# US 2022/0037479 A1 · Oxide layer, semiconductor structure, and manufacturing methods therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0037479 A1
- Document ID: US20220037479A1
- Status: Published application
- Kind: A1
- Application number: 17/447,183
- Filed: 2021-09-08
- Published: 2022-02-03
- Earliest claimed: 2020-08-03
- Assignees: Changxin Memory Technologies, Inc.
- Applicants: Changxin Memory Technologies, Inc.
- Inventors: Li ZHANG
- Web page: https://patentgrep.com/patent/US20220037479A1

## CPC

- H10D 64/01: Manufacture or treatment
- H10B 12/00: Dynamic random access memory [DRAM] devices
- H10D 64/011: {of electrodes ohmically coupled to a semiconductor}
- H10D 64/01344: {in a nitrogen-containing ambient, e.g. N2O oxidation}
- H10D 64/27: Electrodes not carrying the current to be rectified, amplified, oscillated or switched, e.g. gates
- H10D 64/514: {characterised by the insulating layers}
- H10D 64/681: {having a compositional variation, e.g. multilayered}
- H10D 64/685: {being perpendicular to the channel plane}
- H10D 64/693: {the insulator comprising nitrogen, e.g. nitrides, oxynitrides or nitrogen-doped materials}
- H10P 14/60: of insulating materials
- H10B 12/05: {Making the transistor}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10B: ELECTRONIC MEMORY DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for manufacturing an oxide layer includes: reacting a nitrogen-oxide-containing gas with hydrogen at a first temperature to form a first oxide layer, a volume concentration of the hydrogen in a first reaction gas being a first concentration; and reacting oxygen with hydrogen at a second temperature to form a second oxide layer on a surface of the first oxide layer, a volume concentration of the hydrogen in a second reaction gas being a second concentration; where the first temperature is less than the second temperature, and the first concentration is greater than the second concentration.

## Claims

### Claim 1

A method for manufacturing an oxide layer, comprising:
reacting a nitrogen-oxide-containing gas with hydrogen at a first temperature to form a first oxide layer, a volume concentration of the hydrogen in a first reaction gas being a first concentration; and
reacting oxygen with hydrogen at a second temperature, to form a second oxide layer on a surface of the first oxide layer, a volume concentration of the hydrogen in a second reaction gas being a second concentration;
wherein the first temperature is lower than the second temperature, and the first concentration is higher than the second concentration.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the first oxide layer and the second oxide layer are manufactured by using an In-Situ Steam Generation (ISSG) process.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the first temperature is 600° C. to 800° C.; and the second temperature is 800° C. to 1050° C.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the first temperature is 650° C. to 750° C., or 700° C. to 730° C.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the first temperature is 600° C., 650° C., 700° C., 720° C., 725° C., 750° C., or 800° C.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the second temperature is 900° C. to 1000° C., 950° C. to 980° C. or 970° C. or 975° C.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the first concentration is 5% to 33%; and the second concentration is less than 5%.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the first concentration is 10% to 25%, 20% to 23%, or 21% or 23%.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the second concentration is 1% to 3%.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the second concentration is 0.5%, 1%, 1.5%, 2.5%, 2%, 3%, 3.5%, 4.5%, or 4.5%.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the nitrogen-oxide-containing gas comprises at least one of nitrous oxide, nitric oxide, nitrogen dioxide, dinitrogen trioxide, dinitrogen tetroxide, and dinitrogen pentoxide.

### Claim 12 (depends on 1)

The method according to claim 1, wherein a thickness of the first oxide layer accounts for 20%-50% of a thickness of the oxide layer.

### Claim 13 (depends on 1)

An oxide layer manufactured by using the method according to claim 1.

### Claim 14 (depends on 1)

A method for manufacturing a semiconductor structure comprising the method for manufacturing the oxide layer according to claim 1, further comprising:
providing a substrate;
forming an inter-gate dielectric layer on a surface of the substrate, wherein the inter-gate dielectric layer comprises the oxide layer;
forming a gate conductive layer on a surface of the inter-gate dielectric layer distal from the substrate;
patterning the inter-gate dielectric layer and the gate conductive layer to form a gate structure; and
forming a side wall on a sidewall of the gate structure.

### Claim 15 (depends on 14)

The method according to claim 14, wherein the forming an inter-gate dielectric layer on a surface of the substrate further comprises:
forming a nitride layer on the surface of the oxide layer distal from the substrate, the nitride layer and the oxide layer together constituting the inter-gate dielectric layer.

### Claim 16 (depends on 14)

The method according to claim 14, wherein the nitride layer comprises at least one of a plasma nitriding layer and a silicon oxynitride layer.

### Claim 17 (depends on 14)

The method according to claim 14, wherein a shallow trench isolation structure is formed in the substrate, and the shallow trench isolation structure isolates a plurality of active regions in the substrate; and the inter-gate dielectric layer is formed on surfaces of the plurality of active regions.

### Claim 18 (depends on 14)

A semiconductor structure manufactured by using the method according to claim 14.

### Claim 19 (depends on 2)

A method for manufacturing a semiconductor structure comprising the method for manufacturing the oxide layer according to claim 2, further comprising:
providing a substrate;
forming an inter-gate dielectric layer on a surface of the substrate, wherein the inter-gate dielectric layer comprises the oxide layer;
forming a gate conductive layer on a surface of the inter-gate dielectric layer distal from the substrate;
patterning the inter-gate dielectric layer and the gate conductive layer to form a gate structure; and
forming a side wall on a sidewall of the gate structure.

### Claim 20 (depends on 3)

A method for manufacturing a semiconductor structure comprising the method for manufacturing the oxide layer according to claim 3, further comprising:
providing a substrate;
forming an inter-gate dielectric layer on a surface of the substrate, wherein the inter-gate dielectric layer comprises the oxide layer;
forming a gate conductive layer on a surface of the inter-gate dielectric layer distal from the substrate;
patterning the inter-gate dielectric layer and the gate conductive layer to form a gate structure; and
forming a side wall on a sidewall of the gate structure.