# US 2022/0037477 A1 · METHOD FOR FORMING OHMIC CONTACTS, PARTICULARLY OF Ni(GeSn) TYPE IMPLEMENTING LASER ANNEALING

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0037477 A1
- Document ID: US20220037477A1
- Status: Published application
- Kind: A1
- Application number: 17/443,842
- Filed: 2021-07-28
- Published: 2022-02-03
- Earliest claimed: 2020-07-31
- Assignees: Commissariat A L'energie Atomique Et Aux Energies Alternatives
- Applicants: Commissariat A L'energie Atomique Et Aux Energies Alternatives
- Inventors: Andréa-Carolina QUINTERO COLMENA; Pablo ACOSTA ALBA; Philippe RODRIGUEZ
- Web page: https://patentgrep.com/patent/US20220037477A1

## CPC

- H10D 64/01: Manufacture or treatment
- H10P 95/50: {Alloying conductive materials with semiconductor bodies}
- H10F 77/20: Electrodes
- H10P 14/418: {the conductive layers comprising transition metals}
- H10P 34/42: with electromagnetic radiation, e.g. laser annealing (laser cutting H10P54/20)
- H10P 95/00: Generic processes or apparatus for manufacture or treatments not covered by the other groups of this subclass
- H10F 77/1226: comprising multiple Group IV elements, e.g. SiC
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION

## Abstract

The invention relates to a method for producing ohmic contacts, of type including a metal, a semiconductor and tin, including: a) forming a first layer (6), of an alloy of the semiconductor and of tin; b) then, on the first layer, forming a second layer (8), of said metal; c) laser annealing the first layer and the second layer at an energy density between 0.1 and 2 J/cm2.

## Claims

### Claim 1

Method for producing ohmic contacts, comprising a metal, a semiconductor and tin, including:
a) forming a first layer, of an alloy of the semiconductor and of tin;
b) then, on the first layer, forming a second layer, of said metal;
c) laser annealing at least the first layer at an energy density between 0.1 and 2 J/cm2

### Claim 2 (depends on 1)

Method according to claim 1, the semiconductor being silicon or germanium.

### Claim 3 (depends on 1)

Method according to claim 1, the metal being selected from nickel (Ni), cobalt (Co), titanium (Ti), platinum (Pt), nickel-platinum (NiPt) alloy, nickel-cobalt (NiCo) alloy, tantalum (Ta), tantalum nitride (TaN), titanium nitride (TiN), aluminium (Al), zirconium (Zr), ytterbium (Yb).

### Claim 4 (depends on 1)

Method according to claim 1, the energy density of the laser being between 0.44 J/cm2 and 0.7 J/cm2.

### Claim 5 (depends on 1)

Method according to claim 1, further including, after step c), a step of rapid thermal annealing, preferably at low temperature, for example between 150° C. and 250° C.

### Claim 6 (depends on 1)

Method according to claim 1, including, between steps a) and b), a step of amorphising the first layer.

### Claim 7 (depends on 6)

Method according to claim 6, the amorphisation step being obtained by implantation of one or more atomic species, for example carbon (C), and/or germanium (Ge) and/or silicon (Si).

### Claim 8 (depends on 1)

Method according to claim 1, further including, after step b) and before step c), forming a protective metal layer.

### Claim 9 (depends on 8)

Method according to claim 8, the protective metal layer being made of titanium nitride (TiN) or tantalum nitride (TaN).

### Claim 10 (depends on 1)

Method according to claim 1, the first layer, made of an alloy of the semiconductor and of tin, being obtained by epitaxial growth on a substrate of said semiconductor.

### Claim 11 (depends on 1)

Method according to claim 1, the laser annealing of the first layer having an energy density between 0.1 and 0.8 J/cm2.

### Claim 12 (depends on 1)

Method according to claim 1, step c) of laser annealing being performed with the aid of a pulse laser, in one or more pulses.

### Claim 13 (depends on 12)

Method according to claim 12, the pulse laser having a wavelength lower than 450 nm and/or a pulse width at mid-height between 10 ns and 300 ns.

### Claim 14 (depends on 1)

Method according to claim 1, further including a step of doping the first layer, and optionally the substrate of said semiconductor.

### Claim 15 (depends on 1)

Method according to claim 1, including a preliminary step of determining or estimating the melting limit of the alloy of the semiconductor and of tin.

### Claim 16 (depends on 1)

Method according to claim 1, the first layer, of an alloy of the semiconductor and of tin, and optionally said semiconductor substrate being produced on a silicon substrate.

### Claim 17 (depends on 16)

Method according to claim 16, said silicon substrate forming part of an optical component or of a CMOS device.