
producing a chalcogen-containing absorber layer on the back electrode layer, the chalcogen-containing absorber layer being treated according to the method of claim 16;
depositing at least one buffer layer on the chalcogen-containing absorber layer; and
producing a front electrode layer on the at least one buffer layer.

### Claim 34 (depends on 33)

The method according to claim 33, wherein the at least one buffer layer is deposited in a vacuumed environment.

### Claim 35 (depends on 34)

The method according to claim 34, wherein the at least one buffer layer is deposited by sputtering.

### Claim 36 (depends on 16)

A thin-film solar cell production method, comprising:
producing a layer system for thin-film solar cells,
wherein the producing comprises the method of claim 16.